Abstract An additive of Y to Ni_3Al based alloy may form a phase YNi_5 which increases in amount with the increase of Y content. It was found that the YNi_5 phase in Ni_5Al alloy could remarkably make its grains finer and its grain boundaries more crooked other than straigh. If the Y content≤0.1 wt-%, it occurs as solid solution state and is favourable to high temperature compressive properties and oxidation resistance of the alloy. While Y≥0.3 wt-%, the formation of YNi_5 is predominant in the shape of irregular strips inside Ni_3Al grains and along their grain boundaries. This seems to be quite harmful to high temperature strength, ductility and oxidation resistance of the alloy.
|
Received: 18 June 1991
|
1 青木清,和泉修,日本金属学会会志,1979;43:1190 2 郭建亭,李辉,孙超,朱耀霄.金属学报,1989;25:A406 3 Holt R T, Wallace W. Int Metall Rev, 1976; 21(1) : 1 4 Beaudry B J, Daans A H. Trans AIME, 1960; 218: 854 5 Guo Jianting, Sun Chao, Li Hui, Lai Wanhui, Tan Minghu:, Wang Shuhe. International Symposium on High-Temperature Corrosion and Protection, June 26--30. 1990, Shenyangr |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|