| FORMATION OF A GRADIENT NANOSTRUCTURED SURFACE LAYER ON A MARTENSITIC STAINLESS STEEL AND ITS EFFECTS ON THE ELECTRO- CHEMICAL CORROSION BEHAVIOR |
Haiwei HUANG1,Zhenbo WANG1( ),Li LIU2,Xingping YONG3,Ke LU1,4 |
1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
3 Shenyang Blower Works Group Co. Ltd., Shenyang 110869
4 Herbert Gleiter Institute of Nanoscience, Nanjing University of Science and Technology, Nanjing 210094 |
|
Cite this article:
Haiwei HUANG, Zhenbo WANG, Li LIU, Xingping YONG, Ke LU. FORMATION OF A GRADIENT NANOSTRUCTURED SURFACE LAYER ON A MARTENSITIC STAINLESS STEEL AND ITS EFFECTS ON THE ELECTRO- CHEMICAL CORROSION BEHAVIOR. Acta Metall Sin, 2015, 51(5): 513-518.
|
|
|
Abstract A gradient nanostructured (GNS) surface layer was fabricated on a Z5CND16-4 martensitic stainless steel by means of surface mechanical rolling treatment (SMRT). The microstructure in the GNS surface layer was characterized by using SEM and TEM. The results showed that the mean grain size increases with depth, from about 25 nm at the topmost surface layer to the initial value in the matrix. The total thickness of the grain-refined layer is about 150 mm. The electrochemical corrosion property of the SMRT sample was compared with that of the as-received sample in a 3.5%NaCl aqueous solution. It is shown that the pitting corrosion potential increases from about 0.179 V in the as-received sample to about 0.313 V in the SMRT sample, and the self-corrosion potential also increases evidently. The formation of nanostructures, the increased structural homogeneity, and the introduction of compressive residual stresses in the GNS surface layer, as well as the decreased surface roughness, were discussed to promote the pitting corrosion resistance of the SMRT sample.
|
|
Received: 10 October 2014
|
| Fund: National Basic Research Program of China (No.2012CB932201) |
| [1] | Lu K, Lu J. J Mater Sci Technol, 1999; 15: 193 | | [2] | Lu K, Lu J. Mater Sci Eng, 2004; A375: 38 | | [3] | Fang T H, Li W L, Tao N R, Lu K. Science, 2011; 331: 1587 | | [4] | Wang Z B, Tao N R, Li S, Wang W, Liu G, Lu J, Lu K. Mater Sci Eng, 2003; A352: 144 | | [5] | Villegas J C, Shaw L L. Acta Mater, 2009; 57: 5782 | | [6] | Huang H W, Wang Z B, Yong X P, Lu K. Mater Sci Technol, 2013; 29: 1200 | | [7] | Pacquentin W, Caron N, Oltra R. Appl Surf Sci, 2014; 288: 34 | | [8] | Li Y, Wang F, Liu G. Corrosion, 2004; 60: 891 | | [9] | Hao Y W, Deng B, Zhong C, Jiang Y M, Li J. J Iron Steel Res Int, 2009; 16: 68 | | [10] | Balusamy T, Sankara Narayanan T S N, Ravichandran K, Park I S, Lee M H. Corros Sci, 2013; 74: 332 | | [11] | Chen T, John H, Xu J, Lu Q, Hawk J, Liu X. Corros Sci, 2013; 77: 230 | | [12] | Wang T, Yu J, Dong B. Surf Coat Technol, 2006; 200: 4777 | | [13] | Huang R, Han Y. Mater Sci Eng, 2013; C33: 2353 | | [14] | Jelliti S, Richard C, Retraint D, Roland T, Chemkhi M, Demangel C. Surf Coat Technol, 2013; 224: 82 | | [15] | Raja K S, Namjoshi S A, Misra M. Mater Lett, 2005; 59: 570 | | [16] | Wang X Y, Li D Y. Electrochim Acta, 2002; 47: 3939 | | [17] | Huang H W, Wang Z B, Lu J, Lu K. Acta Mater, 2015; 87: 150 | | [18] | Zhou L, Liu G, Ma X L, Lu K. Acta Mater, 2008; 56: 78 | | [19] | Wang L M, Wang Z B, Lu K. Acta Mater, 2011; 59: 3710 | | [20] | Arifvianto B, Suyitno, Mahardika M. Appl Surf Sci, 2012; 258: 4538 | | [21] | Bagherifard S, Guagliano M. Eng Fract Mech, 2012; 81: 56 | | [22] | Meng G Z, Li Y, Wang F H. Electrochim Acta, 2006; 51: 4277 | | [23] | Liu L, Li Y, Wang F H. Acta Metall Sin, 2014; 50: 212 (刘 莉, 李 瑛, 王福会. 金属学报, 2014; 50: 212) | | [24] | Moon J, Ha H Y, Lee T H, Lee C. Mater Chem Phys, 2013; 142: 556 | | [25] | Hara T, Asahi H. ISIJ Int, 2000; 40: 1134 | | [26] | Peyre P, Scherpereel X, Berthe L, Carboni C, Fabbro R, Béranger G, Lemaitre C. Mater Sci Eng, 2000; A280: 294 | | [27] | Sun Y, Bailey R. Surf Coat Technol, 2014; 253: 284 | | [28] | Li W, Li D Y. Acta Mater, 2006; 54: 445 |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|