Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (20): 366-372    DOI:
Current Issue | Archive | Adv Search |
MAGNETIC PROPERTIES AND HOT PLASTICITY OF HOT-PRESSING CAST PrFeB SYSTEM ALLOYS
ZHOU Shouzeng;DONG Qingfei;SHI Zhenghua;ZHANG Shouhua(University of Science and Technology Beijing)
Cite this article: 

ZHOU Shouzeng;DONG Qingfei;SHI Zhenghua;ZHANG Shouhua(University of Science and Technology Beijing). MAGNETIC PROPERTIES AND HOT PLASTICITY OF HOT-PRESSING CAST PrFeB SYSTEM ALLOYS. Acta Metall Sin, 1994, 30(20): 366-372.

Download:  PDF(459KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Correlation between hot-pressing deformation and magnetic properties,such as μ_0 M_s,B_r iH_c and (B.H)_m of pr_(17)Fe_(76.5) Cu_(1.5)B_5 alloy has been studied.The μ_0M_s, B_r and (B.H)_m may be improved with the increase of strain along direction parallel to pressure applied at 973 K at hot pressing rate of 70 × 10~(10)s~(-1).The improvement of μ_0M_s relates to the decrease of contents of Pr and Cu.The iH_c increases with the fineness of grains of Pr_2Me_(14)B phase. And increase of B_r and (B H)_m is mainly dependent on the aligned factor(cosθ)p B_r= 1.2 T, iH_c= 1220 kA/ m and (B .H)_m= 260 kJ/ m3 of hot pressed magnets were obtained.
Key words:  PrFeB magnet      hot-deformation magnet      strain      magnetic property     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I20/366

1周寿增编著.稀土永磁材料及其应用.北京:冶金工业出版社,1990:2082ShimodaT,AkiokaK,KobayashiO,YamagamiT.IEEETransMagn,1989;MAG—25:40993董清飞,北京科技大学博士学位论文,1991:1124周寿增,GrahamCDJr.金属材料研究,1989;15(1):15SchneiderG,HenigET,StadelmaierHH,PetzouG.Proc5thInterSymposiumonMagneticAnisotropyandCoercivityinRareEarth—transitionMetalAlloysBeijing,1987:3476田静华,黄毅英,梁敬魁.中国科学,1987;(2)A:159
[1] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[2] WAN Tao, CHENG Zhao, LU Lei. Effect of Component Proportion on Mechanical Behaviors of Laminated Nanotwinned Cu[J]. 金属学报, 2023, 59(4): 567-576.
[3] WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei. Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K[J]. 金属学报, 2023, 59(2): 277-288.
[4] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[5] WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng. Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel[J]. 金属学报, 2023, 59(10): 1299-1310.
[6] WU Jin, YANG Jie, CHEN Haofeng. Fracture Behavior of DMWJ Under Different Constraints Considering Residual Stress[J]. 金属学报, 2022, 58(7): 956-964.
[7] LIU Xuxi, LIU Wenbo, LI Boyan, HE Xinfu, YANG Zhaoxi, YUN Di. Calculation of Critical Nucleus Size and Minimum Energy Path of Cu-Riched Precipitates During Radiation in Fe-Cu Alloy Using String Method[J]. 金属学报, 2022, 58(7): 943-955.
[8] REN Shihao, LIU Yongli, MENG Fanshun, QI Yang. Strain-Engineered Semiconductor to Semimetallic Transition and Its Mechanism in Bi(111) Film[J]. 金属学报, 2022, 58(7): 911-920.
[9] GAO Yubi, DING Yutian, LI Haifeng, DONG Hongbiao, ZHANG Ruiyao, LI Jun, LUO Quanshun. Effect of Deformation Rate on the Elastic-Plastic Deformation Behavior of GH3625 Alloy[J]. 金属学报, 2022, 58(5): 695-708.
[10] CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng. Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact[J]. 金属学报, 2022, 58(5): 660-672.
[11] GUO Xiangru, SHEN Junjie. Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects[J]. 金属学报, 2022, 58(3): 375-384.
[12] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[13] GUO Haohan, YANG Jie, LIU Fang, LU Rongsheng. Constraint Related Fatigue Crack Initiation Life of GH4169 Superalloy[J]. 金属学报, 2022, 58(12): 1633-1644.
[14] ZHAO Yonghao, MAO Qingzhong. Toughening of Nanostructured Metals[J]. 金属学报, 2022, 58(11): 1385-1398.
[15] WU Xiaolei, ZHU Yuntian. Heterostructured Metallic Materials: Plastic Deformation and Strain Hardening[J]. 金属学报, 2022, 58(11): 1349-1359.
No Suggested Reading articles found!