Acta Metall Sin  2026, Vol. 62 Issue (6): 993-1008    DOI: 10.11900/0412.1961.2025.00387
Overview Current Issue | Archive | Adv Search |
Tuning Local Chemical Order and Multiple Properties in High-Entropy Films via Interstitial Filling with Non-Metallic Small Atoms: A Percolation- Theory-Based Perspective
LI Xiaona1(), WANG Xiao1, WANG Dazhe2, ZHENG Yuehong3, DONG Chuang1,4, P. K. LIAW5
1 Key Laboratory of Materials Modification by Laser, Ion and Electron Beams (Ministry of Education), School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
2 Leicester International Institute, Dalian University of Technology, Panjin 124221, China
3 State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China
4 School of Materials Science and Engineering, Dalian Jiaotong University, Dalian 116028, China
5 Department of Materials Science and Engineering, The University of Tennessee, Knoxville, Tennessee 37996, USA
Cite this article: 

LI Xiaona, WANG Xiao, WANG Dazhe, ZHENG Yuehong, DONG Chuang, P. K. LIAW. Tuning Local Chemical Order and Multiple Properties in High-Entropy Films via Interstitial Filling with Non-Metallic Small Atoms: A Percolation- Theory-Based Perspective. Acta Metall Sin, 2026, 62(6): 993-1008.

Download:  HTML  PDF(2864KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Interstitial filling with non-metallic small atoms (SAs) provides a crucial pathway for tuning the structure and properties of high-entropy films. Owing to their small atomic size, SAs preferentially occupy interstitial sites and, through their distinct chemical interactions with constituent metallic elements, induce changes in local chemical order (LCO). With increasing SAs content, high-entropy films exhibit a progressive transition from disordered interstitial solid solutions to locally ordered states, and eventually to ordered crystalline or amorphous structures, accompanied by pronounced property variations. Accordingly, this review focuses on high-entropy films and systematically summarizes the effects of SAs filling on crystal structure, LCO, and mechanical, magnetic, and electrical properties. A percolation-theory framework is introduced, in which different LCO types are treated as percolating units with characteristic properties, thereby establishing intrinsic correlations between LCO content and macroscopic property evolution. On this basis, the commonalities and distinctions among different SAs in regulating material properties are summarized and compared. Finally, an outlook on future research directions is provided.

Key words:  high-entropy film      crystal structure      local chemical ordering      percolation theory      hardness      magnetic property      electrical resistivity     
Received:  24 November 2025     
ZTFLH:  TG139  
Fund: Sino-Russian Cooperative Research Project Funded by the National Natural Science Foundation of China(W2412042);Fundamental Research Funds for the Central Universities(DUT24LAB116)
Corresponding Authors:  LI Xiaona, professor, Tel: (0411)84708389, E-mail: lixiaona@dlut.edu.cn

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2025.00387     OR     https://www.ams.org.cn/EN/Y2026/V62/I6/993

Fig.1  Common types of crystal structures after non-metallic small atoms (SAs) interstitial filling: rock-salt structure, fluorite structure, spinel structure, and perovskite structure
Fig.2  Schematics of typical diffraction features in reciprocal space for local chemical ordering (LCO) at different length scales in an fcc alloy
(a) diffuse disk corresponding to short-range order (SRO)[12]
(b) weak diffraction spot corresponding to medium-range order (MRO)[13]
(c) bright diffraction spot corresponding to long-range order (LRO)[14]
Fig.3  Schematic illustration of the polyamorphous transition mechanism in high-entropy metallic glasses[18]: two distinct types of SRO exist in the liquid state; rapid quenching forms a high energy glassy state I, which transforms into a low energy glassy state II upon heating as SRO units interconnect to form MRO; slow cooling leads to the formation of a stable two-phase crystalline structure (Red and blue circles represent the two different types of SRO structures)
Structurezvpcsitepcbondz·pcbondv·pcsite
fcc120.74050.1980.1191.430.147
bcc80.68020.2450.1791.430.167
Simple cubic60.52360.3110.2471.480.163
Diamond40.34010.4280.3881.550.146
Table 1  Relationships among percolation threshold, coordination number (z), and filling factor (v) in different crystal lattice systems[33]
Fig.4  Atom probe tomography elemental mapping of (TiNbZr)86O12C1N1 film (a), one-dimensional compositional profile along the arrow direction in Fig.4a (b), engineering stress-strain curves from microcompression testing (c), and load-displacement curves measured via cantilever beam bending (d)[45] (Inset in Fig.4c shows the O-12 massive interstitial solid solution (MISS) alloy pillar prior to compression; inset in Fig.4d shows the position of the diamond indenter tool, deforming the O-12 cantilever)
Fig.5  Ashby-type maps of hardness (H) vs Young's modulus (E) for high-entropy films incorporating different SAs (Data are sourced from: high-entropy films without SAs[54-56], N-containing high-entropy films[46,48,49,52,53,57-65], C-containing high-entropy films[66-69], O-containing high-entropy films[47,70,71], and high-entropy films with combined C and N additions[72,73]. Content here refers to atomic percentage)
(a) relationship of H / E (b) relationship of H3/E2
Fig.6  Diverse magnetic exchange interactions between different elements in the La(Cr0.2Mn0.2Fe0.2Co0.2Ni0.2)O3 (L5BO) film (a), magnetic hysteresis loops of the L5BO film (b), and exchange bias in the L5BO/LSMO multilayer on STO (001) (c)[88] (FM—ferromagnetic; AFM—antiferromagnetic; ZFC—zero field cooling; T—temperature; Mpin and Mrot—pinned and rotated uncompensated magnetizations, respectively; LSMO—La0.7Sr0.3MnO3; STO—SrTiO3)
Fig.7  Magnetic hysteresis loops and the variation of exchange bias field in La(Cr0.2Mn0.2Fe0.2Co0.2Ni0.2)O3 films with different Mn contents (a-c); and corresponding Monte Carlo simulation results, showing the evolution of percolating networks for FM (red) and AFM (blue) exchange interactions, where the color depth represents the magnetic exchange interaction strength (d-f)[79] (M—magnetization, μB—Bohr magneton per unit cell, FC—field cooling, μ0—vacuum permeability, H—magnetic field intensity)
Fig.8  Effects of N and O contents on the electrical resistivity of high-entropy films (Data in Fig.8a are sourced from Refs.[58,92,93] and data in Fig.8b from Refs.[47,94])
(a) dependence of resistivity on N content (b) dependence of resistivity on O content
Fig.9  Schematic of the stoichiometric (CoCrFeNi)O crystal structure (a)[94], fcc stacking configuration of [O-M6] and [□-M6] (□ represents vacancy) octahedrons in space (b)[94], and octahedral equivalence in the classic two-sphere percolation model (c)[33]
[1] Gao T C, Gao J B, Yang S L, et al. Data-driven design of novel lightweight refractory high-entropy alloys with superb hardness and corrosion resistance[J]. npj Comput. Mater., 2024, 10: 256
doi: 10.1038/s41524-024-01457-6
[2] Li S, Hou X T, Wang X X, et al. Weldability of high entropy alloys: Microstructure, mechanical property, and corrosion resistance[J]. J. Manuf. Processes, 2023, 99: 209
doi: 10.1016/j.jmapro.2023.05.049
[3] Zhu C H, Xu L J, Liu M J, et al. A review on improving mechanical properties of high entropy alloy: Interstitial atom doping[J]. J. Mater. Res. Technol., 2023, 24: 7832
doi: 10.1016/j.jmrt.2023.05.002
[4] Yu Q, Qiu S, Jiao Z B. Atomic-scale understanding of interstitial-strengthened high-entropy alloys[J]. Rare Met., 2025, 44: 6002
doi: 10.1007/s12598-025-03358-z
[5] Yang Z, Xiang X L, Yang J, et al. High-entropy oxides as energy materials: From complexity to rational design[J]. Mater. Futures, 2024, 3: 042103
[6] Salian A, Mandal S. Review on the deposition, structure and properties of high entropy oxide films: Current and future perspectives[J]. Bull. Mater. Sci., 2022, 45: 49
doi: 10.1007/s12034-021-02617-w
[7] Sharma Y, Mazza A R, Musico B L, et al. Magnetic texture in insulating single crystal high entropy oxide spinel films[J]. ACS Appl. Mater. Interfaces, 2021, 13: 17971
doi: 10.1021/acsami.1c01344
[8] Sharma Y, Zheng Q, Mazza A R, et al. Magnetic anisotropy in single-crystal high-entropy perovskite oxide La(Cr0.2 Mn0.2Fe0.2Co0.2Ni0.2)O3 films[J]. Phys. Rev. Mater., 2020, 4: 014404
[9] Inoue A, Shibata T, Zhang T. Effect of additional elements on glass transition behavior and glass formation tendency of Zr-Al-Cu-Ni alloys[J]. Mater. Trans., JIM, 1995, 36: 1420
[10] An Z B, Yang T, Shi C J, et al. Negative enthalpy alloys and local chemical ordering: A concept and route leading to synergy of strength and ductility[J]. Natl. Sci. Rev., 2024, 11: nwae026
[11] Wu X L. Chemical short-range orders in high-/medium-entropy alloys[J]. J. Mater. Sci. Technol., 2023, 147: 189
doi: 10.1016/j.jmst.2022.10.070
[12] Chen X F, Wang Q, Cheng Z Y, et al. Direct observation of chemical short-range order in a medium-entropy alloy[J]. Nature, 2021, 592: 712
doi: 10.1038/s41586-021-03428-z
[13] Wang J, Jiang P, Yuan F P, et al. Chemical medium-range order in a medium-entropy alloy[J]. Nat. Commun., 2022, 13: 1021
doi: 10.1038/s41467-022-28687-w pmid: 35197473
[14] Dasari S, Jagetia A, Sharma A, et al. Tuning the degree of chemical ordering in the solid solution of a complex concentrated alloy and its impact on mechanical properties[J]. Acta Mater., 2021, 212: 116938
doi: 10.1016/j.actamat.2021.116938
[15] Ding Q Q, Zhang Y, Chen X, et al. Tuning element distribution, structure and properties by composition in high-entropy alloys[J]. Nature, 2019, 574: 223
doi: 10.1038/s41586-019-1617-1
[16] Ying H Q, Liu S N, Wu Z D, et al. Phase selection rule of high-entropy metallic glasses with different short-to-medium-range orders[J]. Rare Met., 2022, 41: 2021
doi: 10.1007/s12598-022-01973-8
[17] Bonfanti S, Guerra R, Alvarez-Donado R, et al. Quasilocalized modes in crystalline and partially crystalline high-entropy alloys[J]. Phys. Rev. Res., 2024, 6: 013146
[18] Yang Q, Yang X M, Zhang T, et al. Structure and entropy control of polyamorphous transition in high-entropy metallic glasses[J]. Acta Mater., 2024, 266: 119701
doi: 10.1016/j.actamat.2024.119701
[19] Luan H W, Zhang X, Ding H Y, et al. High-entropy induced a glass-to-glass transition in a metallic glass[J]. Nat. Commun., 2022, 13: 2183
doi: 10.1038/s41467-022-29789-1 pmid: 35449135
[20] Islam M, Young Kim J, Yoo G H, et al. In-depth analysis of structural heterogeneity in high entropy bulk metallic glasses using 4D-STEM[J]. Microsc. Microanal., 2024, 30: ozae044.668
[21] Zhang X, Luan H, Lou H, et al. Highly variable chemical short-range order in a high-entropy metallic glass[J]. Mater. Today Phys., 2022, 27: 100799
[22] Luo S F, Khong J C, Huang S, et al. Revealing in situ stress-induced short- and medium-range atomic structure evolution in a multicomponent metallic glassy alloy[J]. Acta Mater., 2024, 272: 119917
doi: 10.1016/j.actamat.2024.119917
[23] Takeuchi A, Inoue A. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element[J]. Mater. Trans., 2005, 46: 2817
doi: 10.2320/matertrans.46.2817
[24] Allred A L. Electronegativity values from thermochemical data[J]. J. Inorg. Nucl. Chem., 1961, 17: 215
doi: 10.1016/0022-1902(61)80142-5
[25] Wang Y H, Jiao M Y, Wu Y, et al. Enhancing properties of high-entropy alloys via manipulation of local chemical ordering[J]. J. Mater. Sci. Technol., 2024, 180: 23
doi: 10.1016/j.jmst.2023.10.003
[26] He Z F, Guo Y X, Sun L F, et al. Interstitial-driven local chemical order enables ultrastrong face-centered cubic multicomponent alloys[J]. Acta Mater., 2023, 243: 118495
doi: 10.1016/j.actamat.2022.118495
[27] Lei Z F, Liu X J, Wu Y, et al. Enhanced strength and ductility in a high-entropy alloy via ordered oxygen complexes[J]. Nature, 2018, 563: 546
doi: 10.1038/s41586-018-0685-y
[28] Zhao D D, Yang Q, Wang D W, et al. Ordered nitrogen complexes overcoming strength-ductility trade-off in an additively manufactured high-entropy alloy[J]. Virtual Phys. Prototyping, 2020, 15: 532
doi: 10.1080/17452759.2020.1840783
[29] Jiao M Y, Lei Z F, Wu Y, et al. Manipulating the ordered oxygen complexes to achieve high strength and ductility in medium-entropy alloys[J]. Nat. Commun., 2023, 14: 806
doi: 10.1038/s41467-023-36319-0 pmid: 36781880
[30] Wang Q, Wang Z H, Zhang Q X, et al. Achieving high damping capacity in oxygen-enhanced BCC Zr-Hf-Ti-Nb multi-principal-element alloys with low Young's modulus[J]. Adv. Sci., 2025, 12: 2501068
[31] Shi L X, Shao Y, Fan Z Y, et al. Connecting the composition, structure, and magnetic property in high-entropy metallic glasses[J]. Acta Mater., 2023, 254: 118983
doi: 10.1016/j.actamat.2023.118983
[32] Wu Y, Cao D, Yao Y L, et al. Substantially enhanced plasticity of bulk metallic glasses by densifying local atomic packing[J]. Nat. Commun., 2021, 12: 6582
doi: 10.1038/s41467-021-26858-9 pmid: 34772939
[33] Zallen R. The Physics of Amorphous Solids[M]. New York: John Wiley & Sons, Inc, 1998: 135
[34] Stauffer D, Aharony A. Introduction to Percolation Theory[M]. 2nd Ed., London: Taylor & Francis, 2003: 15
[35] Scher H, Zallen R. Critical density in percolation processes[J]. J. Chem. Phys., 1970, 53: 3759
doi: 10.1063/1.1674565
[36] Rost C M, Sachet E, Borman T, et al. Entropy-stabilized oxides[J]. Nat. Commun., 2015, 6: 8485
doi: 10.1038/ncomms9485 pmid: 26415623
[37] Takeuchi A, Yubuta K, Wada T. Critically percolated states in high-entropy alloys with exact equi-atomicity[J]. Mater. Trans., 2019, 60: 330
doi: 10.2320/matertrans.M2018216
[38] Takeuchi A, Wada T. Os-free Fe12Ir20Re20Rh20Ru28 high-entropy alloy with single hcp structure including Fe from late transition metals[J]. Mater. Trans., 2022, 63: 7
doi: 10.2320/matertrans.MT-M2021150
[39] Lun Z, Ouyang B, Kwon D H, et al. Cation-disordered rocksalt-type high-entropy cathodes for Li-ion batteries[J]. Nat. Mater., 2021, 20: 214
doi: 10.1038/s41563-020-00816-0 pmid: 33046857
[40] Kim H K, Ahn J P, Lee B J, et al. Role of atomic-scale chemical heterogeneities in improving the plasticity of Cu-Zr-Ag bulk amorphous alloys[J]. Acta Mater., 2018, 157: 209
doi: 10.1016/j.actamat.2018.07.040
[41] Hasmy A, Ispas S, Hehlen B. Percolation transitions in compressed SiO2 glasses[J]. Nature, 2021, 599: 62
doi: 10.1038/s41586-021-03918-0
[42] Mora-Barzaga G, Urbassek H M, Deluigi O R, et al. Chemical short-range order increases the phonon heat conductivity in a refractory high-entropy alloy[J]. Sci. Rep., 2024, 14: 20628
doi: 10.1038/s41598-024-70500-9 pmid: 39232091
[43] Kirnbauer A, Spadt C, Koller C M, et al. High-entropy oxide thin films based on Al-Cr-Nb-Ta-Ti[J]. Vacuum, 2019, 168: 108850
doi: 10.1016/j.vacuum.2019.108850
[44] Fritze S, Malinovskis P, Riekehr L, et al. Hard and crack resistant carbon supersaturated refractory nanostructured multicomponent coatings[J]. Sci. Rep., 2018, 8: 14508
doi: 10.1038/s41598-018-32932-y pmid: 30266967
[45] Liu C, Lu W J, Xia W Z, et al. Massive interstitial solid solution alloys achieve near-theoretical strength[J]. Nat. Commun., 2022, 13: 1102
doi: 10.1038/s41467-022-28706-w pmid: 35232964
[46] Yan X H, Zhu B H, Zhang Y, et al. Phase formation and unusual interstitial solid-solution strengthening behavior of (CoCrFeMnNi)Nx high-entropy ceramic films[J]. Surf. Coat. Technol., 2024, 477: 130392
doi: 10.1016/j.surfcoat.2024.130392
[47] Bi L X, Li X N, Li Z M, et al. Performance and local structure evolution of NbMoTaWV entropy-stabilized oxide thin films with variable oxygen content[J]. Surf. Coat. Technol., 2020, 402: 126326
doi: 10.1016/j.surfcoat.2020.126326
[48] Li H, Jiang N, Li J L, et al. Hard and tough (NbTaMoW)Nx high entropy nitride films with sub-stoichiometric nitrogen[J]. J. Alloys Compd., 2021, 889: 161713
doi: 10.1016/j.jallcom.2021.161713
[49] Li Y T, Jiang X, Wang X T, et al. Integration of hardness and toughness in (CuNiTiNbCr)Nx high entropy films through nitrogen-induced nanocomposite structure[J]. Scr. Mater., 2024, 238: 115763
doi: 10.1016/j.scriptamat.2023.115763
[50] Liu W, Wang C T, Zhao S C, et al. Enhancing wear resistance: In-situ ceramic phase precipitation for strengthening and toughening FeCoNiCrNx high-entropy alloy films[J]. Surf. Coat. Technol., 2024, 478: 130466
doi: 10.1016/j.surfcoat.2024.130466
[51] Scavini M, Coduri M, Allieta M, et al. Percolating hierarchical defect structures drive phase transformation in Ce1-xGdxO2-x/2: A total scattering study[J]. IUCrJ, 2015, 2: 511
doi: 10.1107/S2052252515011641 pmid: 26306193
[52] Sha C H, Zhou Z F, Xie Z H, et al. FeMnNiCoCr-based high entropy alloy coatings: Effect of nitrogen additions on microstructural development, mechanical properties and tribological performance[J]. Appl. Surf. Sci., 2020, 507: 145101
doi: 10.1016/j.apsusc.2019.145101
[53] Chen Y J, Ma J S, Lin Y C, et al. Interstitial engineering enabling superior mechanical properties of nitrogen-supersaturated Fe50Mn30-Co10Cr10 high-entropy alloys[J]. Acta Mater., 2024, 277: 120214
doi: 10.1016/j.actamat.2024.120214
[54] Sha C H, Zhou Z F, Xie Z H, et al. Extremely hard, α-Mn type high entropy alloy coatings[J]. Scr. Mater., 2020, 178: 477
doi: 10.1016/j.scriptamat.2019.12.029
[55] Sha C H, Zhou Z F, Xie Z H, et al. High entropy alloy FeMnNiCoCr coatings: Enhanced hardness and damage-tolerance through a dual-phase structure and nanotwins[J]. Surf. Coat. Technol., 2020, 385: 125435
doi: 10.1016/j.surfcoat.2020.125435
[56] Feng X B, Zhang J Y, Wang Y Q, et al. Size effects on the mechanical properties of nanocrystalline NbMoTaW refractory high entropy alloy thin films[J]. Int. J. Plast., 2017, 95: 264
doi: 10.1016/j.ijplas.2017.04.013
[57] Zhao Y M, Chen S N, Chen Y J, et al. Super-hard and anti-corrosion (AlCrMoSiTi)Nx high entropy nitride coatings by multi-arc cathodic vacuum magnetic filtration deposition[J]. Vacuum, 2022, 195: 110685
doi: 10.1016/j.vacuum.2021.110685
[58] Wang X, Li X N, Li Z M, et al. Utilizing cluster percolation theory to analyze electrical resistivity jumps in high-entropy alloy thin films containing small atoms[J]. Scr. Mater., 2024, 238: 115727
doi: 10.1016/j.scriptamat.2023.115727
[59] Zhang F Y, Ma H L, Zhao R B, et al. Microstructure, mechanical and corrosion performance of magnetron sputtered (Al0.5CoCrFeNi)Nx high-entropy alloy nitride films[J]. J. Alloys Compd., 2023, 968: 172158
doi: 10.1016/j.jallcom.2023.172158
[60] Lin Y C, Hsu S Y, Lai Y T, et al. Effect of the N2/(Ar + N2) ratio on mechanical properties of high entropy nitride (Cr0.35Al0.25Nb0.12Si0.08-V0.20)Nx films[J]. Mater. Chem. Phys., 2021, 274: 125195
doi: 10.1016/j.matchemphys.2021.125195
[61] Zhang C X, Lu X L, Wang C, et al. Tailoring the microstructure, mechanical and tribocorrosion performance of (CrNbTiAlV)Nx high-entropy nitride films by controlling nitrogen flow[J]. J. Mater. Sci. Technol., 2022, 107: 172
doi: 10.1016/j.jmst.2021.08.032
[62] Chen L Q, Li W, Liu P, et al. Microstructure and mechanical properties of (AlCrTiZrV)Nx high-entropy alloy nitride films by reactive magnetron sputtering[J]. Vacuum, 2020, 181: 109706
doi: 10.1016/j.vacuum.2020.109706
[63] El Garah M, Touaibia D E, Achache S, et al. Effect of nitrogen content on structural and mechanical properties of AlTiZrTaHf(-N) high entropy films deposited by reactive magnetron sputtering[J]. Surf. Coat. Technol., 2022, 432: 128051
doi: 10.1016/j.surfcoat.2021.128051
[64] Cui P P, Li W, Liu P, et al. Effects of nitrogen content on microstructures and mechanical properties of (AlCrTiZrHf)N high-entropy alloy nitride films[J]. J. Alloys Compd., 2020, 834: 155063
doi: 10.1016/j.jallcom.2020.155063
[65] Hsueh H T, Shen W J, Tsai M H, et al. Effect of nitrogen content and substrate bias on mechanical and corrosion properties of high-entropy films (AlCrSiTiZr)100-xNx[J]. Surf. Coat. Technol., 2012, 206: 4106
doi: 10.1016/j.surfcoat.2012.03.096
[66] Li Y T, Chen X M, Zeng X K, et al. Hard yet tough and self-lubricating (CuNiTiNbCr)Cx high-entropy nanocomposite films: Effects of carbon content on structure and properties[J]. J. Mater. Sci. Technol., 2024, 173: 20
doi: 10.1016/j.jmst.2023.05.082
[67] Zendejas Medina L, Tavares da Costa M V, Paschalidou E M, et al. Enhancing corrosion resistance, hardness, and crack resistance in magnetron sputtered high entropy CoCrFeMnNi coatings by adding carbon[J]. Mater. Des., 2021, 205: 109711
doi: 10.1016/j.matdes.2021.109711
[68] Jhong Y S, Huang C W, Lin S J. Effects of CH4 flow ratio on the structure and properties of reactively sputtered (CrNbSiTiZr)Cx coatings[J]. Mater. Chem. Phys., 2018, 210: 348
doi: 10.1016/j.matchemphys.2017.08.002
[69] Liu W, Wang C, Yang K, et al. Carbon-driven microstructural tuning enhances tribological and corrosion performance in FeCoNiCrCx high-entropy alloy films[J]. Carbon, 2025, 238: 120237
doi: 10.1016/j.carbon.2025.120237
[70] Khan N A, Akhavan B, Zheng Z, et al. Nanostructured AlCoCrCu0.5FeNi high entropy oxide (HEO) thin films fabricated using reactive magnetron sputtering[J]. Appl. Surf. Sci., 2021, 553: 149491
doi: 10.1016/j.apsusc.2021.149491
[71] Lin M I, Tsai M H, Shen W J, et al. Evolution of structure and properties of multi-component (AlCrTaTiZr)Ox films[J]. Thin Solid Films, 2010, 518: 2732
doi: 10.1016/j.tsf.2009.10.142
[72] Lee C Y, Chien C H, Yeh J W, et al. Effects of the carbon-to-nitrogen ratio on the microstructure and properties of (CrNbSiTiZr)CxNy high-entropy carbonitride films[J]. Mater. Chem. Phys., 2022, 277: 125374
doi: 10.1016/j.matchemphys.2021.125374
[73] Chang S Y, Lin S Y, Huang Y C. Microstructures and mechanical properties of multi-component (AlCrTaTiZr)NxCy nanocomposite coatings[J]. Thin Solid Films, 2011, 519: 4865
doi: 10.1016/j.tsf.2011.01.043
[74] Zok F W, Miserez A. Property maps for abrasion resistance of materials[J]. Acta Mater., 2007, 55: 6365
pmid: 18836523
[75] Ling Y C, Yu X, Yuan S J, et al. Flexomagnetic effect enhanced ferromagnetism and magnetoelectrochemistry in freestanding high-entropy alloy films[J]. ACS Nano, 2023, 17: 17299
doi: 10.1021/acsnano.3c05255
[76] Pavithra C L P, Janardhana R K S K, Reddy K M, et al. An advancement in the synthesis of unique soft magnetic CoCuFeNiZn high entropy alloy thin films[J]. Sci. Rep., 2021, 11: 8836
doi: 10.1038/s41598-021-87786-8 pmid: 33893346
[77] Chaudhary V, Chaudhary R, Banerjee R, et al. Accelerated and conventional development of magnetic high entropy alloys[J]. Mater. Today, 2021, 49: 231
doi: 10.1016/j.mattod.2021.03.018
[78] Chen J W, Chen S H, Shafer P, et al. Role of the structure order in the transport and magnetic properties of high-entropy alloy films[J]. NPG Asia Mater., 2024, 15: 72
doi: 10.1038/s41427-023-00518-4
[79] Mazza A R, Skoropata E, Sharma Y, et al. Designing magnetism in high entropy oxides[J]. Adv. Sci., 2022, 9: 2200391
doi: 10.1002/advs.v9.10
[80] Sarkar A, Kruk R, Hahn H. Magnetic properties of high entropy oxides[J]. Dalton Trans., 2021, 50: 1973
doi: 10.1039/d0dt04154h pmid: 33443275
[81] Ogale S B, Venkatesan T V, Blamire M G. Functional Metal Oxides: New Science and Novel Applications[M]. Germany: John Wiley & Sons, Inc, 2013: 26
[82] Roth W L. Magnetic structures of MnO, FeO, CoO, and NiO[J]. Phys. Rev., 1958, 110: 1333
doi: 10.1103/PhysRev.110.1333
[83] Hillebrecht F U, Ohldag H, Weber N B, et al. Magnetic moments at the surface of antiferromagnetic NiO(100)[J]. Phys. Rev. Lett., 2001, 86: 3419
pmid: 11327985
[84] Srdić V V, Cvejić Z, Milanović M, et al. Metal Oxide Structure, Crystal Chemistry, and Magnetic Properties[M]. Amsterdam: Elsevier, 2018: 313
[85] Teillet J, Bouree F, Krishnan R. Magnetic structure of CoFe2O4[J]. J. Magn. Magn. Mater., 1993, 123: 93
doi: 10.1016/0304-8853(93)90017-V
[86] Bouferrache K, Charifi Z, Baaziz H, et al. Electronic structure, magnetic and optic properties of spinel compound NiFe2O4[J]. Semicond. Sci. Technol., 2020, 35: 095013
[87] Ke W E, Chen J W, Liu C E, et al. Crystalline magnetic anisotropy in high entropy (Fe, Co, Ni, Cr, Mn)3O4 oxide driven by single-element orbital anisotropy[J]. Adv. Funct. Mater., 2024, 34: 2312856
[88] Wang H L, Huang H L, Feng Y P, et al. Enhanced exchange bias in epitaxial high-entropy oxide heterostructures[J]. ACS Appl. Mater. Interfaces, 2023, 15: 58643
doi: 10.1021/acsami.3c14943
[89] Mayandi J, Dias M, Stange M, et al. Partial oxidation of high entropy alloys: A route toward nanostructured ferromagnets[J]. Materialia, 2021, 20: 101250
doi: 10.1016/j.mtla.2021.101250
[90] Zhang J Y, Wang X, Li X N, et al. Native oxidation and complex magnetic anisotropy-dominated soft magnetic CoCrFeNi-based high-entropy alloy thin films[J]. Adv. Sci., 2022, 9: 2203139
doi: 10.1002/advs.v9.33
[91] Minouei H, Kheradmandfard M, Saboktakin Rizi M, et al. Formation mechanism of high-entropy spinel thin film and its mechanical and magnetic properties: Linking high-entropy alloy to high-entropy ceramic[J]. Appl. Surf. Sci., 2022, 576: 151719
doi: 10.1016/j.apsusc.2021.151719
[92] Bachani S K, Wang C J, Lou B S, et al. Fabrication of TiZrNb-TaFeN high-entropy alloys coatings by HiPIMS: Effect of nitrogen flow rate on the microstructural development, mechanical and tribological performance, electrical properties and corrosion characteristics[J]. J. Alloys Compd., 2021, 873: 159605
doi: 10.1016/j.jallcom.2021.159605
[93] Xia A, Dedoncker R, Glushko O, et al. Influence of the nitrogen content on the structure and properties of MoNbTaVW high entropy alloy thin films[J]. J. Alloys Compd., 2021, 850: 156740
doi: 10.1016/j.jallcom.2020.156740
[94] Wang X, Li X N, Li Z M, et al. Percolation theory analysis on the variation of magnetic and electrical properties in oxygen-containing CoCrFeNi high-entropy films[J]. Acta Mater., 2025, 293: 121123
doi: 10.1016/j.actamat.2025.121123
[95] Yu R S, Huang R H, Lee C M, et al. Synthesis and characterization of multi-element oxynitride semiconductor film prepared by reactive sputtering deposition[J]. Appl. Surf. Sci., 2012, 263: 58
doi: 10.1016/j.apsusc.2012.08.109
[96] Chen T K, Wong M S. Hard transparent conducting hex-element complex oxide films by reactive sputtering[J]. J. Mater. Res., 2008, 23: 3075
doi: 10.1557/JMR.2008.0371
[97] Pristáš G, Gruber G C, Orendáč M, et al. Multiple transition temperature enhancement in superconducting TiNbMoTaW high entropy alloy films through tailored N incorporation[J]. Acta Mater., 2024, 262: 119428
doi: 10.1016/j.actamat.2023.119428
[98] Hu R W, Bozin E S, Warren J B, et al. Superconductivity, magnetism, and stoichiometry of single crystals of Fe1+y (Te1-xSx)z[J]. Phys. Rev., 2009, 80B: 214514
[1] ZHU Chunjian, LI Yanhui, ZHU Zhengwang, WU Licheng, ZHANG Haifeng, ZHANG Wei. Regulation of Structure and Magnetic Properties of Fe98.5 -x B x Cu1.5 Nanocrystalline Alloys Based on B Content[J]. 金属学报, 2025, 61(8): 1174-1182.
[2] GE Penghua, ZHANG Yong, LI Zhiming. Soft-Magnetic and Mechanical Behaviors of Heterostructured FeCoNi Medium-Entropy Alloys[J]. 金属学报, 2025, 61(7): 1119-1128.
[3] SUN Huanteng, MA Yunzhu, CAI Qingshan, WANG Jianning, DUAN Youteng, ZHANG Mengxiang. Differential Microstructure Between fcc and bcc Steel Plates Under Hyper-Velocity Impact[J]. 金属学报, 2025, 61(7): 1011-1023.
[4] WANG Qiang, LI Xiaobing, HAO Junjie, CHEN Bo, ZHANG Bin, ZHANG Erlin, LIU Kui. Solid-State Phase Transformation Behavior of a Novel Ti-Al-Mn-Nb Alloy[J]. 金属学报, 2025, 61(7): 1060-1070.
[5] MENG Xianglong, LIU Ruiliang, Li D. Y.. First Principles Study on the Precipitation and Properties of Carbides in the Surface Carburized Layer of Tantalum Alloys[J]. 金属学报, 2025, 61(5): 797-808.
[6] JU Yulin, WEI Qi, YUAN Zhizhong, CHENG Xiaonong. Hardness and Microstructural Evolution of Lower Bainite and Martensite Mixtures on Tempering of High-Strength Low-Alloy Steel Plates[J]. 金属学报, 2025, 61(10): 1531-1541.
[7] LIU Zhongwu, ZHOU Bang, LIAO Xuefeng, HE Jiayi. Research Status and Future Development of (Ce, La, Y)-Fe-B Permanent Magnets Based on Full High-Abundance Rare Earth Elements[J]. 金属学报, 2024, 60(5): 585-604.
[8] LI Kangjie, SUN Zeyu, HE Bei, TIAN Xiangjun. Microstructure and Hardness of Al-Cu-Li Alloy Fabricated by Arc Additive Manufacturing Based on In Situ Metallurgy of Molten Pool[J]. 金属学报, 2024, 60(5): 661-669.
[9] YANG Ping, MA Dandan, GU Chen, GU Xinfu. Influence of Initial Microstructure and Cold Rolling Reduction on Transformation Texture and Magnetic Properties of Industrial Low-Grade Electrical Steel[J]. 金属学报, 2024, 60(3): 377-387.
[10] ZHANG Shuqian, MA Yingjie, WANG Qian, QI Min, HUANG Sensen, LEI Jiafeng, YANG Rui. Mechanical Properties and Electrical Conductivity of α + β Titanium Alloy Sheet Regulated by Heat Treatment[J]. 金属学报, 2024, 60(12): 1622-1636.
[11] JIANG Huazhen, PENG Shuang, HU Qiyun, WANG Guangyi, CHEN Qisheng, LI Zhengyang, SUN Huilei, FANG Jiahuiyu. Corrosion and Cavitation Erosion Resistance of 316L Stainless Steels Produced by Laser Metal Deposition[J]. 金属学报, 2024, 60(11): 1512-1530.
[12] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[13] WANG Haifeng, ZHANG Zhiming, NIU Yunsong, YANG Yange, DONG Zhihong, ZHU Shenglong, YU Liangmin, WANG Fuhui. Effect of Pre-Oxidation on Microstructure and Wear Resistance of Titanium Alloy by Low Temperature Plasma Oxynitriding[J]. 金属学报, 2023, 59(10): 1355-1364.
[14] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[15] ZENG Xiaoqin, WANG Jie, YING Tao, DING Wenjiang. Recent Progress on Thermal Conductivity of Magnesium and Its Alloys[J]. 金属学报, 2022, 58(4): 400-411.
No Suggested Reading articles found!