| HIGH TEMPERATURE OXIDATION AND STRUCTURE OF SCALE AND WHISKERS FOR Fe-Ni-Cr SEALING ALLOYS |
| DONG Zhili; MA Jusheng; TANG Xiangyun; YOU Liang (Tsinghua University; Beijing) |
|
Cite this article:
DONG Zhili; MA Jusheng; TANG Xiangyun; YOU Liang (Tsinghua University; Beijing). HIGH TEMPERATURE OXIDATION AND STRUCTURE OF SCALE AND WHISKERS FOR Fe-Ni-Cr SEALING ALLOYS. Acta Metall Sin, 1992, 28(10): 69-72.
|
|
|
Abstract The oxidation rate, the growth, morphology and structure of oxide scale and whiskers for Fe-Ni-Cr sealing alloys in H_2-H_2O atmosphere at high temperatures have been studied. The growth rate of scale is controlled by diffusion. The scale is composed of Cr_2O_3 and spinel(Fe, Mn)O Cr_2O_3 and the oxide whiskers are spinel (Fe, Mn) O Cr_2O_3.
|
|
Received: 18 October 1992
|
1 久世孝,岩井直次,平泽康伸.日本金属学会志,1972;36:1141 2 久世孝,岩井直次,幕内昭司.日本金属学会志,1973;37:272 3 Ma J S, Kojima, Takada M, Dong Z L. Tang X Y. Trans Nonferrous Met Soc Chin, 1991; 1: 66 4 Rapp R A. Metall Trans, 1984; 15A: 765 5 Raynaud G M, Rapp R A. Microstruct Sci, 1985; 12: 197 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|