| DETERMINATION OF FATIGUE RELIABILITY UNDER COMPLEX LOADING |
| HAN Yumei; HAN Enhou;KE Wei (State Key Laboratory for Corrosion Science;Institute of Corrosion and Protection of Metals; Chinese Aeademy of Sciences;Shenyang)(Manuscript received 4 June; 1992) |
|
Cite this article:
HAN Yumei; HAN Enhou;KE Wei (State Key Laboratory for Corrosion Science;Institute of Corrosion and Protection of Metals; Chinese Aeademy of Sciences;Shenyang)(Manuscript received 4 June; 1992). DETERMINATION OF FATIGUE RELIABILITY UNDER COMPLEX LOADING. Acta Metall Sin, 1994, 30(4): 170-175.
|
|
|
Abstract A new non-linear accumulate damage model was derived from the concept of equal failure probabilities under different stress levels. Based on this model,a method of calculating fatigue reliability under complex loading was obtained when the fatigue life is obeying logical normal distribution. At last, the calculating formulas were discussed when the P-S-N curve is described as a power function or an exponential function.Correspondent: HAN Yumei, research assistant, Institute of Corrosion and Protection of Metals, Chinese Academy of Sciences, Shenyang 110015
|
|
Received: 18 April 1994
|
| 1谢里阳.机械工程学报,1987;23(2):102曾春华,邹十践.疲劳分析方法及应用.北京:国防工业出版社,1991:263CepeHCeHCB,KoraeBBⅡ,PM著,汪一麟译.机械零件的承载能力和强度计算.北京:机械工业出版社,1984:2284徐灏.疲劳强度设计.北京:机械工业出版社,1981:475徐灏.机械强度的可靠性设计.北京:机械工业出版社,1984:2256高镇同.疲劳应用统计学.北京:国防工业出版社,1986:3717MincerMA.JApplMechASMETrans,1945;9:A1598MacroSM,StarkeyWL.ASMETrans,1954;76:627 9 WeibullW.FatigueTestingandAnalysisofResults.NewYork:MacmillanCompany,1961:12610TanakaT.ProceedingsofInterConfonFatigue,Birmingham:MaterialsandComponentEngineeringPublicationLtd.,1984:211FuHuimin,GaoZhentong.ProceedingsofInterConfonStrucSafetyandReliability.1985:76512韩恩厚,韩玉梅,柯伟,自然科学进展,1994待发表13楼志文.损伤力学基础,西安交通大学出版社,1991:9814CioclovD.Proc4thConfonWeldingandMetalTesting,Tokyo:PergamonPress,Timisoara,1969:37115HashinZ,SubramanyanD.FatigueEngMaterStruct,1980;2:345 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|