EFFECT OF Mg AND Zr ADDITION ON CREEP CRACK GROWTH BEHAVIOUR OF A Ni-BASE SUPERALLOY
GUO Encai;XU Fengqin Central Iron and Steel Research Institute; Ministry Metallurgical Industry Beijing
Cite this article: 

GUO Encai;XU Fengqin Central Iron and Steel Research Institute; Ministry Metallurgical Industry Beijing. EFFECT OF Mg AND Zr ADDITION ON CREEP CRACK GROWTH BEHAVIOUR OF A Ni-BASE SUPERALLOY. Acta Metall Sin, 1988, 24(5): 366-372.

Download:  PDF(487KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The growth rate of creep cracks and the times to initiation of crackand to rupture of specimen (t_(rc) and t_r) were measured by means of electrical poten-tial method using single edge-notched specimens at 700℃. The field near the cracktip under steady-state creep was represented by energy rate integral (C), and thegrowth rate as a function of C has been obtained. The agreement between the pre-dicted and observed t_(rc) values is quite good. It was found that the addition ofsmall amounts of Mg and Zr causes t_(rc) and t_r of the specimens to increase signifi-cantly.
Key words:  Ni-base alloy      Mg      Zr      creep crack growth rate     
Received:  18 May 1988     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/366

1 Floreen S, Kane R H. Metall Trans, 1976; 7A: 1157
2 Scarlin R B. Mater Sci Eng, 1977; 30: 53
3 Sadananda K. Shahinian P. Metall Trans, 1983; 14A: 1467
4 Sadananda K, Shahinian P. In: Gittus J ed., Cavities and Cracks in Creep and Fatigue, London: Applied Science, 1981: 109
5 Floreen S. Metall Trans, 1975; 6A: 1741
6 Sadananda K, Shahinian P. Metall Trans, 1977; 8A: 439
7 Nazmy M Y, Wuthrich C. Mater Sci Eng, 1983; 61: 119
8 Riedel H, Rice J R. In Fracture Mechanics, ASTM STP 700, 1980: 112
9 郭桂雄,申辉旺,蔡其巩.钢铁研究总院学报,1983;3(3) :487
[1] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[2] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[3] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[4] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[5] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[6] SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang. Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys[J]. 金属学报, 2023, 59(3): 371-386.
[7] LI Qian, SUN Xuan, LUO Qun, LIU Bin, WU Chengzhang, PAN Fusheng. Regulation of Hydrogen Storage Phase and Its Interface in Magnesium-Based Materials for Hydrogen Storage Performance[J]. 金属学报, 2023, 59(3): 349-370.
[8] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[9] GONG Xiangpeng, WU Cuilan, LUO Shifang, SHEN Ruohan, YAN Jun. Effect of Natural Aging on Artificial Aging of an Al-2.95Cu-1.55Li-0.57Mg-0.18Zr Alloy at 160oC[J]. 金属学报, 2023, 59(11): 1428-1438.
[10] PENG Liming, DENG Qingchen, WU Yujuan, FU Penghuai, LIU Ziyi, WU Qianye, CHEN Kai, DING Wenjiang. Additive Manufacturing of Magnesium Alloys by Selective Laser Melting Technology: A Review[J]. 金属学报, 2023, 59(1): 31-54.
[11] FENG Di, ZHU Tian, ZANG Qianhao, LEE Yunsoo, FAN Xi, ZHANG Hao. Solution Behavior of Spray-Formed Hypereutectic AlSiCuMg Alloy[J]. 金属学报, 2022, 58(9): 1129-1140.
[12] YANG Tianye, CUI Li, HE Dingyong, HUANG Hui. Enhancement of Microstructure and Mechanical Property of AlSi10Mg-Er-Zr Alloys Fabricated by Selective Laser Melting[J]. 金属学报, 2022, 58(9): 1108-1117.
[13] GENG Yaoxiang, TANG Hao, XU Junhua, ZHANG Zhijie, YU Lihua, JU Hongbo, JIANG Le, JIAN Jianglin. Formability and Mechanical Properties of High-Strength Al-(Mn, Mg)-(Sc, Zr) Alloy Produced by Selective Laser Melting[J]. 金属学报, 2022, 58(8): 1044-1054.
[14] SONG Qingzhong, QIAN Kun, SHU Lei, CHEN Bo, MA Yingche, LIU Kui. Interfacial Reaction Between Nickel-Based Superalloy K417G and Oxide Refractories[J]. 金属学报, 2022, 58(7): 868-882.
[15] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
No Suggested Reading articles found!