| EFFECT OF Zr ON PHASE TRANSFORMATION IN Cu-Zn-Al SHAPE MEMORY ALLOY |
| XIAO Jichuang;FANG Jianneng;South China University of Technology; Guangzhou XIAO Jichuang; associate professor; Department of Mechanical Engineering No.2;South China University of Technology; 510641; Guangzhou |
|
Cite this article:
XIAO Jichuang;FANG Jianneng;South China University of Technology; Guangzhou XIAO Jichuang; associate professor; Department of Mechanical Engineering No.2;South China University of Technology; 510641; Guangzhou. EFFECT OF Zr ON PHASE TRANSFORMATION IN Cu-Zn-Al SHAPE MEMORY ALLOY. Acta Metall Sin, 1989, 25(5): 19-24.
|
|
|
Abstract An investigation was made of the influence of Zr addition on the hightemperature phase transformation, the martensitic forward-and-back transformationand the shape memory effect of a Cu-Zn-Al base alloy by means of the differen-tial scanning calorimetry (DSC), X-ray diffraction and TEM. An addition of 0.35wt-% Zr may effectively inhibit the precipitation of α and γ phases and facilitatethe order transformation β_2→DO_3→18RM. It was observed that the M_s—M_f and A_s—A_f temperature ranges of the alloy are rather narrow, its activation energy ofmartensitic transformation is minimum and its interface between two martensitevariants is more mobile, thus, its shape memory effect is the optimum.
|
|
Received: 18 May 1989
|
1 Miyazaki S, Otsuka K, Sakamoto H, Shimizu K. Trans Jpn Inst Met, 1981; 22: 244 2 Miyazaki S, Kawai T, Otsuka K. Scr Metall, 1982; 16: 431 3 Humbeeck J V, Segers D, Delaey L. Scr Metall, 1984; 18: 893 4 Lee J S, Wayman C M. Metallography, 1986; 19: 401--419 5 Shinoda G, Amano Y. Trans, Jpn Inst Met, 1960; 1: 54 6 方健能.华南理工大学硕士学位论文,1988 7 Cook J M, Brown L M. Scr Metall, 1978; 12: 949% |