| AN ASPECT OF INTERNAL FATIGUE LIMIT FOR METALS WITH AID OF STRENGTH APPRAISAL ON HARDERED STEELS |
| YAO Mei;WANG Shengping;LI Jinkui;WANG Renzhi;LI Xiangbin Harbin Institute of Technology Beijing Institute of Aeronautical Materials |
|
Cite this article:
YAO Mei;WANG Shengping;LI Jinkui;WANG Renzhi;LI Xiangbin Harbin Institute of Technology Beijing Institute of Aeronautical Materials. AN ASPECT OF INTERNAL FATIGUE LIMIT FOR METALS WITH AID OF STRENGTH APPRAISAL ON HARDERED STEELS. Acta Metall Sin, 1993, 29(11): 33-41.
|
|
|
Abstract An aspect of the intermal fatigue limit for metals was proposed with the aid ofappraisal of the fatigue behaviour of shot peened, nitrided or carbonitrided steels. The inter-nal fatigue limit of metals seems to be 1.35 times of surface one. Based on this aspect, the fa-tigue strength of surface hardened steels was analysed.
|
|
Received: 18 November 1993
|
1 Hammond D W, Meguid S A. Eng Fract Mech, 1990; 37(2) : 373 2 Kang Ki J, Song Ji H, Earmme Youn Y. Fatigue Fract Eng Mater Struct, 1990; 13(1) : 1 3 谈育煦,任立平,李刚.金属学报,1989;25:A369 4 Collins J A. Failure of Materials in Mechanical Design, New York: John Wiley Sons, 1981; 368 5 王声平.哈尔滨工业大学工学硕士学位论文,1991 6 李金魁.哈尔滨工业大学工学博士学位论文,1989 7 哈宽富.金属力学性质的微观理论.北京:科学出版社,1983:579 8 Thompson N, Wadsworth N J, Louat N. Philos Mag. 1965; 1: 113 9 Forsyth P J E. Proc Roy Soc, 1957; A242: 198 10 Cottrell A H, Hull D. Proc Roy Soc, 1957; A242: 211 11 Koanda S著,颜鸣皋,刘才穆译.金属的疲劳与断裂.上海科学技术出版社,1983:46' |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|