PROPOSAL OF STRUCTURE FORMATIONIN SELFPROPAGATING HIGH TEMPERATURE SYNTHESIS OF TiB_2-xAl COMPOSITES
FU Zhengyi;WANG Weimin;WANG Hao;YUAN Runzhang(Wuhan University of Technology);MUNIR;Zuhair A.(University of California;Davis; USA)
Cite this article: 

FU Zhengyi;WANG Weimin;WANG Hao;YUAN Runzhang(Wuhan University of Technology);MUNIR;Zuhair A.(University of California;Davis; USA). PROPOSAL OF STRUCTURE FORMATIONIN SELFPROPAGATING HIGH TEMPERATURE SYNTHESIS OF TiB_2-xAl COMPOSITES. Acta Metall Sin, 1994, 30(20): 373-378.

Download:  PDF(437KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Effect of of Ti or B particle size on the combustion temperature and propa gating rate in the self—propagating high temperature synthesis(SHS) process of TiB_2-xAl composites has been investigated.The size change of Al particles,which does not directly enter into the chemical reaction as Ti and B,may be much less influential to the SHS process.But the molten Al, formed during reaction, may retard the growth of TiB_2grains. Thus, the structure of SHS product can be controlled.By means of combustion front quenching (CFQ) with copper wedge, the structure formation of TiB_2-xAl composites in the SHS process was discussed
Key words:  TiB_2-xAl composite      structure formation      self—propagating high temperature synthesis     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I20/373

1傅正义,袁润章,MunirZA.金属学报,1993;29:B3342MerzhanovAG.PureApplChem,1992;64:9413RogachevAS,MukasyanAS,MerzhanovAGDoklAkadNaukSSSR,1987;297:14254FuZY,WangWM,WangH,YuanRZ.PACRIMMeetingProceed,Hawaii,USA,1993:1425YuanRZ,FuZY,YangZL,MunirZA.JMaterSynthProcess,1993;1:153
No related articles found!
No Suggested Reading articles found!