Abstract The mechanical properties and structure of bainite and martensite af-ter tempered in 6-5-4-2 high speed steel have been investigated. It was found thatthe secondary hardening effect and resistance to heat softening as well as impacttoughness are higher in the bainite than in the martensite. TEM observations showthat the Fe_3C precipitated in the martensite after temrering at the temperaturenear the peak of hardening-tempering temperature curve. However, no Fe_3C but thedispersive MC and M_2C precipitated in the ferrite and austenite of bainite aftertempering at the same temperature. This shows the diffusion of alloy elements form-ing carbide must be taken during the process of bainite growing.
|
|
Received: 18 May 1989
|
1 Kuo Kehsin (郭可信). J Iron Steel Inst, 1953; 174: 223 2 俞学节.金属学报,1980;16:53 3 俞学节,徐祖耀.金属学报,待发表 4 Baker G R, Nutting J. Precipitation Processes in Steels, Spec. Rep. No. 64, London: The Iron Steel Inst, 1959: 1 5 俞学节,郭继良,朱家华,黄家平.金属学报,1982;18:571 6 Hehemann R F, Kinsman K R, Aaronson H I. Metall Trans, 1972; 3: 1077 7 徐祖耀,牟翊文.金属学报,1987;22:A33 8 肖纪美.高速钢的金属学问题,北京:冶金工业出版社,1976:18 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|