| GROWTH MORPHOLOGY OF γ'-DENDRITE DURING HIGH TEMPERATURE AGEING OF Ni-BASE SUPERALLOY |
| YU Xihong;ZHANG Jinghua;HU Zhuangqi (Institute of Metal Research;Chinese Academy of Sciences; Shenyang) |
|
Cite this article:
YU Xihong;ZHANG Jinghua;HU Zhuangqi (Institute of Metal Research;Chinese Academy of Sciences; Shenyang). GROWTH MORPHOLOGY OF γ'-DENDRITE DURING HIGH TEMPERATURE AGEING OF Ni-BASE SUPERALLOY. Acta Metall Sin, 1994, 30(12): 551-554.
|
|
|
Abstract The morphology of γ' precipitate changed from cubic to flower like dendritic shape during high temperature ageing for a Rene'N4 single crystal Ni-base superalloy.The dendritic growth of γ' precipetate was of the selection area characteristic. The analysis results indicated that there was a critical growth size a* of γ' precipitate.As soon as the size of γ'was larger than the value of a * , the γ' precipitate would hollow and split by dismatch dislocation in order to match the increase of systematic energe of γ' and develop into dendrite.YU Xihong. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110015
|
|
|
| 1GabbTP,GardaJ,MminerRV.MetallTrans,1986;19A:4972Mever-ClberslebenF,GoldschmidtD,Rezai-AriaF.In:AntolovichSDetaleds.,Superalloys1992,TheMinerals,MetalsMaterialsSociety,1992:7853YeomSJ,YoonDV,HenryMF.MetallTrans,1993;24:19754HenryNF,YooVS,YoonDV,ChoiJ.metallTrans,1993;24A:17335DoiM,MiyazakiT,WakatsukiT.MaterSciEng,1985;74:1396PorterDA,EasterlingKE著.李长海,余永宁译.金属和合金中的相变.北京:冶金工业出版社,1988:1447胡汉起著.金属凝固.北京:冶金工业出版社,1985:738MiyazakiT,ImamuraH,MoriH,KozakaiT.JMaterSci,1981;16:1197 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|