QUANTITATIVE RELATIONSHIP BETWEENYIELD STRESS AND r-VALUE OF Ti SHEET |
ZHOU Weixian Northwestern Polytechnical University; Xi'an |
|
Cite this article:
ZHOU Weixian Northwestern Polytechnical University; Xi'an. QUANTITATIVE RELATIONSHIP BETWEENYIELD STRESS AND r-VALUE OF Ti SHEET. Acta Metall Sin, 1991, 27(6): 44-49.
|
Abstract Based on the experimenial data, it was clarified that the plastic strain ratio R-value is not equal to Hill's γ-value for Ti sheet. From the non-quadratic orthotropic yield function proposed recently by the author, an optimal expression between yield stress and γ-value for Ti sheet was developed on overall investigation. The suituble value of exponeat in the function seems to be 6-8. Thus, an equation was suggested to estimate strength for the pressure vessel to be made of Ti sheet.
|
Received: 18 June 1991
|
1 Lankford W T. Snyder S C. Bausher J A. Trans ASM. 1950; 42: 1197 2 张德荣.金属学报,1989;25:B415 3 Hill R. The Mathematical Theory. of Plasticity. Oxford: Clarendon Press, 1950: 317--340 4 周维贤.TC1钛板的机械性能及其异性情况,西北工业大学科技资料,总字第1059期,1979 5 翟平.TA2M钛板的机械性能及各向异性,西北工业大学科技资料,ZHZ8018,1981 6 周维贤.材料科学进展,1990;4:381 7 周维贤.稀有金属,1990;14:338 8 Larson F R. Trans ASM, 1964; 57: 620--631 9 Zhou Weixian. Int J Mech Sci, 1990; 32: 513--520 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|