INFLUENCE OF DEFORMATION AT MARTENSITIC STATE ON SHAPE RECOVERY IN Cu-Zn-Al ALLOYS
LI Bing;JIANG Bohong;XU Zuyao T. Y. Hsu Shanghai Jiaotong University
Cite this article:
LI Bing;JIANG Bohong;XU Zuyao T. Y. Hsu Shanghai Jiaotong University. INFLUENCE OF DEFORMATION AT MARTENSITIC STATE ON SHAPE RECOVERY IN Cu-Zn-Al ALLOYS. Acta Metall Sin, 1989, 25(4): 1-9.
Abstract A systematic investigation of the influence of deformation on shaperecovery has been put forward in Cu-Zn-Al shape memory alloys in this paper.Starting at the model of the re-orientation of martensitic variants, the principle andessentiality of the influence of the amount of pre-deformation ε on shape recoveryrate η is elucidated.
1 Perkins J. Mater Sci Eng, 1981; 51: 181 2 福元一郎,富田正吾,铃木雄一.日本金属学会志,1982;46:1109 3 Chen Shuchuan (陈树川), Hsu T Y (Xu Zuyao) (徐祖耀), Wang Chengbao (王承宝), In: Chu Youyi (褚幼义), Hsu T Y (Xu Zuyao) (徐祖耀), Ko T (柯俊) eds., Shape Memory Alloy'86, Beijing: Acdemic Press, 1986: 147 4 江伯鸿,李兵,徐祖耀,材料科学进展,1988;2(5) :27 5 Christian J W, Crocker A G. In: Nabarro F R N ed, Dislocation in Solids, Vol. Ⅲ, Amsterdam: North-Holland, 1980: 165 6 Tong H C, Wayman C M. Acta Metall, 1975; 23: 209 7 Volkov A Te, Likhachev V A, Shikhovalov L S. Fiz Met Metalloved, 1981; 51: 935 8 朱伟光,江伯鸿,徐祖耀.金属学报,1986;22:A229 9 Warlimont H, Delaey L, Krishnan R V, Tas H. J Mater Sci, 1974; 9: 1545 10 Abbe D, Gaudron R, Dynn R. J Phys F: Metal Physics, 1984; 14: 1117 11 Wollants P. Marc de Bonte, Roos J R. Z Metallk, 1983; 74: 127