INFLUENCE OF DEFORMATION AT MARTENSITIC STATE ON SHAPE RECOVERY IN Cu-Zn-Al ALLOYS
LI Bing;JIANG Bohong;XU Zuyao T. Y. Hsu Shanghai Jiaotong University
Cite this article: 

LI Bing;JIANG Bohong;XU Zuyao T. Y. Hsu Shanghai Jiaotong University. INFLUENCE OF DEFORMATION AT MARTENSITIC STATE ON SHAPE RECOVERY IN Cu-Zn-Al ALLOYS. Acta Metall Sin, 1989, 25(4): 1-9.

Download:  PDF(1597KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A systematic investigation of the influence of deformation on shaperecovery has been put forward in Cu-Zn-Al shape memory alloys in this paper.Starting at the model of the re-orientation of martensitic variants, the principle andessentiality of the influence of the amount of pre-deformation ε on shape recoveryrate η is elucidated.
Key words:  shape memory alloy      martensitic variant      re-orientation      CuZnAl alloy     
Received:  18 April 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I4/1

1 Perkins J. Mater Sci Eng, 1981; 51: 181
2 福元一郎,富田正吾,铃木雄一.日本金属学会志,1982;46:1109
3 Chen Shuchuan (陈树川), Hsu T Y (Xu Zuyao) (徐祖耀), Wang Chengbao (王承宝), In: Chu Youyi (褚幼义), Hsu T Y (Xu Zuyao) (徐祖耀), Ko T (柯俊) eds., Shape Memory Alloy'86, Beijing: Acdemic Press, 1986: 147
4 江伯鸿,李兵,徐祖耀,材料科学进展,1988;2(5) :27
5 Christian J W, Crocker A G. In: Nabarro F R N ed, Dislocation in Solids, Vol. Ⅲ, Amsterdam: North-Holland, 1980: 165
6 Tong H C, Wayman C M. Acta Metall, 1975; 23: 209
7 Volkov A Te, Likhachev V A, Shikhovalov L S. Fiz Met Metalloved, 1981; 51: 935
8 朱伟光,江伯鸿,徐祖耀.金属学报,1986;22:A229
9 Warlimont H, Delaey L, Krishnan R V, Tas H. J Mater Sci, 1974; 9: 1545
10 Abbe D, Gaudron R, Dynn R. J Phys F: Metal Physics, 1984; 14: 1117
11 Wollants P. Marc de Bonte, Roos J R. Z Metallk, 1983; 74: 127
[1] YANG Chao, LU Haizhou, MA Hongwei, CAI Weisi. Research and Development in NiTi Shape Memory Alloys Fabricated by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 55-74.
[2] CHEN Fei, QIU Pengcheng, LIU Yang, SUN Bingbing, ZHAO Haisheng, SHEN Qiang. Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition[J]. 金属学报, 2023, 59(1): 180-190.
[3] ZHANG Xin, CUI Bo, SUN Bin, ZHAO Xu, ZHANG Xin, LIU Qingsuo, DONG Zhizhong. Effect of Y Element on the Properties of Cu-Al-Ni High Temperature Shape Memory Alloy[J]. 金属学报, 2022, 58(8): 1065-1071.
[4] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Lüders-Like Deformation and Stress Transfer Behavior in an In Situ NiTi-NbTi Composite[J]. 金属学报, 2021, 57(7): 921-927.
[5] YE Junjie, HE Zhirong, ZHANG Kungang, DU Yuqing. Effect of Ageing on Microsturcture, Tensile Properties, and Shape Memory Behaviors of Ti-50.8Ni-0.1Zr Shape Memory Alloy[J]. 金属学报, 2021, 57(6): 717-724.
[6] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[7] XIAO Fei, CHEN Hong, JIN Xuejun. Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy[J]. 金属学报, 2021, 57(1): 29-41.
[8] CHEN Xiang,CHEN Wei,ZHAO Yang,LU Sheng,JIN Xiaoqing,PENG Xianghe. Assembly Performance Simulation of NiTiNb Shape Memory Alloy Pipe Joint Considering Coupling Effect of Phase Transformation and Plastic Deformation[J]. 金属学报, 2020, 56(3): 361-373.
[9] Lishan CUI, Daqiang JIANG. Progress in High Performance Nanocomposites Based ona Strategy of Strain Matching[J]. 金属学报, 2019, 55(1): 45-58.
[10] Zhirong HE, Peize WU, Kangkai LIU, Hui FENG, Yuqing DU, Rongyao JI. Microstructure, Phase Transformation and Shape Memory Behavior of Chilled Ti-47Ni Alloy Ribbons[J]. 金属学报, 2018, 54(8): 1157-1164.
[11] Jing BAI,Ze LI,Zhen WAN,Xiang ZHAO. A First-Principles Study on Crystal Structure, Phase Stability and Magnetic Properties of Ni-Mn-Ga-Cu Ferromagnetic Shape Memory Alloys[J]. 金属学报, 2017, 53(1): 83-89.
[12] Zhe LI,Chen XU,Kun XU,Hao WANG,Yuanlei ZHANG,Chao JING. STUDY OF MARTENSITIC TRANSFORMATION AND STRAIN BEHAVIOR IN Ni50-xCoxMn39Sn11 (x=0, 2, 4, 6) HEUSLER ALLOYS[J]. 金属学报, 2015, 51(8): 1010-1016.
[13] ZHANG Chengyan, SONG Fan, WANG Shanling, PENG Huabei, WEN Yuhua. EFFECT MECHANISM OF Mn CONTENTS ON SHAPE MEMORY OF Fe-Mn-Si-Cr-Ni ALLOYS[J]. 金属学报, 2015, 51(2): 201-208.
[14] CHEN Feng, SU Dexi, TONG Yunxiang, NIU Liqun,WANG Haibo, LI Li. MICROSTRUCTURE AND PHASE TRANSFORMATION OF Ni43Co7Mn41Sn9 HIGH TEMPERATURE SHAPE MEMORY ALLOY RIBBON[J]. 金属学报, 2013, 49(8): 976-980.
[15] LIU Qinghua,HUANG Yujin,LIU Jian,HU Qiaodan,LI Jianguo . MICROSTRUCTURE AND CRYSTAL ORIENTATION OF THE STEADY GROWTH ZONE IN THE DIRECTION ALLY SOLIDIFIED Ni-Fe-Ga-Co MAGNETIC SHAPE MEMORY ALLOYS[J]. 金属学报, 2013, 29(4): 391-398.
No Suggested Reading articles found!