| STABILIZATION OF NON-EQUILIBRIUM CARBIDES IN POWDER SUPERALLOY RENE 95 |
| HU Benfu;LI Huiying;ZHANG Shouhua University of Science and Technology Beijing; MAO Jian;ZHOU Ruifa Institute of Aeronautical Materials; Beijing |
|
Cite this article:
HU Benfu;LI Huiying;ZHANG Shouhua University of Science and Technology Beijing; MAO Jian;ZHOU Ruifa Institute of Aeronautical Materials; Beijing. STABILIZATION OF NON-EQUILIBRIUM CARBIDES IN POWDER SUPERALLOY RENE 95. Acta Metall Sin, 1991, 27(3): 131-135.
|
|
|
Abstract The high temperature pre-heat treatment was used for Rene95 pow-der-particles before HIP consolidation. It is shown that during pre-heat treatment,the microstrucutre of the powder-particles may be more homogenized and the non-equilibrium carbides can be transformed into stable carbides MC. The appropriatecontrol of this transformation may suppress the formation of detrimental PPB car-bides.
|
|
Received: 18 March 1991
|
1 胡本芙,李慧英,吴承建,章守华.金属学报,1990;26(5) :A334 2 Domingue J A, Boesch W J, Radavich J F. In; Tien J K, Wlodek S T, Morrow H III, Gell M, Maurer G E eds., Superalloys 1980, Ohio: ASM. 1980: 335--344 3 胡本芙,李慧英,章守华.北京钢铁学院学报,1987;9(专辑2) :97-103 4 Aubin C, Davidson J H, Trottier J P. In: Tien J K, Wlodek S T, Morrow H III, Gell M, Maurer G E eds., Superalloys 1980, Ohio: ASM, 1980: 345--354 5 Dahlen M, Ingesten N G, Fischmeister H. Mod Dev Powder Metall, 1981; 14: 3--14 6 Dahlen M, Fischmeister H. In: Tien J K, Wlodek S T, Morrow H III, Gell M, Maurer G E eds., Superalloys 1980, Ohio: ASM, 1980: 449--454A |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|