| MAGNETIC PROPERTIES AND HOT PLASTICITY OF HOT-PRESSING CAST PrFeB SYSTEM ALLOYS |
| ZHOU Shouzeng;DONG Qingfei;SHI Zhenghua;ZHANG Shouhua(University of Science and Technology Beijing) |
|
Cite this article:
ZHOU Shouzeng;DONG Qingfei;SHI Zhenghua;ZHANG Shouhua(University of Science and Technology Beijing). MAGNETIC PROPERTIES AND HOT PLASTICITY OF HOT-PRESSING CAST PrFeB SYSTEM ALLOYS. Acta Metall Sin, 1994, 30(20): 366-372.
|
|
|
Abstract Correlation between hot-pressing deformation and magnetic properties,such as μ_0 M_s,B_r iH_c and (B.H)_m of pr_(17)Fe_(76.5) Cu_(1.5)B_5 alloy has been studied.The μ_0M_s, B_r and (B.H)_m may be improved with the increase of strain along direction parallel to pressure applied at 973 K at hot pressing rate of 70 × 10~(10)s~(-1).The improvement of μ_0M_s relates to the decrease of contents of Pr and Cu.The iH_c increases with the fineness of grains of Pr_2Me_(14)B phase. And increase of B_r and (B H)_m is mainly dependent on the aligned factor(cosθ)p B_r= 1.2 T, iH_c= 1220 kA/ m and (B .H)_m= 260 kJ/ m3 of hot pressed magnets were obtained.
|
|
|
| 1周寿增编著.稀土永磁材料及其应用.北京:冶金工业出版社,1990:2082ShimodaT,AkiokaK,KobayashiO,YamagamiT.IEEETransMagn,1989;MAG—25:40993董清飞,北京科技大学博士学位论文,1991:1124周寿增,GrahamCDJr.金属材料研究,1989;15(1):15SchneiderG,HenigET,StadelmaierHH,PetzouG.Proc5thInterSymposiumonMagneticAnisotropyandCoercivityinRareEarth—transitionMetalAlloysBeijing,1987:3476田静华,黄毅英,梁敬魁.中国科学,1987;(2)A:159 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|