| LIQUID-LIQUID PHASE SEPARATION AND FORMA-TION OF TWO GLASSY PHASES IN Zr-Ce-Co-CuIMMISCIBLE ALLOYS |
Zhongyuan WANG1,2,Jie HE1( ),Baijun YANG1,Hongxiang JIANG1,Jiuzhou ZHAO1,Tongmin WANG2,Hongri HAO1 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China |
|
Cite this article:
Zhongyuan WANG,Jie HE,Baijun YANG,Hongxiang JIANG,Jiuzhou ZHAO,Tongmin WANG,Hongri HAO. LIQUID-LIQUID PHASE SEPARATION AND FORMA-TION OF TWO GLASSY PHASES IN Zr-Ce-Co-CuIMMISCIBLE ALLOYS. Acta Metall Sin, 2016, 52(11): 1379-1387.
|
|
|
Abstract The liquid-liquid phase separation has been used recently to design two-glassy-phase alloys with desirable mechanical, magnetic and thermal properties. The occurrence of the liquid-liquid phase separation in the Zr-Ce binary immiscible alloys can lead to the formation of two coexistent crystalline Zr-rich and Ce-rich phases after complete solidification. In this work, a new quaternary complex alloy system (ZraCeb)(1-x)(CocCud)x was designed on the basis of the addition of metastable Co-Cu immiscible alloys in the stable Zr-Ce immiscible alloys. Distribution ratio of Co and Cu in two coexistent liquids was calculated. The mechanisms of phase formation and microstructure evolution were investigated using OM, SEM, EDS, XRD and DTA. The results show that a single-phase homogeneous melt of (ZraCeb)(1-x)(CocCud)x alloys takes place the liquid-liquid phase separation during cooling through the miscibility gap. The metal elements Co and Cu are mainly concentrated in the Zr-rich and Ce-rich liquids, respectively, which results in the formation of the two coexistent Zr-Co-rich and Ce-Cu-rich liquids. It was found that the coexistent Zr-Co-rich and Ce-Cu-rich liquids undergo liquid-to-glass transition and thus form dual glassy phases under the rapid quenching, respectively. The effects of the atomic ratio of Co and Cu, the addition amount and the cooling rate on the formation of the glassy phases have been discussed in detail by combining the experimental investigation with the thermodynamic analysis. A strategy for synthesizing liquid-phase-separated metallic glasses on the basis of suitably designed immiscible alloys has been proposed. Two-glassy-phase alloys can be obtained by rapidly quenching alloy melt in which the atomic ratio of Co and Cu and the addition amount are 4∶1 and 38.5%, respectively.
|
|
Received: 02 February 2016
|
| Fund: Supported by National Natural Science Foundation of China (Nos.51374194, 51574216 and 51271185) and Natural Science Foundation of Liaoning Province (No.2015020172) |
| [1] | Jia J, Zhao J Z, Guo J J, Liu Y.Immiscible Alloys and Their Manufacturing Technique. Harbin: Harbin Institure of Technology Press, 2002: 1 | | [1] | (贾均, 赵九洲, 郭景杰, 刘源. 难混溶合金及其制备技术. 哈尔滨: 哈尔滨工业大学出版社, 2002: 1 ) | | [2] | Massalski T B, Okamoto H, Subramanian P R, Kacprzak L.Binary Alloy Phase Diagrams. New York: ASM International, 1990: 1 | | [3] | Cao C D, G?rler G P, Herlach D M, Wei B.Mater Sci Eng, 2002; A325: 503 | | [4] | He J, Zhao J Z, Ratke L.Acta Mater, 2006; 54: 1749 | | [5] | Wilde G, Perepezko H J.Acta Mater, 1999; 47: 3009 | | [6] | Gr?bner J, Schmid-Fetzer R.JOM, 2005; 57(9): 19 | | [7] | Wang C P, Liu X J, Ohnuma I, Kainuma R, Ishida K.J Phase Equilib, 2002; 23(3): 236 | | [8] | Mirkovic D, Gr?bner J, Schmid-Fetzer R. Acta Mater, 2008; 56: 5214 | | [9] | Wang C P, Liu X J, Ohnuma I, Kainuma R, Ishida K.Science, 2002; 297: 990 | | [10] | Zhao J Z.Scr Mater, 2006; 54: 247 | | [11] | He J, Zhao J Z, Wang X F, Gao L L.Metall Mater Trans, 2005; 36A: 2449 | | [12] | Jiang H X, He J, Zhao J Z.Sci Rep, 2015; 5: 12680 | | [13] | Wang W L, Wu Y H, Li L H, Zhai W, Zhang X M, Wei B.Sci Rep, 2015; 5: 16335 | | [14] | Li J Q, Ma B Q, Min S, Lee J, Yuan Z F, Zang L K.Mater Lett, 2010; 64: 814 | | [15] | He J, Li H Q, Zhao J Z, Dai C L.Appl Phys Lett, 2008; 93: 131907 | | [16] | He J, Li H Q, Xing C Y, Zhao J Z.Acta Metall Sin, 2010; 46: 41 | | [16] | (何杰, 李海权, 兴成尧, 赵九洲. 金属学报, 2010; 46: 41) | | [17] | Yu Y, Takaku Y, Nagasako M, Wang C P, Liu X J, Kainuma R, Ishida K.Intermetallics, 2012; 25: 95 | | [18] | Cao C D, Gong S L, Guo J B, Song R B, Sun Z B, Yang S, Wang W M.Chin Phys, 2012; 21B: 086102 | | [19] | He J, Jiang H X, Chen S, Zhao J Z, Zhao L.J Non-Cryst Solids, 2011; 357: 3561 | | [20] | Ratke L, Diefenbach S.Mater Sci Eng, 1995; R15: 263 | | [21] | Liu Y, Guo J J, Jia J. Foundry, 2000; 49(1): 11(刘源, 郭景杰, 贾均. 铸造, 2000; 49(1): 11) | | [22] | He J H, Sheng H W, Schilling P J, Chien C L, Ma E.Phys Rev Lett, 2001; 86: 2826 | | [23] | Ma E.Prog Mater Sci, 2005; 50: 413 | | [24] | Zhong L, Wang J W, Sheng H W, Zhang Z, Mao S X.Nature, 2014; 512: 177 | | [25] | Sugiyama K, Shinohara A H, Waseda Y, Chen S, Inoue A.Mater Trans JIM, 1994; 35: 481 | | [26] | Kündig A A, Ohnuma M, Ping D H, Ohkubo T, Hono K.Acta Mater, 2004; 52: 2441 | | [27] | Mattern N, Kühn U, Gebert A, Gemming T, Zinkevich M, Wendrock H, Schultz L.Scr Mater, 2005; 53: 271 | | [28] | Park E S, Jeong E Y, Lee J K, Bae J C, Kwon A R, Gebert A, Schultz L, Chang H L, Kim D H.Scr Mater, 2007; 56: 197 | | [29] | Chang H J, Yook W, Park E S, Kyeong J S, Kim D H.Acta Mater, 2010; 58: 2483 | | [30] | Park B J, Chang H J, Kim D H, Kim W T, Chattopadhyay K, Abinandanan T A, Bhattacharyya S.Phys Rev Lett, 2006; 96: 245503 | | [31] | He J, Mattern N, Tan J, Zhao J Z, Kaban I, Wang Z, Ratke L, Kim D H, Kim W T, Eckert J.Acta Mater, 2013; 61: 2102 | | [32] | He J, Matern N, Kaban I, Dai F, Song K, Yan Z, Zhao J Z, Kim D H, Eckert J.J Alloys Compd, 2015; 618: 795 | | [33] | Hui X D, Chen G L. Bulk Metallic Glass.Beijing: Chemical Industry Press, 2007: 8 | | [33] | (惠希东, 陈国良. 块体非晶合金. 北京: 化学工业出版社, 2007: 8) | | [34] | Kim D H, Kim W T, Park E S, Mattern N, Eckert J.Prog Mater Sci, 2013; 58: 1103 | | [35] | Concustell A, Mattern N, Wendrock H, Kuehn U, Gebert A, Eckert J, Greer A L, Sort J, Baró M D.Scr Mater, 2007; 56: 85 | | [36] | Park E S, Jeong E Y, Lee J K, Bae J C, Kwon A R, Gebert A, Schultz L, Chang H J, Kim D H.Scr Mater, 2007; 56: 197 | | [37] | Gebert A, Kündig A A, Schultz L, Hono K.Scr Mater, 2004; 51: 961 | | [38] | He J, Kaban I, Mattern N, Song K, Sun B, Zhao J Z, Kim D H, Eckert J, Greer A L.Sci Rep, 2016; 6: 25832 | | [39] | Takeuchi A, Inoue A.Mater Trans, 2005; 46: 2817 | | [40] | Liu X J, Zhang H H, Wang C P, Ishida K.J Alloys Compd, 2009; 482: 99 | | [41] | He X C, Wang H, Liu H S, Jin Z P.Calphad, 2006; 30: 367 | | [42] | Su X P, Zhang W J, Du Z M.J Alloys Compd, 1998; 267: 121 | | [43] | Bo H, Zhang L G, Chen X M, Chen H M, Liu L B, Zheng F, Jin Z P.J Alloys Compd, 2009; 484: 286 | | [44] | Palumbo M, Curiotto S, Battezzati L.Calphad, 2006; 30: 171 | | [45] | Marangoni C. Ann Phys Chem#/magtechI#, 1871; 143: 337 | | [46] | Ratke L, Voorhees P W.Growth and Coarsening. Berlin: Springer, 2002: 1 | | [47] | Zhai W, Liu H M, Wei B.Mater Lett, 2015; 141: 221 | | [48] | Li Y.Mater Trans, 2001; 42: 556 | | [49] | Lu Z P, Liu C T.Acta Mater, 2002; 50: 3501 |
|