Acta Metall Sin  1991, Vol. 27 Issue (3): 13-18    DOI:
Current Issue | Archive | Adv Search |
THERMODYNAMICS OF MARTENSITIC TRANSPORMATION IN β-Cu BASE ALLOYS
XU Zuyao T. Y. Hsu; ZHOU Xiaowang Shanghai Jiaotong University
Cite this article: 

XU Zuyao T. Y. Hsu; ZHOU Xiaowang Shanghai Jiaotong University. THERMODYNAMICS OF MARTENSITIC TRANSPORMATION IN β-Cu BASE ALLOYS. Acta Metall Sin, 1991, 27(3): 13-18.

Download:  PDF(501KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An approach for the thermodynamics of the thermoelastic martensitictransformation in β-Cu base alloys is suggested. Driving forces for martensitic trans-formation, T_0 and M_s temperatures in Cu-Zn, Cu-Al and Cu-Zn-Al alloys werecalculated and the calculated M_s are in good agreement with the experimental ones.Ordering of the parent phase lowers M_s in Cu-Zn and Cu-Zn-Al alloys, but risesM_s (T_0) in Cu-Al alloys. Two methods for estimation of the non-chemical freeenergy attending the thermoelastic martensitic transformation are also introduced.
Key words:  β-Cu base alloy      martensitic transformation      thermodynamics     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/13

1 Tong H G, Wayman C M. Acta Metall, 1975: 23: 209
2 Humbeeck J V, Janssen J, Mwamba-Ngoie, Delaey L. Scr Metall, 1984; 18: 893
3 Selected Values of the Thermodynamic Properties of Binary Alloys, Metals Park, Ohio: ASM, 1973: 812, 151
4 Inden G. Z Metallk, 1975; 66: 648
5 Cornelis I, Wayman C M. Acta Metall, 1974; 22: 291
6 Zhou X W, Hsu T Y (Xu Zuyao). Acta Metall, 1989; 37: 3085
7 Warlimont H, Delaey L, Krishnan R V, Has T. J Mater Sci, 1974; 9: 1545
8 Pops H, Massalski T B. Trans Metall Soc AIME, 1964; 230: 1662
9 Rapacioli R, Ahlers M. Scr Metall, 1977; 11: 1147
10 Singh S C, Murakami Y, Delaey L. Scr Metall. 1978; 12: 435
11 Ahlers M. Prog Mater Sci, 1986; 30
12 Abu-Arab A, Ahlers M. Acta Metall, 1988; 36: 2627
13 Swan P R, Warlimont H. Acta Metall, 1963; 11: 511
14 Hsu T Y (Xu Zuyao), Zhou X W, Humbeeck J V, Delaey L. Scr Metall, Mater, 1991; 25:165
16 刘锦文,李俊惠,隋晓红,顾敏,阳志英,中南矿冶学院学报,1983;38;43
[1] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[2] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[3] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[4] LI Wei, JIA Xingqi, JIN Xuejun. Research Progress of Microstructure Control and Strengthening Mechanism of QPT Process Advanced Steel with High Strength and Toughness[J]. 金属学报, 2022, 58(4): 444-456.
[5] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[6] YUAN Jiahua, ZHANG Qiuhong, WANG Jinliang, WANG Lingyu, WANG Chenchong, XU Wei. Synergistic Effect of Magnetic Field and Grain Size on Martensite Nucleation and Variant Selection[J]. 金属学报, 2022, 58(12): 1570-1580.
[7] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[8] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[9] XIAO Fei, CHEN Hong, JIN Xuejun. Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy[J]. 金属学报, 2021, 57(1): 29-41.
[10] LIU Feng, WANG Tianle. Precipitation Modeling via the Synergy of Thermodynamics and Kinetics[J]. 金属学报, 2021, 57(1): 55-70.
[11] WANG Zumin,ZHANG An,CHEN Yuanyuan,HUANG Yuan,WANG Jiangyong. Research Progress on Fundamentals and Applications of Metal-Induced Crystallization[J]. 金属学报, 2020, 56(1): 66-82.
[12] Chengming ZHENG, Qingchao TIAN. Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel[J]. 金属学报, 2019, 55(4): 427-435.
[13] CHEN Lei , HAO Shuo , MEI Ruixue , JIA Wei , LI Wenquan , GUO Baofeng . Intrinsic Increment of Plasticity Induced by TRIP and Its Dependence on the Annealing Temperature in a Lean Duplex Stainless Steel[J]. 金属学报, 2019, 55(11): 1359-1366.
[14] Lishan CUI, Daqiang JIANG. Progress in High Performance Nanocomposites Based ona Strategy of Strain Matching[J]. 金属学报, 2019, 55(1): 45-58.
[15] Cheng WEI, Changbo KE, Haitao MA, Xinping ZHANG. A Modified Phase Field Model Based on Order Parameter Gradient and Simulation of Martensitic Transformation in Large Scale System[J]. 金属学报, 2018, 54(8): 1204-1214.
No Suggested Reading articles found!