APPARENT CRYSTALLIZATION KINETICS OF AMORPHOUS Fe_(80)B_(20) ALLOY
DONG Zhenfu; LU Ke; LIU Xuedong; DING Bingzhe; WEI Wenduo; WANGJingtang(State Key Laboratory of RSA; Institute of Metal Reseach; Chinese Academy of Sciences; Shenyang)
Cite this article: 

DONG Zhenfu; LU Ke; LIU Xuedong; DING Bingzhe; WEI Wenduo; WANGJingtang(State Key Laboratory of RSA; Institute of Metal Reseach; Chinese Academy of Sciences; Shenyang). APPARENT CRYSTALLIZATION KINETICS OF AMORPHOUS Fe_(80)B_(20) ALLOY. Acta Metall Sin, 1994, 30(17): 218-222.

Download:  PDF(310KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By use of a differential scanning calorimeter, the crystallization kinetics of an amorphous Fe80B20 alloy was studied. The kinetic parameters of crystallization, such as the transformed fraction x(t),the local activation energy Ec(x), and the average Avrami exponent n, were analyzed. The crystal growth in this alloy is not only interface-controlled but also diffusion-controlled.
Key words:  amorphous alloy      crystallization kinetics      interface-control      diffusion-con-trol      Fe_(80)B_(20)     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I17/218

1ChristainJW.TheThoeryofTransformationinMetalsandAlloys,1stEd.,Oxford:PergamonPress,19652卢柯,王景唐.中国科学,1992;22:A4143GreerAL.ActaMetall.1982;30:1714RanganathanS,HeimendahlMV,JMaterSci,1981;16:24015ChenHS,KirerlingLC,PoateJM,BrownWL.ApplPhysLett,1978;32:4616RosenblumMP,SpaEpenF,TurnbullD.ApplPhysLett,1980;37:1847LuK,WangJT.MaterSciEng,1991;A133:5000
[1] LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng. Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region[J]. 金属学报, 2022, 58(6): 807-815.
[2] GUO Lu, ZHU Qianke, CHEN Zhe, ZHANG Kewei, JIANG Yong. Non-Isothermal Crystallization Kinetics of Fe76Ga5Ge5B6P7Cu1 Alloy[J]. 金属学报, 2022, 58(6): 799-806.
[3] LI Jinfu, LI Wei. Structure and Glass-Forming Ability of Al-Based Amorphous Alloys[J]. 金属学报, 2022, 58(4): 457-472.
[4] ZHANG Jinyong, ZHAO Congcong, WU Yijin, CHEN Changjiu, CHEN Zheng, SHEN Baolong. Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons[J]. 金属学报, 2022, 58(2): 215-224.
[5] HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen. Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy[J]. 金属学报, 2022, 58(10): 1316-1324.
[6] LIU Riping, MA Mingzhen, ZHANG Xinyu. New Development of Research on Casting of Bulk Amorphous Alloys[J]. 金属学报, 2021, 57(4): 515-528.
[7] HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si. Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon[J]. 金属学报, 2021, 57(4): 542-552.
[8] ZHU Min, OUYANG Liuzhang. Kinetics Tuning and Electrochemical Performance of Mg-Based Hydrogen Storage Alloys[J]. 金属学报, 2021, 57(11): 1416-1428.
[9] HUANG Huogen, ZHANG Pengguo, ZHANG Pei, WANG Qinguo. Comparison of Glass Forming Ability Between U-Co and U-Fe Base Systems[J]. 金属学报, 2020, 56(6): 849-854.
[10] GENG Yaoxiang, WANG Yingmin. Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research[J]. 金属学报, 2020, 56(11): 1558-1568.
[11] XU Xiuyue, LI Yanhui, ZHANG Wei. Fabrication of Nanoporous PtRuFe by Dealloying Amorphous Fe(Pt, Ru)B Ribbons and Their Methanol Electrocatalytic Properties[J]. 金属学报, 2020, 56(10): 1393-1400.
[12] JIN Chenri, YANG Suyuan, DENG Xueyuan, WANG Yangwei, CHENG Xingwang. Effect of Nano-Crystallization on Dynamic Compressive Property of Zr-Based Amorphous Alloy[J]. 金属学报, 2019, 55(12): 1561-1568.
[13] Hongyang XU,Haibo KE,Huogen HUANG,Pei ZHANG,Pengguo ZHANG,Tianwei LIU. Nanoindentation Creep Behavior of U65Fe30Al5 Amorphous Alloy[J]. 金属学报, 2017, 53(7): 817-823.
[14] Dianguo MA,Yingmin WANG,Kunio YUBUTA,Yanhui LI,Wei ZHANG. Effect of Co Content on the Structure and Magnetic Properties of Melt-Spun Fe55-xCoxPt15B30 Alloys[J]. 金属学报, 2017, 53(5): 609-614.
[15] Huogen HUANG,Hongyang XU,Pengguo ZHANG,Yingmin WANG,Haibo KE,Pei ZHANG,Tianwei LIU. U-Cr Binary Alloys with Anomalous Glass-Forming Ability[J]. 金属学报, 2017, 53(2): 233-238.
No Suggested Reading articles found!