EQUILIBRIA OF Sr, Ba AND O, S IN LIQUID Fe |
YUE Kexiang;DONG Yuanchi East China Institute of Metallurgy; Maanshan Department of Metallurgy;East China Institute of Metallurgy; Maanshan 243004 |
|
Cite this article:
YUE Kexiang;DONG Yuanchi East China Institute of Metallurgy; Maanshan Department of Metallurgy;East China Institute of Metallurgy; Maanshan 243004. EQUILIBRIA OF Sr, Ba AND O, S IN LIQUID Fe. Acta Metall Sin, 1990, 26(4): 98-102.
|
Abstract The reaction equilibrium constants and inieraction coefficients of SrO,Ba-O, Sr-S and Ba-S in liquid Fe at 1570℃ have been determined as follows:K_(SrO)=1.897×10~(-7) e_O~(Sr)=-43.8 e_(Sr)~O=-240.0K_(BaO)=8.204×10~(-8) e_O~(Ba)=-98.0 e_(Ba)~O=-841.2K_(SrS)=8.356×10~(-7) e_S~(Sr)=-3.9 e_(Sr)~S=-10.6K_(BaS)=4.083×10~(-7) e_S~(Ba)=-3.5 e_(Ba)~S=-14.9
|
Received: 18 April 1990
|
1 日本铁钢协会.铁钢便览,Ⅰ:基础,第三版,九善株式会社,1981:15 2 小林三郎,大森康男,三本木贡治。铁钢,1970;56:998 3 Gustafsson S,Mellberg P-O.Scand J Metall,1980;9:111 4 铃木健一郎,江岛彬夫,仲春秀夫,三本木贡治.铁钢,1977;63:S585 5 韩其勇,周德璧.第六届冶金过程物理化学学术会议论文集上册,中国金属学会冶金过程物理化学学会,重庆,1986:166 6 韩其勇,张晓东,王鹏飞,王杰,陈冬.第六届冶金过程物理化学学术会议论文集,上册,中国金属学会冶金过程物理化学学会,重庆,1986:208 7 韩其勇,王丛桦,段贵生,第七届冶金过程物理化学学术会议论文集,中国金属学会冶金过程物理化学学会,沈阳,1989:131 8 董元篪,洪道敏,李联生,彭(忄育)强.耐火材料,1985;(5) :50 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|