ON THE YNi_5 PHASE AND ITS EFFECT UPON PROPERTIES OF Ni_3 Al ALLOY
WANG Shuhe;GUO Jianting;LI Hui; SUN Chao;TAN Minghui;LAI Wanhui Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

WANG Shuhe;GUO Jianting;LI Hui; SUN Chao;TAN Minghui;LAI Wanhui Institute of Metal Research; Academia Sinica; Shenyang. ON THE YNi_5 PHASE AND ITS EFFECT UPON PROPERTIES OF Ni_3 Al ALLOY. Acta Metall Sin, 1991, 27(6): 39-43.

Download:  PDF(1084KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An additive of Y to Ni_3Al based alloy may form a phase YNi_5 which increases in amount with the increase of Y content. It was found that the YNi_5 phase in Ni_5Al alloy could remarkably make its grains finer and its grain boundaries more crooked other than straigh. If the Y content≤0.1 wt-%, it occurs as solid solution state and is favourable to high temperature compressive properties and oxidation resistance of the alloy. While Y≥0.3 wt-%, the formation of YNi_5 is predominant in the shape of irregular strips inside Ni_3Al grains and along their grain boundaries. This seems to be quite harmful to high temperature strength, ductility and oxidation resistance of the alloy.
Key words:  Ni_3Al      YNi_5 phase      Y      compressive property      oxidation resistance     
Received:  18 June 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I6/39

1 青木清,和泉修,日本金属学会会志,1979;43:1190
2 郭建亭,李辉,孙超,朱耀霄.金属学报,1989;25:A406
3 Holt R T, Wallace W. Int Metall Rev, 1976; 21(1) : 1
4 Beaudry B J, Daans A H. Trans AIME, 1960; 218: 854
5 Guo Jianting, Sun Chao, Li Hui, Lai Wanhui, Tan Minghu:, Wang Shuhe. International Symposium on High-Temperature Corrosion and Protection, June 26--30. 1990, Shenyangr
[1] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[2] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[3] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[4] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[5] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[6] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[7] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[8] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[9] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[10] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[11] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[12] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[13] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[14] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[15] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
No Suggested Reading articles found!