| INFLUENCE OF CARBONATION ON THE CORROSION PERFORMANCE OF STEEL HRB335 IN SIMULATED CONCRETE PORE SOLUTION |
| SHI Jinjie, SUN Wei, GENG Guoqing |
| College of Materials Science and Engineering, Jiangsu Key Laboratory of Construction Materials, Southeast University, Nanjing 211189 |
|
Cite this article:
SHI Jinjie SUN Wei GENG Guoqing. INFLUENCE OF CARBONATION ON THE CORROSION PERFORMANCE OF STEEL HRB335 IN SIMULATED CONCRETE PORE SOLUTION. Acta Metall Sin, 2011, 47(1): 17-24.
|
|
|
Abstract Electrochemical impedance spectroscopy, cyclic voltammetry and potentiodynamic polarization were used to investigate the effect of the decrease in pH values of simulated concrete pore (SCP) solutions due to carbonation on the corrosion of steel HRB335. The results indicated that the stability and corrosion inhibition of passive film on the steel surface decrease with decreasing pH value of SCP solutions. In SCP solutions with pH values of 12.5 and 11.5, the stability of passive film is in a competitive balance, the competition results from the dissolution of passive film due to the decreasing pH and the protective effect of calcium-iron containing protective layer CaFe2O4 or deposit CaCO3 formed on the steel surface. When the pH value decreased unceasingly (pH=10.5, 10.0), the stability of passive film decreased gradually, and the active uniform corrosion occurred on the steel surface.
|
|
Received: 26 September 2010
|
|
|
| Fund: Supported by National Basic Research Program of China (No.2009CB623203), High Technology Research and Development Program of China (No.2008AA030704) and The Scientific Research Foundation of Graduate School of Southeast University (No.YBJJ1017) |
| [1] Kulakowski M P, Pereira F M, Dal-Molin D C C. Constr Build Mater, 2009; 23: 1189[2] Aperador W, Gutiérrez R M, Bastidas D M. Corros Sci, 2009; 51: 2027[3] Bertolini L, Carsana M, Redaelli E. J Cult Herit, 2008; 9: 376[4] Moreno M, Morris W, Alvarez M G, Duffo G S. Corros Sci, 2004; 46: 2681[5] Valcarce M B, Vázquez M. Mater Chem Phys, 2009; 115: 313[6] Huet B, L'Hostis V, Tricheux L, Idrissi H. Mater Corros, 2010; 61: 111[7] Huet B, L’Hostis V, Miserque F, Idrissi H. Electrochimi Acta, 2005; 51: 172[8] Kitowski C J, Wheat H G. Corrosion, 1997; 53: 216[9] Etteyeb N, Dhouibi L, Sanchez M, Alonso C, Andrade C, Triki E. J Mater Sci, 2007; 42: 4721[10] Sanchez M, Gregori J, Alonso C, Garcia-Jareno J J, Takenouti H, Vicente F. Electrochimi Acta, 2007; 52: 7634[11] Jamil H E, Shriri A, Boulif R, Montemor M F, Ferreira M G S. Cem Concr Compos, 2005; 27: 671[12] Vedalakshmi R, Palaniswamy N. Mag Concr Res, 2010; 62: 177[13] Hinatsu J T, Graydon W F, Foulkes F R. J Appl Electrochem, 1988; 19: 868[14] Veleva L, Alpuche-Aviles M A, Graves-Brook M K, Wipf D O. J Electroanal Chem, 2005; 578: 45[15] Foulkes F R, McGrath P. Cem Concr Res, 1999; 29: 873[16] Videm K. Electrochimi Acta, 2001; 46: 3895[17] Qian S Y, Cusson D. Cem Concr Compos, 2004; 26: 217[18] Andrade C, Keddam M, Novoa X R. Electrochimi Acta, 2001; 46: 3905[19] Flis J, Pickering H W, Osseo-Asare K. Electrochimi Acta, 1998; 43: 1921[20] Ghods P, Isgor O B, McRae G, Miller T. Cem Concr Compos, 2009; 31: 2 |