Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (4): 145-150    DOI:
Current Issue | Archive | Adv Search |
THICKENING OF BAINITE AND EQUILIBRIUM PHASE AND SHEAR STRESS FIELD ACCOMPANYING BAINITE GROWTH IN A Cu-Zn ALLOY
YANG Yanqing; MENG Xiangkang; JIA Husheng; KANG Mokuang; MA Qin(Northweslern Polytechnical University; Xi'an 710072)
Cite this article: 

YANG Yanqing; MENG Xiangkang; JIA Husheng; KANG Mokuang; MA Qin(Northweslern Polytechnical University; Xi'an 710072). THICKENING OF BAINITE AND EQUILIBRIUM PHASE AND SHEAR STRESS FIELD ACCOMPANYING BAINITE GROWTH IN A Cu-Zn ALLOY. Acta Metall Sin, 1995, 31(4): 145-150.

Download:  PDF(406KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  篢he thickening of bainite and equilibrium phase in a Cu-Zn alloy was in situ observed by means of TEM at heating stage. The thickening kinetics of both bainite and equilibrium phase is inconsistent with diffusional ledge mechanism. There is an obvious shear feature during bainite thickening.
Key words:  Cu-Zn alloy      bainite      in situ observation      thickening kinetics      shear     
Received:  18 April 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I4/145

1杨正清,刘东慧,康沫狂,孙原.金属学报,1992;28:A952MengXK,KangMK,YangYQ,LiuDH.MetallTrans,1994;25A:26013方鸿生,李春明,王家军.金属学报,1993;29:A3834AaronsonHl.DecompositionofAustenitebyDiffusionalProcesses.Interscience,NY,1962:3875YangYQ,KangMK,HanD,ZhouZG,WnagJE.In:ShiCX,LiHD,ScottAeds.,Proc.lstPacificRimInt.Conf.onAdvancedMaterialsandProcessing,TMSPress,1993:4696AaronsonHI,LaidC.TransTMS-AIME,1968;242:14377IvantsovGP.AkadDokNaukSSSR.1947:58:5678BrandesEA.SmithellsMetalsReferenceBook.6thed.,London:Batterworth.1983:5839ZenerC.J ApplPhys1949;20:95010FrankFCProcRSoc.l950:A201:113711KosticMM,HawboltEB,BrownLC.MetallTrans.1976:7A:164312FlewittPEJ.TownerJM.JInstMet.1967;95:27313孟祥康,康沫狂.金属学报、1993;29:A35914YangYQ,ZhangZF.ShenHM,WangYN、ZhaoXN.HongJM、KangMK.MaterLett.1993;17:36915TakezawaKSatoS.ProcICOMAT-86,Nara,1986:631
[1] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[2] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[3] ZHU Dongming, HE Jiangli, SHI Genhao, WANG Qingfeng. Effect of Welding Heat Input on Microstructure and Impact Toughness of the Simulated CGHAZ in Q500qE Steel[J]. 金属学报, 2022, 58(12): 1581-1588.
[4] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[5] CHEN Wei, ZHANG Huan, MU Juan, ZHU Zhengwang, ZHANG Haifeng, WANG Yandong. Effects of Microstructure and Strain Rate on Dynamic Mechanical Properties and Adiabatic Shear Band of TC4 Alloy[J]. 金属学报, 2022, 58(10): 1271-1280.
[6] JIANG Zhonghua, DU Junyi, WANG Pei, ZHENG Jianneng, LI Dianzhong, LI Yiyi. Mechanism of Improving the Impact Toughness of SA508-3 Steel Used for Nuclear Power by Pre-Transformation of M-A Islands[J]. 金属学报, 2021, 57(7): 891-902.
[7] QU Ruitao, WANG Xiaodi, WU Shaojie, ZHANG Zhefeng. Research Progress in Shear Banding Deformation and Fracture Mechanisms of Metallic Glasses[J]. 金属学报, 2021, 57(4): 453-472.
[8] JIANG Minqiang, GAO Yang. Structural Rejuvenation of Metallic Glasses and Its Effect on Mechanical Behaviors[J]. 金属学报, 2021, 57(4): 425-438.
[9] ZHANG Nizhen, MA Xindi, GENG Chuan, MU Yongkun, SUN Kang, JIA Yandong, HUANG Bo, WANG Gang. Effect of Adding Ag on the Nanoindentation Behavior of Cu-Zr-Al-Based Metallic Glass[J]. 金属学报, 2021, 57(4): 567-574.
[10] GUAN Pengfei, SUN Shengjun. Atomic-Level Study in the Structure and Its Instability of Metallic Glasses[J]. 金属学报, 2021, 57(4): 501-514.
[11] ZHU Liang, GUO Mingxing, YUAN Bo, ZHUANG Linzhong, ZHANG Jishan. Effect of Ageing Routes on Precipitation Behaviors of Al-0.7Mg-0.5Si-0.2Cu-0.5Zn Alloy[J]. 金属学报, 2020, 56(7): 997-1006.
[12] XIAO Hong,XU Pengpeng,QI Zichen,WU Zonghe,ZHAO Yunpeng. Preparation of Steel/Aluminum Laminated Composites by Differential Temperature Rolling with Induction Heating[J]. 金属学报, 2020, 56(2): 231-239.
[13] Jialin ZHU,Shifeng LIU,Yu CAO,Yahui LIU,Chao DENG,Qing LIU. Effect of Cross Rolling Cycle on the Deformed and Recrystallized Gradient in High-Purity Tantalum Plate[J]. 金属学报, 2019, 55(8): 1019-1033.
[14] Hua JI,Yunlai DENG,Hongyong XU,Weiqiang GUO,Jianfeng DENG,Shitong FAN. The Influence of Welding Line Energy on the Microstructure and Property of CMT Overlap Joint of 5182-Oand HC260YD+Z[J]. 金属学报, 2019, 55(3): 376-388.
[15] CAO Lihua, CHEN Yinbo, SHI Qiyuan, YUAN Jie, LIU Zhiquan. Effects of Alloy Elements on the Interfacial Microstructure and Shear Strength of Sn-Ag-Cu Solder[J]. 金属学报, 2019, 55(12): 1606-1614.
No Suggested Reading articles found!