| EFFFECT OF CURRENT PULSE ON SUPERPLASTICITY AND FRACTURE BEHAVIOUR OF 2091 Al-Li ALLOY |
| LIU Zhiyi;CUI Jianzhong;BAI Guangrun Northeast University of Technology; Shenyang |
|
Cite this article:
LIU Zhiyi;CUI Jianzhong;BAI Guangrun Northeast University of Technology; Shenyang. EFFFECT OF CURRENT PULSE ON SUPERPLASTICITY AND FRACTURE BEHAVIOUR OF 2091 Al-Li ALLOY. Acta Metall Sin, 1993, 29(2): 41-44.
|
|
|
Abstract Effects of current pulse on mechanical behaviors and fracture mechanism of2091 Al-Li superplastically deformed at high strain rate have been investigated. Applying adirect current pulse makes the 2091 Al-Li alloy still with high stress-strain rate sensiitivityexponent and superplastic properties under superplastically deformed at high strain rate of10~(-2)s~(-1). SEM observation showed that the fracture for 2091 Al-Li alloy, superplastically de-formed at high strain rate by applying current pulse, transforms from intergranular tear totypical superplastic failure, i. e., fracture by formation and coalescene of cavities at particlesand boundaries.
|
|
Received: 18 February 1993
|
1 Ho P S, Kwok T. Rep Prog Phys, 1989; 52: 301 2 Hummel R E. In: Hummel R E, Huntington H B eds., Electro and Thermo-Transport in Metals and Alloys, New York: AIME, 1976: 93 3 Verbruggen A H, Griessen R, De Groot D G. J Phys F: Metal Phys, 1986; 16: 557 4 Troitskiy O A, Roshchupkin A M, Stashenko V I, Moiseyenko M M. Kalymbetov P U. Phys Met Metallogr, 1987; 61 (5) : 143 5 Sprecher A F, Mannan S L, Conrad H. Acta Metall, 1986; 34: 1145 6 Arieli A, Mukherjee A K. Mater Sci Eng, 1980; 45: 61 7 Gifkins R C. Metall Trans, 1976; 7A: 1225v |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|