Please wait a minute...
Acta Metall Sin  2010, Vol. 46 Issue (10): 1250-1257    DOI: 10.3724/SP.J.1037.2010.00201
论文 Current Issue | Archive | Adv Search |
EFFECTS OF SRB ON CORROSION OF Zn–Al–Cd ANODE IN MARINE SEDIMENT
ZHANG Jie 1, LIU Fengling 1,2, LI Weihua 1, DUAN Jizhou 1, HOU Baorong 1
1. Institute of Oceanology, Chinese Academy of Sciences, Qingdao 266071
2. College of Chemistry and Chemical Engineering, Chongqing University, Chongqing 400044
Cite this article: 

ZHANG Jie LIU Fengling LI Weihua DUAN Jizhou HOU Baorong. EFFECTS OF SRB ON CORROSION OF Zn–Al–Cd ANODE IN MARINE SEDIMENT. Acta Metall Sin, 2010, 46(10): 1250-1257.

Download:  PDF(2193KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  With the development of marine industry, the corrosion of metal structures in marine sediment has received increasing attention. Marine sediment is a very complex marine corrosion environment. The corrosion of sulfate–reducing bacteria (SRB) in the marine sediment is thought as one of major corrosion factors. Sacrificial anodes are widely used for protection of steel structures in the marine environment due to their high theoretical current efficiency, low active potential and low cost. However, in the marine environment, the sacrificial anodes may be attacked by microbial activity, which leads to serious failure and energy loss. Some researchers have investigated the biocidal activity of sacrificial anode, but work about the influence of microbes on the performance of sacrificial anode has been rarely reported. In this paper, a comparative study of the corrosion behavior of Zn–Al–Cd sacrificial anode in marine sediment without and with SRB was carried out using electrochemical impedance spectroscopy (EIS), polarization curve (PC), scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS). The results of EIS and PC showed that the corrosion of the sample was enhanced sharply in the presence of SRB at the beginning, while the corrosion performance of the sample in marine sediment with and without SRB gradually became similar with each other due to the decreasing SRB populations. SEM images revealed that the damage of the sample in the SRB–containing medium was severer than that in the sterile medium. EDS analysis showed that the concentration of Al and Zn in the surface film of the sample with SRB was much lower than that for the sample without SRB, which suggests that the corrosion rate of the sacrificial anode is accelerated by SRB.
Key words:  sulfate reducing bacteria      Zn–Al–Cd      marine sediment      electrochemical impedance spectroscopy     
Received:  26 April 2010     
Fund: 

Supported by National Key Technology R&D Program (No.2007BAB27B01) and National Natural Science Foundation of China (No.41006054)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2010.00201     OR     https://www.ams.org.cn/EN/Y2010/V46/I10/1250

[1] Huang Y L. Mater. Corros.,2004; 55:124 [2] Zhao X D, Wu P, Jiang J, Duan J Z, Hou B R. Chin. J. Mater. Res., 2007; 21:230 (赵晓栋,吴鹏,姜江,段继周,侯保荣. 材料研究学报, 2007;21:230) [3] Wei A J, Huo F Y, Xiong X J, Jiang H Y, Yang H L. Corros. & Prot., 2009; 30:100 (魏爱军,霍富永,熊相军,蒋华义,杨海龙. 腐蚀与防护, 2009; 30:100 [4] Sun C,Han E H,Wang X. Corros. Sci. Prot. Technol.?, 2003; 15:104 (孙成,韩恩厚,王旭. 腐蚀科学与防护技术, 2003; 15:104) [5] Zhu Y Y,Huang Y L,Huang S D,Zhang Y Y. Corros. Sci. Prot. Technol.?, 2008; 20:118 (朱永艳, 黄彦良, 黄侣迪, 张杨杨. 腐蚀科学与防护技术, 2008; 20: 118) [6] Antony P J, Chongdar S, Kumar P, Raman R. Electrochim. Acta, 2007; 52:3985 [7] Duan J Z, Hou B R, Yu Z G. Mater. Sci. Eng. C, 2006; 26:624 [8] Antony P J, Singh Raman R K , Mohanram R, Kumar P, Raman R. Corros. Sci.?, 2008; 50:1858 [9] Castaneda H, Benetton X D. Corros. Sci.?, 2008; 50: 1169 [10] T S Rao, Kora A J, Anupkumar B, Narasimhan S V, Feser R. Corros. Sci.?, 2005; 47:1071 [11] Chang X T, CHEN S G, GAO G H, YIN Y S, CHENG S, LIU T. Acta Metall, 2009; 22:313 [12] Yuan C J, Liang C H,An X W. Wuhan Univ. J. Nat. Sci.? , 2010; 15:064 [13] Fu Y, Zhai X R, Wang J, Li T, Liu Z B, Zhang X S. Chin. Rare Earths, 2005; 26:49 (符 岩,翟秀静,王 杰,李 涛,柳忠宝,张晓顺. 稀 土, 2005; 26:49) [14] Long P, Li Q F. Corros. Sci. Prot. Technol., 2007; 19:235 (龙萍, 李庆芬. 腐蚀科学与防护技术, 2007; 19:235) [15] Sun C, Han E H. The Chin. J. Nonferrous Met.?, 2003; 13:1262 (孙成,韩恩厚. 中国有色金属学报, 2003; 13:1262) [16] Ilhan-Sungur E, Cansever N, Cotuk A. Corros. Sci.?, 2007; 49:1097 [17] Santana Rodr?′guez J J, Santana Herna′ndez F J, Gonza′lez Gonza′lez J E. Corros. Sci.?, 2006;48:1265 [18] Sheng X X, Ting Y P, Pehkonen S O. Corros. Sci.?, 2007;49:2159 [19] Xu C M, Zhang Y H, Cheng G X, Zhu W S. Mater. Charact., 2008; 59:245 [20] Wan Yi, Zhang D, Liu H Q, Li Y J, Hou B R. Electrochim. Acta., 2010; 55:1528
[1] BAI Yang, WANG Zhenhua, LI Xiangbo, LI Yan. Corrosion Behavior of Al(Y)-30%Al2O3 Coating Fabricated by Low Pressure Cold Spray Technology[J]. 金属学报, 2019, 55(10): 1338-1348.
[2] Yun SHU, Maocheng YAN, Yinghua WEI, Fuchun LIU, En-Hou HAN, Wei KE. Characteristics of SRB Biofilm and Microbial Corrosionof X80 Pipeline Steel[J]. 金属学报, 2018, 54(10): 1408-1416.
[3] Yongchang QING,Zhiwei YANG,Jun XIAN,Jin XU,Maocheng YAN,Tangqing WU,Changkun YU,Libao YU,Cheng SUN. CORROSION BEHAVIOR OF Q235 STEEL UNDER THE INTERACTION OF ALTERNATING CURRENT AND MICROORGANISMS[J]. 金属学报, 2016, 52(9): 1142-1152.
[4] WEI Renchao, XU Fengling, LIN Cunguo, TANG Xiao, LI Yan. CORROSION BEHAVIOR OF B10 ALLOY EXPOSED TO SEAWATER CONTAINING VIBRIO AZUREUS, SULFATE-REDUCING BACTERIA, AND THEIR MIXTURE[J]. 金属学报, 2014, 50(12): 1461-1470.
[5] FU Xinxin, DONG Junhua, HAN En-hou, KE Wei. ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY MONITORING ON MILD STEEL Q235 IN SIMULATED INDUSTRIAL ATMOSPHERIC CORROSION ENVIORNMENT[J]. 金属学报, 2014, 50(1): 57-63.
[6] ZHOU Xiaowei,SHEN Yifu. CORROSION BEHAVIOR AND EIS STUDY OF NANOCRYSTALLINE Ni-CeO2 COATINGS IN AN ACID NaCl SOLUTION[J]. 金属学报, 2013, 49(9): 1121-1130.
[7] ZHAO Bo DU Cuiwei LIU Zhiyong LI Xiaogang YANG Jike LI Yueqiang. CORROSION BEHAVIOR OF X80 STEEL IN YINGTAN SOIL SIMULATED SOLUTION UNDER DISBONDED COATING[J]. 金属学报, 2012, 48(12): 1530-1536.
[8] ZHANG Jie SONG Xiuxia LUAN Xin SUN Caixia DUAN Jizhou HOU Baorong . EFFECTS OF SHEWANELLA ALGAE ON CORROSION OF Zn–Al–Cd ANODE[J]. 金属学报, 2012, 48(12): 1495-1502.
[9] ZHU Xuemei CAO Xuemei LIU Ming LEI Mingkai ZHANG Yansheng. AN ANTIFERROMAGNETIC Fe24Mn4Al5Cr COVAR ALLOY IMPULSE--PASSIVATED BY AN ALTERNATING CURRENT VOLTAGE OVERLAPPING A DIRECT CURRENT VOLTAGE AND ITS CORROSION RESISTANCE[J]. 金属学报, 2012, 48(11): 1357-1364.
[10] WANG Changgang DONG Junhua KE Wei CHEN Nan. EFFCTS OF pH AND Cl− CONCENTRATION ON THE CORROSION BEHAVIOR OF COPPER IN BORIC ACID BUFFER SOLUTION[J]. 金属学报, 2011, 47(3): 354-360.
[11] SONG Lixiao ZHANG Zhao ZHANG Jianqing CAO Chunan. ELECTROPLATING MECHANISM OF NANOSTRUCTURED BLACK Ni FILMS[J]. 金属学报, 2011, 47(1): 123-128.
[12] SHI Jinjie SUN Wei GENG Guoqing. INFLUENCE OF CARBONATION ON THE CORROSION PERFORMANCE OF STEEL HRB335 IN SIMULATED CONCRETE PORE SOLUTION[J]. 金属学报, 2011, 47(1): 17-24.
[13] YANG Bo LI Moucheng YAO Meiyi ZHOU Bangxin SHEN Jianian. IN SITU IMPEDANCE CHARACTERISTICS OF ZIRCONIUM ALLOY CORROSION IN HIGH TEMPERATURE AND PRESSURE WATER ENVIRONMENT[J]. 金属学报, 2010, 46(8): 946-950.
[14] ZHOU Jianlong LI Xiaogang DU Cuiwei LI Yunling LI Tao PAN Ying. ANODIC ELECTROCHEMICAL BEHAVIOR OF X80 PIPELINE STEEL IN NaHCO3 SOLUTION[J]. 金属学报, 2010, 46(2): 251-256.
[15] . EFFECT OF RE (RARE EARTH) ON THE CORROSION RESISTANCE OF CARBON STEEL IN 0.3 mol/L NACL SOLUTION[J]. 金属学报, 2008, 44(7): 863-866 .
No Suggested Reading articles found!