Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (6): 132-136    DOI:
Current Issue | Archive | Adv Search |
CARBON FIBRE ELECTROPLATED BY Cu-Ni DUPLEX COATING AND ITS COMPOSITE
SUN Shoujin;ZHANG Mingda Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

SUN Shoujin;ZHANG Mingda Institute of Metal Research; Academia Sinica; Shenyang. CARBON FIBRE ELECTROPLATED BY Cu-Ni DUPLEX COATING AND ITS COMPOSITE. Acta Metall Sin, 1990, 26(6): 132-136.

Download:  PDF(1302KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The carbon fibre electroplated continuously by a compound coating ofNi prior to Cu, the composite made of this carbon fibre together with Cu substratehave been investigated. The compatibility, between carbon fibre and duplex coatingand flexual strength, linear thermal expansion coefficient and electric resistivity ofthe composite have also been examined. Owing to the transformation of face-cen-tred-cubic Cu-Ni solid solution in the compound coating under high temperature,both the nodulizing shrinkage of Cu coating alone and the graphitization of carbonfibre accelerated by single Ni coating with a consequent loss of strength were imp-roved. Because of the dissolving of minute carbon fibre in the interfacial Cu-Ni so-lid solution, the bonding strength and flexual strength of the composite were signi-ficantly increased, and the length of carbon fibre pulled out on the fracture surfa-ce was obviously reduced. The interface of the composite seems to be of the disso-lution bonding.
Key words:  duplex coating      fibre compatibility      composite      interface     
Received:  18 June 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I6/132

1 国谷启一,荒川英夫,阪上正,御法川齐,明山健二,坂本达事.日本金属学会志,1986:50:583
2 Mortimer D A, Nicholas M. J Mater. Sci, 1970, 5: 149.
3 Arakawa H, Kuniya K, Namekawa T, Litzba T. US Pat, 1978: 4 083 719
4 Warren R, Anderson C H, Carlsson M. J Mater Sci, 1978; 13: 178
5 易沛,陈汴琨,吴云书.复合材料学报,1987;4(3) :56
6 Sun Shoujin, Wang Yuqing, Zhang Mingda. In: Li Hengde ed., Proc C-MRS International'90, 18--22 June, 1990, Beijin, in pressed
7 孙守金,王作明,张名大,复合材料学报,1990;7(1) :30
[1] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[2] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[3] MA Zongyi, XIAO Bolv, ZHANG Junfan, ZHU Shize, WANG Dong. Overview of Research and Development for Aluminum Matrix Composites Driven by Aerospace Equipment Demand[J]. 金属学报, 2023, 59(4): 457-466.
[4] LI Qian, SUN Xuan, LUO Qun, LIU Bin, WU Chengzhang, PAN Fusheng. Regulation of Hydrogen Storage Phase and Its Interface in Magnesium-Based Materials for Hydrogen Storage Performance[J]. 金属学报, 2023, 59(3): 349-370.
[5] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[6] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[7] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[8] ZHOU Xiaobin, ZHAO Zhanshan, WANG Wanxing, XU Jianguo, YUE Qiang. Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface[J]. 金属学报, 2023, 59(11): 1523-1532.
[9] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[10] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[11] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[12] PAN Chengcheng, ZHANG Xiang, YANG Fan, XIA Dahai, HE Chunnian, HU Wenbin. Corrosion and Cavitation Erosion Behavior of GLNN/Cu Composite in Simulated Seawater[J]. 金属学报, 2022, 58(5): 599-609.
[13] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[14] WANG Haowei, ZHAO Dechao, WANG Mingliang. A Review of the Corrosion Protection Technology on In SituTiB2/Al Composites[J]. 金属学报, 2022, 58(4): 428-443.
[15] ZHANG Lei, SHI Tao, HUANG Huogen, ZHANG Pei, ZHANG Pengguo, WU Min, FA Tao. Phase Separation and Solidification Sequence of Uranium-Based Amorphous Composites[J]. 金属学报, 2022, 58(2): 225-230.
No Suggested Reading articles found!