| ADSORPTION OF SODIUM OLEATE ON QUARTZ AND FELDSPAR |
| LIU Yachuan;GONG Huangao;ZHANG Keren;TIAN Xilin Northeast University; Shenyang Institute of Multipurpose Utilization of Mineral Resources; Chengdu |
|
Cite this article:
LIU Yachuan;GONG Huangao;ZHANG Keren;TIAN Xilin Northeast University; Shenyang Institute of Multipurpose Utilization of Mineral Resources; Chengdu. ADSORPTION OF SODIUM OLEATE ON QUARTZ AND FELDSPAR. Acta Metall Sin, 1993, 29(11): 49-53.
|
|
|
Abstract The sdsorption behaviour of sodium oleate on quartz or feldspar has been ex-amined by zeta-potential and adsorbabilty measuremant, together with IR spectral analysesand flotation tests. Both electrostatic adsorption with oleate ions and physical one with oleatemolecules were occurred on quartz. While on feldspar, the chemical adsorption was con-ducted between oleate ions and Al. Thus, the adsorbability on feldspar is superior to that onquartz. The sodium cleate is able to activate feldspar flotation with amine as collector.
|
|
Received: 18 November 1993
|
1 刘亚川,龚焕高,张克仁.见:18届国际选矿会议论文集,vol.4,悉尼,澳大利亚,1993:857 2 Cookes S R B,Iwasaki I.Hyung Sup Chol.Min Eng.1959;(2) :920 3 张洪恩,刘慧纳,沈致平,魏德洲.金属矿山,1982;(11) :32 4 丘继存.东北工学院科技资料,1989 5 Lai R W. Ph. D Thesis, Berkeley, 1970 6 Fuerstenau M C, Elgillaxi D A. Trans AIME, 1966; 235: 405 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|