Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (4): 151-155    DOI:
Current Issue | Archive | Adv Search |
PHASE TRANSFORMATIONS IN Fe-28A1 ALLOYS
DU Guowei;W ANG Zheng;XIAO Jimei (University of Science and Technology Beijing; 100083)
Cite this article: 

DU Guowei;W ANG Zheng;XIAO Jimei (University of Science and Technology Beijing; 100083). PHASE TRANSFORMATIONS IN Fe-28A1 ALLOYS. Acta Metall Sin, 1995, 31(4): 151-155.

Download:  PDF(378KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  篢he phase transformations in the Fe-28AI alloys with or without addition of Cr were studied by means of electron microscopy and X-ray diffraction techniques. The B2 antiphase domains (APD) has already been formed during quenching process from 1080℃.The Fe-enriched a-phase may precipitate along the grain boundaries in the alloys when cooling slowly through temperature range of just B2-phase occurred. In the Fe-28A1-5Cr alloy. the fine CrN-phase may also precipitate. The B2→D03 transformation was found to be a slow process in the sheet specimens.
Key words:  Fe_3A1      B2 antiphase domain      D0_3antiphase domain      α-phase      CrN precipitate     
Received:  18 April 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I4/151

1AllenSA,CahnJA.ActaMetall,1976:24:4252SauthoffG.ZMetallk,1986;10:6543殷为民,郭建亭,胡壮麒,材料科学进展,1992;4:2774MckameyC.G.HortonJA,LiuCT.JMaterRes.1989:4:11565王政,杜国维,肖纪美.理学X射线衍射仪用户协会论文选集,19946.CahnRW,HassenP.PhysicalMetallurgy.3rd.Amsterdam:North-Holland.1983:4327OkamotoH.BeckPaulA.MetallTrans,1971:2:5698
[1] GAO Yan;LI Dejun;CAO Zhiben Dalian Institute of Technology; Liaoning. EFFECTS OF DEFORMATION ON MICROSTRUCTURE AND σ-PHASE FORMATION IN Cr_(25)Ni_(20) STAINLESS STEEL[J]. 金属学报, 1988, 24(5): 376-378.