| PREPARATION AND BIOCOMPATIBILITY OF ZnHA/TiO2 HYBRID COATING |
| ZHANG Jingying1, 2), QI Min3), YANG Dayi3), AI Hongjun1) |
1) School of Stomatology, China Medical University, Shenyang 110001
2) School of Medicine, Dalian University, Dalian 116622
3) School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024 |
|
Cite this article:
ZHANG Jingying QI Min YANG Dayi AI Hongjun. PREPARATION AND BIOCOMPATIBILITY OF ZnHA/TiO2 HYBRID COATING. Acta Metall Sin, 2011, 47(4): 429-434.
|
|
|
Abstract A zinc-containing hydroxyapatite (ZnHA)/titania (TiO2) hybrid coating is developed to improve the mechanical character and biocompatibility of titanium (Ti) implants. The ZnHA layer on Ti via sol-gel method after treated by micro-arc oxidation (MAO) to produce an ZnHA/TiO2 porous titania coating on Ti implants. The chemical composition and physical structure of the modified surface layers were characterized by X-ray photoelectron spectroscopy (XPS) as well as scanning electron microscope (SEM). At the same time, in vitro co-culture assays were performed to evaluate the cell morphology, adhesion and proliferation of MG-63 cells to the modified titanium. The cells micro morphology on the ZnHA/TiO2 coatings were more polygonal compared with round than that on HA/TiO2 coatings by SEM. It was confirmed by Fluorescence microscopy observations that the osteoblast-like cells on the hybrid coating layer adhesion and spread favorably. The results in this work suggest that ZnHA/TiO2 hybrid coatings on Ti substrates can function as an implant with good mechanical character and biocompatibility.
|
|
Received: 06 September 2010
|
|
|
| [1] Hing K A, Best S M, Bonfield W. J Mater Sci: Mater Med, 1999; 10: 135[2] Kay J F. Dent Clin North Am, 1992; 36: 1[3] Elliott J C. Structure and Chemistry of the Apatites and Other Calcium Orthophosphates. Amsterdam: Elsevier, 1994: 387[4] Koutsopoulos S. J Biomed Mater Res, 2002; 62: 600[5] Ito A, Otsuka M, Kawamura H, Ikeuchi M, Ohgushi H, Sogo Y, Ichinose N. Curr Appl Phys, 2005; 5: 402[6] Legeros R Z, Legeros J, Mijares D. US Pat, 20090068285, 2009[7] Bigi A, Foresti E, Gandolfi M, Gazzano M, Roveri N. J Inorg Biochem, 1995; 58: 49[8] Miyaji F, Kono Y, Suyama Y. Mater Res Bull, 2005; 40: 209[9] Hayakawa S, Ando K, Tsuru K, Osaka A. J Am Ceram Soc, 2007; 90: 565[10] Li M O, Xiao X, Liu R, Chen C, Huang L Z. J Mater Sci: Mater Med, 2008; 19: 797[11] Ramaswamy Y, Wu C T, Zhou H, Zreiqat H. J Acta Biomaterial, 2008; 4: 1487[12] Yao Z Q, Ivanisenko Y, Diemant T, Caron A, Chuvilin A, Jiang J Z, Valiev R Z, Qi M, Fecht H J. Acta Biomater, 2010; 6: 2816[13] Cheng K, WengWJ, Han G R, Du P Y, Shen G, Yang J, Ferreira J M F. Mater Chem Phys, 2003; 78: 767[14] Le Gue’hennec L, Soueidan A, Layrolle P, Amouriq Y S. Dent Mater, 2007; 23: 844[15] Buser D, Schenk R K, Steinemann S, Fiorellini J P, Fox C H, Stich H. J Biomed Mater Res, 1991; 25: 889[16] Albrektsson T, Wennerberg A. Int J Prosthodont, 2004; 17: 536[17] Wang Y M, Liang B L, Lei T Q, Guo L X. Surf Coat Technol, 2006; 201: 82[18] Li L H, Kong Y M, Kim H W, Kim Y W, Kim H E, Heo S J, Koak J Y. Biomaterials, 2004; 25: 2867[19] Ryu H S, Song W H, Hong S H. Surf Coat Technol, 2008; 202: 1853[20] Nie X, Leyland A, Matthews A, Jiang J C, Meletis E I. J Biomed Mater Res, 2001; 57: 612[21] Vaquila I, Vergara L I, Paaaeggi M C G, Vidal R A, Ferron J. Surf Coat Technol, 1999; 122: 67[22] de Carlos A, Borrajo J P, Serra J, Gonzalez P, Leon B. J Mater Sci: Mater Med, 2006; 17: 523[23] Yamamoto A, Honma R, Sumita M. J Biomed Mater Res, 1998; 39: 331[24] Beyersmann D, Haase H. Biomaterials, 2001; 14: 331[25] Yamasaki S, Sakata–Sogawa K, Hasegawa A, Suzuki T, Kaku K, Sato E, Kurosaki T, Yamashita S, Tokunaga M, Nishida K, Hirano T. J Cell Biology, 2007; 177: 637[26] Yang X F, Xi T F. J Biomed Eng, 2001; 18: 123 |
| No Suggested Reading articles found! |
|
|