| STRESS RELIEF AND MAGNETISM OPTIMIZATION OF AMORPHOUS Fe_(79)B_(16)Si_5 ALLOY |
| CHE Hiaozhou(Shanghai Jiaotong University; Shanghai 200030)(Manuscript received 1994-12-09; in revised forrn 1995-03-27) |
|
Cite this article:
CHE Hiaozhou(Shanghai Jiaotong University; Shanghai 200030)(Manuscript received 1994-12-09; in revised forrn 1995-03-27). STRESS RELIEF AND MAGNETISM OPTIMIZATION OF AMORPHOUS Fe_(79)B_(16)Si_5 ALLOY. Acta Metall Sin, 1995, 31(21): 418-422.
|
|
|
Abstract The correlation between the stress relief and magnetism optimization of amorphous Fe79B16Si5 alloy during annealing process has been analyzed. After annealing,the saturation induction Bs and maximum permeabilityμm of as-quenched amorphous alloy increase by 72% and 22 times, concurrently with the reduction of coercive force Hc and power loss P(0.3 T, 10 kHz) by 86% and 83%, respectively. These changes during the annealing process are primarily due to the effective removal of the stress-induced anistropy.Correspondent: (CHE Hiaozhou, postdoctoral, Departinent of Materials Scicnce, Shanghai Jiaotong University, Shanghai 200030)
|
|
|
| 1林肇华,戴道生,物理学报,1982;31:8712FujimoriH.In:LubroskyFEed.,AmorphousMetallicAlloys,London:Butterworth&CoLtd,1983:3003FujimoriH.In:SteebS,WarlimontHeds.,RapidlyQuenchedMetals,Amsterdam:ElsevierSci-encePublishersBV,1985:11014LuborsiyFE.IEEETransMagnMAG-11,1975;6:16445SongJS,ParkJW,ImHB.ScriptaMetall,1991,25(1):736HuangDR,LiJCM.ScriptaMetall,1990;24:1137 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|