ADSORPTION OF SODIUM OLEATE ON QUARTZ AND FELDSPAR
LIU Yachuan;GONG Huangao;ZHANG Keren;TIAN Xilin Northeast University; Shenyang Institute of Multipurpose Utilization of Mineral Resources; Chengdu
Cite this article: 

LIU Yachuan;GONG Huangao;ZHANG Keren;TIAN Xilin Northeast University; Shenyang Institute of Multipurpose Utilization of Mineral Resources; Chengdu. ADSORPTION OF SODIUM OLEATE ON QUARTZ AND FELDSPAR. Acta Metall Sin, 1993, 29(11): 49-53.

Download:  PDF(423KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The sdsorption behaviour of sodium oleate on quartz or feldspar has been ex-amined by zeta-potential and adsorbabilty measuremant, together with IR spectral analysesand flotation tests. Both electrostatic adsorption with oleate ions and physical one with oleatemolecules were occurred on quartz. While on feldspar, the chemical adsorption was con-ducted between oleate ions and Al. Thus, the adsorbability on feldspar is superior to that onquartz. The sodium cleate is able to activate feldspar flotation with amine as collector.
Key words:  feldspar      quartz      sodium oleate      adsorption      flotation     
Received:  18 November 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I11/49

1 刘亚川,龚焕高,张克仁.见:18届国际选矿会议论文集,vol.4,悉尼,澳大利亚,1993:857
2 Cookes S R B,Iwasaki I.Hyung Sup Chol.Min Eng.1959;(2) :920
3 张洪恩,刘慧纳,沈致平,魏德洲.金属矿山,1982;(11) :32
4 丘继存.东北工学院科技资料,1989
5 Lai R W. Ph. D Thesis, Berkeley, 1970
6 Fuerstenau M C, Elgillaxi D A. Trans AIME, 1966; 235: 405
[1] WANG Xuemei, YIN Zhengzheng, YU Xiaotong, ZOU Yuhong, ZENG Rongchang. Comparison of Corrosion Resistance of Phenylalanine, Methionine, and Asparagine-Induced Ca-P Coatings on AZ31 Magnesium Alloys[J]. 金属学报, 2021, 57(10): 1258-1271.
[2] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[3] CAO Fengting, WEI Jie, DONG Junhua, KE Wei, WANG Tiegang, FAN Qixiang. Corrosion Inhibition Behavior of 1-Hydroxyethylidene-1, 1-Diphosphonic Acid on 20SiMn Steel in Simulated Concrete Pore Solution Containing Cl-[J]. 金属学报, 2020, 56(6): 898-908.
[4] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[5] Mengwei CAO,Tao CAI,Xia ZHANG. Study on Amination Modification of Fe-BTC and Their Adsorption for Dyes and Heavy Metal Ions[J]. 金属学报, 2019, 55(7): 821-830.
[6] ZHOU Xiaowei,SHEN Yifu. CORROSION BEHAVIOR AND EIS STUDY OF NANOCRYSTALLINE Ni-CeO2 COATINGS IN AN ACID NaCl SOLUTION[J]. 金属学报, 2013, 49(9): 1121-1130.
[7] HE Xinkuai, HOU Bailong, JIANG Yumei, LI Chen, WU Luye. INHIBITION PROPERTY AND ADSORPTION BEHAVIOR OF IMIDAZOLE AND 2—PHENYL—2—IMIDAZOLINE ON Cu IN H2SO4 SOLUTION[J]. 金属学报, 2013, 49(8): 1017-1024.
[8] SHI Yongjuan REN Yibin ZHANG Bingchun YANG Ke. THE EFFECT OF PASSIVATION ON THE HAEMOCOMPATIBILITY OF 316L STAINLESS STEEL[J]. 金属学报, 2011, 47(12): 1575-1580.
[9] HUANG He YAN Chao LAI Xinchun LIU Tianwei ZHANG Qingyu. MOLECULAR DYNAMICS SIMULATION OF DEPOSITING LOW–ENERGY ATOM Ti ON Ti(0001) SURFACE[J]. 金属学报, 2009, 45(2): 211-216.
[10] ;. Inhibition Action and Mechanism of the Self-assembled Monolayers of 3-amino-1,2,4-triazole on Cu-Ni Alloy[J]. 金属学报, 2008, 44(2): 203-208 .
[11] . First principle study of O2 adsorption on NiTi alloy (100) surface[J]. 金属学报, 2006, 42(4): 421-425 .
[12] SUN Shuiyu;WANG Dianzuo;LI Bodan Department of Mineral Engineering; Central South University of Technology; Changsha. HYDROPHOBICITY-HYDROPHILICITY BALANCE RELATIONSHIPS FOR COLLECTORLESS FLOTATION OF SULPHIDE MINERALS[J]. 金属学报, 1993, 29(9): 53-59.
[13] REN Jun Baotou Research Institute of Rare Earth Metals; Ministry of Metallurgical Industry engineer;Baotou Research Institute of Rare Earth Metals Baotou 014010. FLOTATION BEHAVIOUR AND MECHANISM OF BASTNAESITE WITH N-HYDROXYLE PHTHALICIMIDE[J]. 金属学报, 1993, 29(6): 49-53.
No Suggested Reading articles found!