Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (6): 419-425    DOI:
Current Issue | Archive | Adv Search |
THERMAL FATIGUE AND FRACTURE MECHANICS ANALYSIS OF GREY CAST IRON
GUO Chengbi;ZHOU Weisheng Dalian Institute of Technology Liaoning
Cite this article: 

GUO Chengbi;ZHOU Weisheng Dalian Institute of Technology Liaoning. THERMAL FATIGUE AND FRACTURE MECHANICS ANALYSIS OF GREY CAST IRON. Acta Metall Sin, 1988, 24(6): 419-425.

Download:  PDF(987KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The in-phase and out-of-phase therznal fatigue, the C-P type and P-Ctype isothermal fatigue of grey cast iron were experimentally studied. The fatiguelife was evaluated analytically by using the elastic-plastic fracture mechanics method(mainly J integral). The results of experiments and calculations showed that thelife of in-phase and C-P type fatigue are longer than that of out-of-phase and P-Ctype fatigue respectively within the same strain range. This is in contrast toresults of other materials such as low carbon steel. On the other hand, the predicted life are consistent with experimental results. This suggests that J integral asa mechanics parameter for characterizing the thermal fatigue strength of grey castiron and the mechanics model and calculation method developed here are efficient.A parameter △W_t was proposed from energy aspect to characterize the capacityof crack propagation. The isothermal fatigue life is the same as the thermal fatiguelife for identical △W_t values.
Key words:  grey cast iron      thermal fatigue      fracture     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/419

1 平修二,藤野宗昭,材料,1978;27:440--445
2 桑原和夫,新田明人,北村隆行.材料,1983;32:1167--1173
3 田中启介,材料,1984;33:961--972
4 大谷隆一,北村隆行.材料,1985;34:843--849
5 Westergaurd H M, J Appl Mech, 1939; 61: A49--53
6 Paris P C, Sih G C. Stress Analysis oi Cracks, ASTM STP 391. 1965: 30--81
7 平修二,大谷隆一.材料,1979,28:414--420
[1] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[2] WU Jin, YANG Jie, CHEN Haofeng. Fracture Behavior of DMWJ Under Different Constraints Considering Residual Stress[J]. 金属学报, 2022, 58(7): 956-964.
[3] LI Min, LI Haoze, WANG Jijie, MA Yingche, LIU Kui. Effect of Ce on the Microstructure, High-Temperature Tensile Properties, and Fracture Mode of Strip Casting Non-Oriented 6.5%Si Electrical Steel[J]. 金属学报, 2022, 58(5): 637-648.
[4] PENG Zichao, LIU Peiyuan, WANG Xuqing, LUO Xuejun, LIU Jian, ZOU Jinwen. Creep Behavior of FGH96 Superalloy at Different Service Conditions[J]. 金属学报, 2022, 58(5): 673-682.
[5] HU Chen, PAN Shuai, HUANG Mingxin. Strong and Tough Heterogeneous TWIP Steel Fabricated by Warm Rolling[J]. 金属学报, 2022, 58(11): 1519-1526.
[6] FAN Guohua, MIAO Kesong, LI Danyang, XIA Yiping, WU Hao. Unraveling the Strength-Ductility Synergy of Heterostructured Metallic Materials from the Perspective of Local Stress/Strain[J]. 金属学报, 2022, 58(11): 1427-1440.
[7] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[8] ZHOU Hongwei, BAI Fengmei, YANG Lei, CHEN Yan, FANG Junfei, ZHANG Liqiang, YI Hailong, HE Yizhu. Low-Cycle Fatigue Behavior of 1100 MPa Grade High-Strength Steel[J]. 金属学报, 2020, 56(7): 937-948.
[9] YANG Jie, WANG Lei. Effect and Optimal Design of the Material Constraint in the DMWJ of Nuclear Power Plants[J]. 金属学报, 2020, 56(6): 840-848.
[10] YU Jiaying, WANG Hua, ZHENG Weisen, HE Yanlin, WU Yurui, LI Lin. Effect of the Interface Microstructure of Hot-Dip Galvanizing High-Strength Automobile Steel on Its Tensile Fracture Behaviors[J]. 金属学报, 2020, 56(6): 863-873.
[11] YI Hongliang,CHANG Zhiyuan,CAI Helong,DU Pengju,YANG Dapeng. Strength, Ductility and Fracture Strain ofPress-Hardening Steels[J]. 金属学报, 2020, 56(4): 429-443.
[12] ZHU Jian, ZHANG Zhihao, XIE Jianxin. Plastic Deformation Behavior and Fracture Mechanism of Rare Earth H13 Steel Based on In Situ TEM Tensile Study[J]. 金属学报, 2020, 56(12): 1592-1604.
[13] LIU Yang,WANG Lei,SONG Xiu,LIANG Taosha. Microstructure and High-Temperature Deformation Behavior of Dissimilar Superalloy Welded Joint of DD407/IN718[J]. 金属学报, 2019, 55(9): 1221-1230.
[14] Li ZHOU,Pengfei ZHANG,Quanzhao WANG,Bolü XIAO,Zongyi MA,Tao YU. Multi-Scale Study on the Fracture Behavior of Hot Compression B4C/6061Al Composite[J]. 金属学报, 2019, 55(7): 911-918.
[15] JIN Chenri, YANG Suyuan, DENG Xueyuan, WANG Yangwei, CHENG Xingwang. Effect of Nano-Crystallization on Dynamic Compressive Property of Zr-Based Amorphous Alloy[J]. 金属学报, 2019, 55(12): 1561-1568.
No Suggested Reading articles found!