Abstract Study was made of the solute content and distribution of cellular structure atdifferent growth rates in rapidly solidified Al-8wt-% Fealloy. The alloy solidified as cellularstructure with inter-cellular regions composed of many randomly oriented Al-Fe particles.At the highest growth rates, the cell-spacing exceeds the characteristic diffusion length D/vby a factor of 83. The rate of increase of the average cell composition with growth rate iscompared with that predicted by different models.
|
|
Received: 18 August 1993
|
1 Sarreal J A, Abbaschian G J. Metall Trans, 1986; 17A: 173 2 Palacio H A, Solari M, Biloni H. J Crystalgrwoth, 1985; 73: 369 3 Boettinger W J, Shechtman D, Schaefer R J Biancaniello F S. Metall Trans, 1984; 15A: 55 4 Goldstein J I, in: Goldstein J I, Joy D C eds., Introduction to Analytical Electron Microscopy, New York: Plenum, 1974; 83 5 Carrard M, Gremand M, Pieranroni M. Scrita Metall, 1991; 25: 925 6 Boettinger W J, Bendersky L A, Coriell S R, Schaefer R J, Biancaniello F S. J Crystal Grwth, 1987; 80: 17 7 Murray J L. Mater Res Soc Symp Proc, 1983; 19: 249 8 Kurz W, Fisher D J, Acta Metall, 1981; 29: 11. 9 Ungar L H, Brown R A. Phys Rev, 1985; B23: 53 10 Aziz M J. Appl Phys, 1982; 53: 1158 11 Aziz M J. Appl Phys Letters, 1983: 43: 552 12 Lipton J, Kurz W, Trivedi R. Acta Metall, 1987; 35: 957 13 Chu M G, Granger D A. Metall Trans, 1990; 21A: 205 14 Boettinger W J, Bendersky L, Early J G. Metall Trans, 1986; 17A: 781 15 汤亚力,郑州工学院硕士学位论文,1990 16 Levi C G, Metall Trans, 1988; 19A: 687 17 Burden M H, Hunt J D. J Crystal Growth, 1974; 22: 109 18 Huang S C, Glicksman M E. Acta Metall, 1981; 29: 701 19 Kurz W, Giovanola B, Trivedi R. Acta Metall, 1986; 34: 823# |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|