| Influences of High-Entropy Alloy Particles on the Microstructure and Mechanical Properties of Selective Laser Melted Al12Si Alloy During Solution Treatment |
WANG Wei1, ZHANG Yubo1,2( ), ZHAO Yan1, WANG Tongmin1,2( ), LI Tingju1,2 |
1 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China 2 Ningbo Institute of Dalian University of Technology, Ningbo 315000, China |
|
Cite this article:
WANG Wei, ZHANG Yubo, ZHAO Yan, WANG Tongmin, LI Tingju. Influences of High-Entropy Alloy Particles on the Microstructure and Mechanical Properties of Selective Laser Melted Al12Si Alloy During Solution Treatment. Acta Metall Sin, 2026, 62(6): 1009-1020.
|
|
|
Abstract Heat treatment has been widely shown to substantially influence the microstructure of selective laser melted Al alloys and composites, enabling precise tuning of their mechanical properties. While extensive research has addressed the optimization of selective laser melting (SLM) process parameters, alloy composition, reinforcement content, and strengthening mechanisms, comparatively limited attention has been paid to the evolution of microstructure and mechanical properties of selective laser melted Al alloys and their composites during heat treatment. A critical knowledge gap remains regarding the mechanisms by which secondary phase particles govern microstructural evolution and mechanical property modifications under thermal processing. To address this gap, an Al12Si alloy modified with an AlCrCuFeNi high-entropy alloy (HEA) was successfully fabricated via SLM. Subsequent solution treatment enabled synergistic control over the microstructure and mechanical properties of the Al12Si-HEA alloy. Comprehensive microstructural characterization and mechanical testing were conducted to systematically investigate the role of HEA particles in influencing microstructural evolution and mechanical behavior during solution treatment. The results showed that the as-built Al12Si alloy exhibited a microstructure composed of primary α-Al and continuous cellular eutectic Si. The addition of HEA particles significantly modified the microstructure, promoting the formation of Si + α-Al(Fe, Cr)Si phases instead of the continuous eutectic Si observed in the unmodified Al12Si alloy. Solution treatment dissolved the cellular eutectic structure, leading to fragmentation and spheroidization of Si into granular phases diffusely distributed within the matrix. With increasing solution treatment time, these Si phases gradually coarsened due to Ostwald ripening, resulting in larger average sizes and reduced number density. Notably, the α-Al(Fe, Cr)Si phases inhibited Si atom diffusion within the matrix, substantially slowing the coarsening rate of the granular Si phases. Under all solution treatment conditions, the Al12Si-HEA alloy exhibited superior performance compared with the Al12Si alloy. This enhancement is attributed to the formation of dual-sized in situ reinforced phases after solution treatment, comprising finer micron-sized Si particles and nano-sized α-Al(Fe, Cr)Si phases. This unique microstructure enabled the Al12Si-HEA alloy to achieve both high str-ength (ultimate tensile strength > 300 MPa) and appreciable plasticity (~14%).
|
|
Received: 13 June 2025
|
|
|
| Fund: National Natural Science Foundation of China(52171135);National Natural Science Foundation of China(U23A20611) |
Corresponding Authors:
ZHANG Yubo, associate professor, Tel: 13500747899, E-mail: ybzhang@dlut.edu.cn; WANG Tongmin, professor, Tel: (0411)84706790, E-mail: tmwang@dlut.edu.cn
|
| [1] |
Opprecht M, Garandet J P, Roux G, et al. A solution to the hot cracking problem for aluminium alloys manufactured by laser beam melting[J]. Acta Mater., 2020, 197: 40
doi: 10.1016/j.actamat.2020.07.015
|
| [2] |
Wang M, Yang Y Q, Vyacheslav T, et al. Effects of particle size on processability of AlSi10Mg alloy manufactured by selective laser melting[J]. Acta Metall. Sin., 2023, 59: 147
doi: 10.11900/0412.1961.2022.00442
|
|
王 孟, 杨永强, Vyacheslav T 等. 粉末粒径对AlSi10Mg合金选区激光熔化成形的影响[J]. 金属学报, 2023, 59: 147
|
| [3] |
Zhao L, Song L B, Santos Macías J G, et al. Review on the correlation between microstructure and mechanical performance for laser powder bed fusion AlSi10Mg[J]. Addit. Manuf., 2022, 56: 102914
|
| [4] |
Yang T Y, Cui L, He D Y, et al. Enhancement of microstructure and mechanical property of AlSi10Mg-Er-Zr alloys fabricated by selective laser melting[J]. Acta Metall. Sin., 2022, 58: 1108
|
|
杨天野, 崔 丽, 贺定勇 等. 选区激光熔化AlSi10Mg-Er-Zr合金微观组织及力学性能强化[J]. 金属学报, 2022, 58: 1108
doi: 10.11900/0412.1961.2021.00085
|
| [5] |
Han Y, Wu Y H, Zhao C L, et al. High-temperature creep behavior of selective laser melting manufactured Al-Si-Fe-Mn-Ni alloy[J]. Acta Metall. Sin., 2025, 61: 154
|
|
韩 英, 吴雨航, 赵春禄 等. 选区激光熔化成形Al-Si-Fe-Mn-Ni合金的高温蠕变行为[J]. 金属学报, 2025, 61: 154
|
| [6] |
Zhu Z G, Hu Z H, Seet H L, et al. Recent progress on the additive manufacturing of aluminum alloys and aluminum matrix composites: Microstructure, properties, and applications[J]. Int. J. Mach. Tools Manuf., 2023, 190: 104047
doi: 10.1016/j.ijmachtools.2023.104047
|
| [7] |
Zhang D Y, Yi D H, Wu X P, et al. SiC reinforced AlSi10Mg composites fabricated by selective laser melting[J]. J. Alloys Compd., 2022, 894: 162365
doi: 10.1016/j.jallcom.2021.162365
|
| [8] |
Liao H L, Zhu H H, Xue G, et al. Alumina loss mechanism of Al2O3-AlSi10 Mg composites during selective laser melting[J]. J. Alloys Compd., 2019, 785: 286
doi: 10.1016/j.jallcom.2019.01.116
|
| [9] |
Xiao Y K, Yang Q, Bian Z Y, et al. Microstructure, heat treatment and mechanical properties of TiB2/Al-7Si-Cu-Mg alloy fabricated by selective laser melting[J]. Mater. Sci. Eng., 2021, A809: 140951
|
| [10] |
Yuan P P, Gu D D, Dai D H. Particulate migration behavior and its mechanism during selective laser melting of TiC reinforced Al matrix nanocomposites[J]. Mater. Des., 2015, 82: 46
doi: 10.1016/j.matdes.2015.05.041
|
| [11] |
Wu W J, Gao C F, Liu Z Q, et al. Laser powder bed fusion of crack-free TiN/Al7075 composites with enhanced mechanical properties[J]. Mater. Lett., 2021, 282: 128625
doi: 10.1016/j.matlet.2020.128625
|
| [12] |
He P D, Kong H, Liu Q, et al. Elevated temperature mechanical properties of TiCN reinforced AlSi10Mg fabricated by laser powder bed fusion additive manufacturing[J]. Mater. Sci. Eng., 2021, A811: 141025
|
| [13] |
Coello I E, Glerum J A, Ekaputra C N, et al. Effect of Zr and Sc additions on coarsening- and creep resistance of AlSi10Mg fabricated by laser powder bed fusion[J]. Addit. Manuf., 2025, 101: 104707
|
| [14] |
Wang J Y, Yang H L, Fu M W. An additively manufactured heat-resistant Al-12Si alloy via introducing stable eutectic engineering[J]. Addit. Manuf., 2024, 95: 104523
|
| [15] |
Wu Y H, Zhao C L, Han Y, et al. A new SLM-manufactured Al-Si alloy with excellent room and elevated-temperature mechanical properties[J]. J. Manuf. Process., 2025, 133: 25
doi: 10.1016/j.jmapro.2024.11.051
|
| [16] |
Zhu H W, Sun J W, Guo Y J, et al. Selective laser melting of a novel Al-Si-Fe-Mn-Ni alloy with superior mechanical properties at both room and elevated temperatures: Influence of processing parameters and heat treatment[J]. Mater. Charact., 2024, 214: 114098
|
| [17] |
Martin A, San Sebastian M, Gil E, et al. Effect of the heat treatment on the microstructure and hardness evolution of a AlSi10MgCu alloy designed for laser powder bed fusion[J]. Mater. Sci. Eng., 2021, A819: 141487
|
| [18] |
Huang N, Luo Q X, Bartles D L, et al. Effect of heat treatment on microstructure and mechanical properties of AlSi10Mg fabricated using laser powder bed fusion[J]. Mater. Sci. Eng., 2024, A895: 146228
|
| [19] |
Li X P, Wang X J, Saunders M, et al. A selective laser melting and solution heat treatment refined Al-12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility[J]. Acta Mater., 2015, 95: 74
|
| [20] |
Zhang X X, Lutz A, Gan W M, et al. Effect of annealing heat treatment on the macroscopic and microscopic deformation behavior of additively manufactured AlSi10Mg alloy[J]. Acta Metall. Sin., 2024, 60: 1091
doi: 10.11900/0412.1961.2024.00116
|
|
张星星, Lutz A, 甘为民 等. 退火热处理对增材制造AlSi10Mg合金宏观和微观变形行为的影响[J]. 金属学报, 2024, 60: 1091
doi: 10.11900/0412.1961.2024.00116
|
| [21] |
Kempf A, Hilgenberg K. Influence of heat treatments on AlSi10Mg specimens manufactured with different laser powder bed fusion machines[J]. Mater. Sci. Eng., 2021, A818: 141371
|
| [22] |
Takata N, Liu M L, Kodaira H, et al. Anomalous strengthening by supersaturated solid solutions of selectively laser melted Al-Si-based alloys[J]. Addit. Manuf., 2020, 33: 101152
|
| [23] |
He P D, Webster R F, Yakubov V, et al. Fatigue and dynamic aging behavior of a high strength Al-5024 alloy fabricated by laser powder bed fusion additive manufacturing[J], Acta Mater., 2021, 220: 117312.
doi: 10.1016/j.actamat.2021.117312
|
| [24] |
Shi S Q, Zhao Y F, Yang H O, et al. Achieving superior strength-plasticity performance in laser powder bed fusion of AlSi10Mg via high-speed scanning remelting[J]. Mater. Res. Lett., 2024, 12: 668
doi: 10.1080/21663831.2024.2370853
|
| [25] |
Martin J H, Yahata B D, Hundley H D, et al. 3D printing of high-strength aluminium alloys[J]. Nature, 2017, 549: 365
doi: 10.1038/nature23894
|
| [26] |
Ma P, Jia Y D, Prashanth K G, et al. Microstructure and phase formation in Al-20Si-5Fe-3Cu-1Mg synthesized by selective laser melting[J]. J. Alloys Compd., 2016, 657: 430
|
| [27] |
Hou L G, Cui C, Zhang J S. Optimizing microstructures of hypereutectic Al-Si alloys with high Fe content via spray forming technique[J]. Mater. Sci. Eng., 2010, A527: 6400
|
| [28] |
Hou L G, Cui C, Cai Y H, et al. Effect of (Mn + Cr) addition on the microstructure and thermal stability of spray-formed hypereutectic Al-Si alloys[J]. Mater. Sci. Eng., 2009, A527: 85
|
| [29] |
Bjurenstedt A, Casari D, Seifeddine S, et al. In-situ study of morphology and growth of primary α-Al(FeMnCr)Si intermetallics in an Al-Si alloy[J]. Acta Mater., 2017, 130: 1
|
| [30] |
Wang M, Song B, Wei Q S, et al. Effects of annealing on the microstructure and mechanical properties of selective laser melted AlSi7Mg alloy[J]. Mater. Sci. Eng., 2019, A739: 463
|
| [31] |
Tang P J, Chen B Q, Yan T Q, et al. Effects of heat treatment on microstructure, properties, and residual stress of additive manufactured AlSi10Mg alloy[J]. Sci. Technol. Rev., 2021, 39(9): 36
doi: 10.3981/j.issn.1000-7857.2021.09.004
|
|
唐鹏钧, 陈冰清, 闫泰起 等. 热处理对增材制造AlSi10Mg合金组织性能及残余应力的影响[J]. 科技导报, 2021, 39(9): 36
doi: 10.3981/j.issn.1000-7857.2021.09.004
|
| [32] |
Mousavi G S, Emamy M, Rassizadehghani J. The effect of mischmetal and heat treatment on the microstructure and tensile properties of A357 Al-Si casting alloy[J]. Mater. Sci. Eng., 2012, A556: 573
|
| [33] |
Hu Z P, Jiang J, Liao F J, et al. Kinetics of precipitation and coarsening of Si-containing phases in a supersaturated Al-20%Si Alloy[J]. Chin. J. Mater. Res., 2018, 32: 743
|
|
胡钟鹏, 江 峻, 廖福锦 等. 过饱和Al-20%Si合金Si相的析出粗化动力学[J]. 材料研究学报, 2018, 32: 743
doi: 10.11901/1005.3093.2018.139
|
| [34] |
Du Y, Chang Y A, Huang B Y, et al. Diffusion coefficients of some solutes in fcc and liquid Al: Critical evaluation and correlation[J]. Mater. Sci. Eng., 2003, A363: 140
|
| [35] |
Wu Z F, Wu R. Research development of secondary phase particle in dual-phase system[J]. Mater. Rep., 2010, 24(1): 113
|
|
吴志方, 吴 润. 两相体系中第二相颗粒粗化的研究进展[J]. 材料导报, 2010, 24(1): 113
|
| [36] |
Wang H, Yu F X, Sun Z G. Coarsening characteristic of Si particles in powders of rapidly solidified Al-Si alloy[J]. Foundry, 2007, 56: 65
|
|
王 话, 于福晓, 孙振国. 快速凝固铝硅合金粉末加热过程中硅颗粒的粗化行为[J]. 铸造, 2007, 56: 65
|
| [37] |
Xu Y, Shi H F, Yuan X G, et al. Effect of alloy elements on heat-resistence of spray deposition Al-Si alloy[J]. Hot Work. Technol., 2010, 39(19): 31
|
|
徐 洋, 时海芳, 袁晓光 等. 合金元素对喷射沉积铝硅合金耐热性能的影响[J]. 热加工工艺, 2010, 39(19): 31
|
| [38] |
Rao J H, Zhang Y, Fang X Y, et al. The origins for tensile properties of selective laser melted aluminium alloy A357[J]. Addit. Manuf., 2017, 17: 113
|
| [39] |
Albu M, Krisper R, Lammer J, et al. Microstructure evolution during in-situ heating of AlSi10Mg alloy powders and additive manufactured parts[J]. Addit. Manuf., 2020, 36: 101605
|
| [40] |
Liang E Q, Dai Y, Bai J, et al. Microstructure and mechanical property of annealing heat treated AlSi10Mg alloy fabricated by selective laser melting[J]. J. Mater. Eng., 2022, 50(5): 156
doi: 10.11868/j.issn.1001-4381.2021.000444
|
|
梁恩泉, 代 宇, 白 静 等. 退火态激光选区熔化成形AlSi10Mg合金组织与力学性能[J]. 材料工程, 2022, 50(5): 156
doi: 10.11868/j.issn.1001-4381.2021.000444
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|