| MOLECULAR DYNAMICS SIMULATION ON THE EVOLUTION OF MICROSTRUCTURES OF LIQUID ZnxAl100−x ALLOYS DURING RAPID SOLIDIFICATION |
| MO Yunfei 1, LIU Rangsu 1, LIANG Yongchao 1, ZHENG Naichao 2, ZHOU Lili 1,TIAN Zean 1, PENG Ping 2 |
1. School of Physics and Microelectronics Science, Hunan University, Changsha 410082
2. School of Materials Science and Engineering, Hunan University, Changsha 410082 |
|
Cite this article:
MO Yunfei, LIU Rangsu, LIANG Yongchao, ZHENG Naichao, ZHOU Lili,TIAN Zean, PENG Ping. MOLECULAR DYNAMICS SIMULATION ON THE EVOLUTION OF MICROSTRUCTURES OF LIQUID ZnxAl100−x ALLOYS DURING RAPID SOLIDIFICATION. Acta Metall Sin, 2012, 48(8): 907-914.
|
|
|
Abstract A molecular dynamics simulation of the rapid solidification process of liquid ZnxAl100−x (x=25, 50, 75) alloys has been performed, and their microstructural evolutions have been analyzed by means of bond–type index method of Honeycutt–Andersen (H–A) and cluster–type index method. Results show that at the cooling rate of 1×1012 K/s all rapid solidified alloys are amorphous structures with majority of 1551 bond–type and icosahedronal basic cluster of (12 0 12 0 0 0).In the rapid solidification process, a peak of the number of 1551 bond–type and icosahedronal basic cluster is demonstrated to exist at the special point corresponding to the glass transition temperature (Tg) of alloys. Tg, the glass forming ability (GFA) and the chemical short–range order (PCSRO) drop with the increase in content of Zn of ZnxAl100−x (x=25, 50, 75) alloys. Segregation and clustering of Zn and Al atoms in molten and rapid solidified alloys are also detected by PCSRO and visualization analysis.
|
|
Received: 13 February 2012
|
| Fund: Supported by National Natural Science Foundation of China (Nos.50871033, 50571037 and 51071065) |
| [1] Sproul W D. Science, 1996; 237: 889[2] Kumar R, Sivaramakrishnan C S. J Mater Sci, 1969; 4: 1008[3] Zhu Y H, Murphy S, Yeung C F. J Mater Process Technol, 1999; 94: 78[4] Zhu Y H, Man H C, Lee W B. J Mater Process Technol, 2003; 139: 296[5] Zhang L, Xu S N, Zhang C B, Qi Y. Acta Metall Sin, 2008; 44: 1101(张林, 徐送宁, 张彩碚, 祁阳. 金属学报, 2008; 44: 1101)[6] Zhao Y, Zhao J Z, Hu Z Q. Acta Metall Sin, 2008; 44: 1157(赵毅, 赵九洲, 胡壮麟. 金属学报, 2008; 44: 1157)[7] Wang R S, Hou H N, Chen G L. Acta Metall Sin, 2009; 45: 692(王荣山, 侯怀宁, 陈国良, 金属学报, 2009; 45: 692)[8] Li H, Bian X F, Zhang J X. Mater Sci Eng, 1999; A271: 116[9] Fang H Z, Hui X, Chen G L, Liu Z K. Appl Phys Lett, 2009; 94: 091904[10] Chen Y Q, Ma E, Sheng H W. Phys Rev Lett, 2009; 102: 245501[11] Liu R S, Dong K J, Li J Y, Yu A B, Zou R P. J Non–Cryst Solids, 2005; 351: 612[12] Liu R S, Li J Y, Dong K J, Zheng C X, Liu H R. Mater Sci Eng, 2002; B94: 141[13] Zhang H T, Liu R S, Hou Z Y, Zhang A L, Chen X Y, Du S H. Acta Phys Sin, 2006; 55: 2409(张海涛, 刘让苏, 侯兆阳, 张爱龙, 陈晓莹, 杜生海. 物理学报, 2006; 55: 2409)[14] Zhou L L, Liu R S, Hou Z Y, Tian Z A, Lin Y, Liu Q H.Acta Phys Sin, 2008; 57: 3653(周丽丽, 刘让苏, 侯兆阳, 田泽安, 林艳, 刘全慧. 物理学报, 2008; 57: 3653)[15] Liang Y C, Liu R S, Zhu X M, Zhou L L, Tian Z A, Liu Q H. Acta Phys Sin, 2010; 59: 7930(梁永超, 刘让苏, 朱轩民, 周丽丽, 田泽安, 刘全慧. 物理学报, 2010; 59: 395)[16] Wang S, Lai S K. J Phys, 1980; 10F: 2717[17] Li D H, Li X R, Wang S. J Phys, 1986; 16F: 309[18] Honeycutt J D, Andersen H C. J Phys Chem, 1987; 91: 4950[19] Liu R S, Dong K J, Tian Z A, Liu H R, Peng P, Yu A B. J Phys: Condens–Matter, 2007; 19: 196103[20] Liu R S, Qi D W, Wang S. Phys Rev, 1992; 45B: 451[21] Li H, Bian X F, Wang G H. Mater Sci Eng, 2001; A298: 245[22] Wang L, Bian X F, Han X F. J At Mol Phys, 2000; 17: 448(王丽, 边秀房, 韩秀峰. 原子与分子物理学报, 2000; 17: 448)[23] Bian X F, Sun B A, Hu L N, Jia Y B. Phys Lett, 2005; 335A: 61[24] Bian X F, Guo J, Lv X Q, Qin X B, Wang C D. Appl Phys Lett, 2007; 91: 221910[25] Wendt H R, Abraham F F. Phys Rev Lett, 1978; 41: 1244[26] Turnbull D. Contemp Phys, 1969; 10; 473[27] Wang D, Li Y, Sun B B, Sui M L, Lu K, Ma E. Appl Phys Lett, 2004; 84: 4029[28] Xu D H, Lohwongwatana B, Duan G, Johnson W L, Garland C. Acta Mater, 2004; 52: 2621[29] Gao T H, Liu R S, Zhou L L, Tian Z A, Xie Q. Acta Phys Chim Sin, 2009; 25: 2093(高廷红, 刘让苏, 周丽丽, 田泽安, 谢泉. 物理化学学报, 2009; 25: 2093)[30] Qi D W, Wang S. Phys Rev, 1991; 44B: 884[31] Hirata A, Guan P F, Fujita T, Hirotsu Y, Inoue A, Yavari A R, Sakurai T, Chen M W. Nat Mater, 2010; 10: 28[32] Hou Z Y, Liu L X, Liu R S, Tian Z A, Wang J G. J Appl Phys, 2010; 107: 083511[33] Sheng H W, Lou W K, Alamgir F M, Bai J M, Ma E. Nature, 2006; 439: 419[34] He J H, Ma E. Phys Rev, 2001; 64B: 144206[35] Dai X D, Li H J, Guo B, Liu B X. J Appl Phys, 2007; 101: 063512[36] Yao Y B. Hankbook of Chemistry and Physics, Shanghai: Shanghai Science and Technology Press, 1985: 105(姚允斌. 物理化学手册. 上海: 上海科学技术出版社, 1985: 105) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|