Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (4): 98-102    DOI:
Current Issue | Archive | Adv Search |
EQUILIBRIA OF Sr, Ba AND O, S IN LIQUID Fe
YUE Kexiang;DONG Yuanchi East China Institute of Metallurgy; Maanshan Department of Metallurgy;East China Institute of Metallurgy; Maanshan 243004
Cite this article: 

YUE Kexiang;DONG Yuanchi East China Institute of Metallurgy; Maanshan Department of Metallurgy;East China Institute of Metallurgy; Maanshan 243004. EQUILIBRIA OF Sr, Ba AND O, S IN LIQUID Fe. Acta Metall Sin, 1990, 26(4): 98-102.

Download:  PDF(326KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The reaction equilibrium constants and inieraction coefficients of SrO,Ba-O, Sr-S and Ba-S in liquid Fe at 1570℃ have been determined as follows:K_(SrO)=1.897×10~(-7) e_O~(Sr)=-43.8 e_(Sr)~O=-240.0K_(BaO)=8.204×10~(-8) e_O~(Ba)=-98.0 e_(Ba)~O=-841.2K_(SrS)=8.356×10~(-7) e_S~(Sr)=-3.9 e_(Sr)~S=-10.6K_(BaS)=4.083×10~(-7) e_S~(Ba)=-3.5 e_(Ba)~S=-14.9
Key words:  equilibrium      Sr      Ba      deoxidisation      desulphuration     
Received:  18 April 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I4/98

1 日本铁钢协会.铁钢便览,Ⅰ:基础,第三版,九善株式会社,1981:15
2 小林三郎,大森康男,三本木贡治。铁钢,1970;56:998
3 Gustafsson S,Mellberg P-O.Scand J Metall,1980;9:111
4 铃木健一郎,江岛彬夫,仲春秀夫,三本木贡治.铁钢,1977;63:S585
5 韩其勇,周德璧.第六届冶金过程物理化学学术会议论文集上册,中国金属学会冶金过程物理化学学会,重庆,1986:166
6 韩其勇,张晓东,王鹏飞,王杰,陈冬.第六届冶金过程物理化学学术会议论文集,上册,中国金属学会冶金过程物理化学学会,重庆,1986:208
7 韩其勇,王丛桦,段贵生,第七届冶金过程物理化学学术会议论文集,中国金属学会冶金过程物理化学学会,沈阳,1989:131
8 董元篪,洪道敏,李联生,彭(忄育)强.耐火材料,1985;(5) :50
[1] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[2] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[3] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[5] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[6] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[7] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[8] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[9] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[10] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[11] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[14] HAN En-Hou, WANG Jianqiu. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. 金属学报, 2023, 59(4): 513-522.
[15] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
No Suggested Reading articles found!