PREPARATION OF Ti-Ni HYDROGEN STORAGE FILMS BY ION BEAM SPUTTERING
ZHANG Yunshi;HU Weikang;WANG Da;YUAN Huatang;CHEN Youxiao Nankai University; Tianjin
Cite this article: 

ZHANG Yunshi;HU Weikang;WANG Da;YUAN Huatang;CHEN Youxiao Nankai University; Tianjin. PREPARATION OF Ti-Ni HYDROGEN STORAGE FILMS BY ION BEAM SPUTTERING. Acta Metall Sin, 1993, 29(1): 84-86.

Download:  PDF(236KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Ti-Ni alloy hydrogen storage films, but particularly amorphous one at roomtemperature, were prepared by ion beam sputtering method with a composite target of Ti andNi plate. The films have superior adhesion to substrate and anti-pulverizability. It was foundthat its hydrogen discharge capacity becomes higher after the amorphous film crystallized byannealing.

Key words:  sputtering      hydrogen storage      Ti-Ni alloy film     
Received:  18 January 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I1/84

1 Adachi G, Niki K, Nagai H, Shiokawa J. J Less-Comm Met, 1982; 88: 213
2 Sakaguchi H, Taniguchi N, Seri H, Shiokawa J, Acachi G. J Appl Phys, 1988; 64: 888
3 Wenzl H, Klatt K H, Meuffels F, Papathanassopoulos K. J Less-Comm Met, 1983; 89: 489
4 Sanyo Electric Co, Ltd. Jpn Kokai Tokkyo Koho, JP 60, 112, 253, 1985
5 Kim J J, Stevenson D A. J Non-Crystal Solida, 1988; 101: 187

[1] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
[2] LI Qian, SUN Xuan, LUO Qun, LIU Bin, WU Chengzhang, PAN Fusheng. Regulation of Hydrogen Storage Phase and Its Interface in Magnesium-Based Materials for Hydrogen Storage Performance[J]. 金属学报, 2023, 59(3): 349-370.
[3] CAO Qingping, LV Linbo, WANG Xiaodong, JIANG Jianzhong. Magnetron Sputtering Metal Glass Film Preparation and the “Specimen Size Effect” of the Mechanical Property[J]. 金属学报, 2021, 57(4): 473-490.
[4] ZHU Min, OUYANG Liuzhang. Kinetics Tuning and Electrochemical Performance of Mg-Based Hydrogen Storage Alloys[J]. 金属学报, 2021, 57(11): 1416-1428.
[5] LIU Yanmei, WANG Tiegang, GUO Yuyao, KE Peiling, MENG Deqiang, ZHANG Jifu. Design, Preparation and Properties of Ti-B-N Nanocomposite Coatings[J]. 金属学报, 2020, 56(11): 1521-1529.
[6] Wentao LI,Zhenyu WANG,Dong ZHANG,Jianguo PAN,Peiling KE,Aiying WANG. Preparation of Ti2AlC Coating by the Combination of a Hybrid Cathode Arc/Magnetron Sputtering with Post-Annealing[J]. 金属学报, 2019, 55(5): 647-656.
[7] Shasha YANG,Feng YANG,Minghui CHEN,Yunsong NIU,Shenglong ZHU,Fuhui WANG. Effect of Nitrogen Doping on Microstructure and Wear Resistance of Tantalum Coatings Deposited by Direct Current Magnetron Sputtering[J]. 金属学报, 2019, 55(3): 308-316.
[8] Houpu WU,Xiubo TIAN,Xinyu ZHANG,Chunzhi GONG. Discharge Characteristics of Novel Dual-Pulse HiPIMS and Deposition of CrN Films with High Deposition Rate[J]. 金属学报, 2019, 55(3): 299-307.
[9] Xiaoqin MA, Qingfeng ZHAN, Jincai LI, Qingfang LIU, Baomin WANG, Runwei LI. Influence of Oblique Sputtering on Stripe Magnetic Domain Structure and Magnetic Anisotropy of CoFeB Thin Films[J]. 金属学报, 2018, 54(9): 1281-1288.
[10] Huiying SHI, Chao YANG, Bailing JIANG, Bei HUANG, Di WANG. Influences of Target Peak Current Density on the Microstructure and Mechanical Properties of TiN Films Deposited by Dual Pulsed Power Magnetron Sputtering[J]. 金属学报, 2018, 54(6): 927-934.
[11] Xudong SUI,Guojian LI,Qiang WANG,Xuesi QIN,Xiangkui ZHOU,Kai WANG,Lijian ZUO. PREPARATION OF Ti1-xAlxN COATING IN CUTTING TITANIUM ALLOY AND ITS CUTTING PERFORMANCE[J]. 金属学报, 2016, 52(6): 741-746.
[12] Baiyang LOU,Yuxing WANG. EFFECTS OF Mo CONTENT ON THE MICRO-STRUCTURE AND TRIBOLOGICAL PROPERTIES OF CrMoAlN FILMS[J]. 金属学报, 2016, 52(6): 727-733.
[13] Fayu WU,Jianwei LI,Yi QI,Wutong DING,Ziming FAN,Yanwen ZHOU. STUDY ON PREPARATION AND PROPERTIES OF AMORPHOUS Al2O3 THIN FILMS BY RADIO FREQUENCY MAGNETRON SPUTTERING FROM POWDER TARGET[J]. 金属学报, 2016, 52(12): 1595-1600.
[14] Min ZHU, Zhongchen LU, Renzong HU, Liuzhang OUYANG. DIELECTRIC BARRIER DISCHARGE PLASMA ASSISTED BALL MILLING TECHNOLOGY AND ITS APPLICATIONS IN MATERIALS FABRICATION[J]. 金属学报, 2016, 52(10): 1239-1248.
[15] Bin WANG,Liangyin XIONG,Shi LIU. MgO SECONDARY ELECTRON EMISSION FILM PREPARED BY RADIO-FREQUENCY REACTIVE SPUTERRING[J]. 金属学报, 2016, 52(1): 10-16.
No Suggested Reading articles found!