Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (1): 11-19    DOI:
Current Issue | Archive | Adv Search |
STRENGTHENING BEHAVIOUR OF A HIGH-TEMPERATURE Ti ALLOY CONTAINING Nd
SUN Fusheng;CAO Chunxiao;(Beijing Institute of Aeronautical Materials)(Manuscript received 15 June;1993;in revised form 24 August;1993)
Cite this article: 

SUN Fusheng;CAO Chunxiao;(Beijing Institute of Aeronautical Materials)(Manuscript received 15 June;1993;in revised form 24 August;1993). STRENGTHENING BEHAVIOUR OF A HIGH-TEMPERATURE Ti ALLOY CONTAINING Nd. Acta Metall Sin, 1994, 30(1): 11-19.

Download:  PDF(608KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Influence of Nd on microstructure,tensile properties,thermal stability and strengthening behaviour of Ti-5.5A1-4.SSn-2Zr-1Mo-0.25Si-Nd alloy was studied,Nd can not only refine the prior β grains and α plates,and especially densify dislocation network subgrain boundaries,but also improves tensile strength and thermal-stability.The strengthening of Nd is superposition of strengthening caused by grain-refinement,particularily the densifying of subgrain boundaries,and weakening caused by depletion of Sn and O2 in matrix phase.Correspondent:SUN Fusheng,senior engineer.Laboratory No.15,(Beijing Institue of Aeronautical Materials,Beijing 100095)
Key words:  TiAlSnZrMoSiNd alloy      strengthening      Nd     
Received:  18 January 1994     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I1/11

1SastrySML,PengTC,O'NealJE,TitaniumScienceandTechnology,1984;l:3972SastrySML,MeschterPJ,O'NealJE,MetallTrans,1984;15A:14513KonitzerDG,MuddleBC,FraserHL,MetallTrans,1983;14A:19794KonitzerDG,ScriptaMetall,1983;17:9635WangSH,ProcMaterResSocSymp,1984;28:367 6Bowden DM,SastrySMLet.al,TitaniumSciTech,1984;2:7837李东,刘羽寅,钛科学与工程,1987;2:498杨冠军,韩传玺.钛科学与工程,1987;2:699秦蔡庆,唐仕生.钛科学与工程,1987;3:6310陈克修,罗月新.钛科学与工程,1987;2:4211金相实验技术,清华大学教学讲义,1983年10月12孙福生,硕士学位论文,北京航空材料研究所,1988年12月13孙福生,曹春晓.材料工程,1991;3:4814MottNF,NabarroFRN,ReportofConferenceonStrengthofSolids,194815EA著,陈石卿译.钛合金金相学,北京:国防工业出版社,198616王金友,葛志明,周彦邦.航空用钛合金,上海科学技术出版社,1985:6017张树文,李永森.钛科学与工程,1987;2:4418FleischerRL.ActaMet,1963;11:20319SastrySML,MetalTrans.1984;15A:146520FelthamP.JApplphys.1968;1:30321AssbyMF,In:KelleyA,etaleds.,StrenglheningMethodsinCrvstals,JohnWiley,NewYork,1971:137.
[1] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[4] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[5] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[6] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[7] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[8] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[9] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[10] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[11] LIU Junpeng, CHEN Hao, ZHANG Chi, YANG Zhigang, ZHANG Yong, DAI Lanhong. Progress of Cryogenic Deformation and Strengthening-Toughening Mechanisms of High-Entropy Alloys[J]. 金属学报, 2023, 59(6): 727-743.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[14] FENG Li, WANG Guiping, MA Kai, YANG Weijie, AN Guosheng, LI Wensheng. Microstructure and Properties of AlCo x CrFeNiCu High-Entropy Alloy Coating Synthesized by Cold Spraying Assisted Induction Remelting[J]. 金属学报, 2023, 59(5): 703-712.
[15] XU Lei, TIAN Xiaosheng, WU Jie, LU Zhengguan, YANG Rui. Microstructure and Mechanical Properties of Inconel 718 Powder Alloy Prepared by Hot Isostatic Pressing[J]. 金属学报, 2023, 59(5): 693-702.
No Suggested Reading articles found!