| RESIDUAL STRESS CONCENTRATION AND ITS EFFECTS ON FATIGUE LIMIT AND SHORT CRACK GROWTH |
| HE Jiawen; HU Naisai; ZHANG Dingquan (Xi'an Jiaotong University) |
|
Cite this article:
HE Jiawen; HU Naisai; ZHANG Dingquan (Xi'an Jiaotong University). RESIDUAL STRESS CONCENTRATION AND ITS EFFECTS ON FATIGUE LIMIT AND SHORT CRACK GROWTH. Acta Metall Sin, 1992, 28(9): 30-34.
|
|
|
Abstract Residual stress concentration at a notch depends on both notch geometry and yield strength of the material. It varies through the depth, and its magnitude may be higher than the theoretical one. Compressive residual stress concentration at the notch of shot-peened specimen of soft material is easy to be relaxed, with the surface damage during shot-peening results in a minor contribution to the fatigue limit. Compressive residual stress increases the crack closure effect at the notch and may lead to a non-propagating crack.
|
|
Received: 18 September 1992
|
1 #12 2 Fuchs H O. Exp Mech, 1971; 11: 548. 3 Wohlfahrt, H, Residual Stress and Stress Relaxation. New York: Plenum, 1982: 71 4 Bergstrom J, Ericsson T. In: Fuchs H O ed., Proc 2nd Int Conf on Shot Peening, ICSP-2, Chicago, 14-17, May, 1984, Paramus, New Jersey: American Shot Feening Society, 1984:241 5 Kloos, K H. Z Werkstofftech, 1981; 12: 359 6 徐可为,张定全,张玉华,胡奈赛,实验力学,1989;4(4) :367' |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|