| Effect of Powder Particle Size on Forming Titanium Alloy Shrouded Impeller |
SHANG Xuewen1,2, CUI Xiaoxiao2, XU Lei2, LU Zhengguan2( ) |
1 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China 2 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
|
Cite this article:
SHANG Xuewen, CUI Xiaoxiao, XU Lei, LU Zhengguan. Effect of Powder Particle Size on Forming Titanium Alloy Shrouded Impeller. Acta Metall Sin, 2025, 61(2): 253-264.
|
|
|
Abstract A shrouded impeller is an essential component of a liquid rocket, mainly responsible for transporting and pressurizing liquid fuel or oxidant. Owing to the low temperature and high-rotation speed of the working environment, materials with high performance are required for fabricating the impeller. With its excellent low temperature mechanical properties and high specific strength, Ti-5Al-2.5Sn extra-low interstitial (ELI) alloy has been widely applied in fabricating liquid rocket components, including the shrouded impeller. Considering the geometric complexity of the impeller, the powder metallurgy-hot isostatic pressing (PM-HIP) route is a suitable method for impeller formation. PM-HIP technology has a similar forming capability as precision casting but avoids casting defects, realizing the parts with reliable service performance. However, the mechanical properties and dimensional accuracy of the impeller may be influenced by the variation of powder particle sizes. Herein, three kinds of Ti-5Al-2.5Sn ELI prealloyed powders with different particle size distributions (average particle size D50 = 125, 94, and 73 μm) were prepared by adjusting the process parameters of gas atomization and screen meshes. Then, their corresponding shrouded impellers were manufactured via the PM-HIP route at 940 oC, 120 MPa for 3 h. Subsequently, the impellers were annealed at 815 oC for 1.5 h, followed by air cooling. The effect of powder particle sizes on the mechanical properties of shrouded impellers was analyzed using cryogenic-temperature tensile tests. The porosity defect of impeller slices was detected using industrial computed tomography. The microstructure of the impellers was characterized using SEM and TEM. Meanwhile, the mechanism of low temperature deformation was also discussed. All three impellers exhibited homogeneous microstructure with fine grains, and their mechanical properties were comparable to the level of wrought alloys; specifically, the tensile strength was about 1300 MPa, and the elongation was 20% at 77 K. In addition, many twins were found in the deformation zones, including the types of {}, {}, and {}. PM-HIP impeller size was calculated using the finite element method in the modified Gurson model and compared with the size of the actual impeller. Dimensional shrinkage was consistent between the finite element simulation result and the actual part, and the deviation in the flow channel was < 0.3 mm.
|
|
Received: 21 October 2022
|
|
|
| Fund: National Science and Technology Major Project of China(J2019-VII-0005-0145);Strategic Priority Research Program of Chinese Academy of Sciences(XDA22010102) |
Corresponding Authors:
LU Zhengguan, Tel: (024)83978843, E-mail: zglu@imr.ac.cn
|
| 1 |
Volkov A M, Karyagin D A, Letnikov M N, et al. Specifics of producing disk blanks for gas-turbine engines using granules of super heat-resistant nickel alloys [J]. Metallurgist, 2020, 64: 362
|
| 2 |
Hashiguchi D H, Heberling J, Campbell J, et al. New decade of shaped beryllium blanks [A]. Proceedings of SPIE 9574, Material Technologies and Applications to Optics, Structures, Components, and Sub-Systems [C]. San Diego: SPIE, 2015: 957403
|
| 3 |
Sergi A, Khan R H U, Irukuvarghula S, et al. Development of Ni-base metal matrix composites by powder metallurgy hot isostatic pressing for space applications [J]. Adv. Powder Technol., 2022, 33:103411
|
| 4 |
Qian Z D, Wang H. Russian pд hydrogen-oxygen engine technology [R]. Technical Report on Aerospace, 1995: 12
|
|
钱宗德, 王 桁. 俄罗斯pд—0120氢氧发动机技术 [R]. 航天技术报告, 1995: 12
|
| 5 |
Guichard D, Laithier F, Fournier J P. Development of powder metallurgy impellers for VINCI hydrogen turbopump [A]. Proceedings of the 36th AIAA/ASME/SAE/ASEE Joint Propulsion Conference and Exhibit [C]. Las Vegas: AIAA. 2000. doi:10.2514/6.2000-3861
|
| 6 |
Alliot P, Marchal N, Goirand B. The VINCI hydrogen turbopump development status [A]. Proceedings of the 38th AIAA/ASME/SAE/ASEE Joint Propulsion Conference & Exhibit [C]. Indianapolis: AIAA, 2013. doi:10.2514/6.2002-4007
|
| 7 |
Bouley S A, Grabowski Jr R C, Rachuk V S, et al. Unified low-risk single-shaft turbopump for cryogenic expander-cycle rocket engines [A]. Proceedings of the 46th AIAA/ASME/SAE/ASEE Joint Propulsion Conference & Exhibit [C]. Nashville: AIAA, 2010. doi:10.2514/6.2010-7130
|
| 8 |
Xu L, Guo R P, Wu J, et al. Progress in hot isostatic pressing technology of titanium alloy powder [J]. Acta Metall. Sin., 2018, 54: 1537
|
|
徐 磊, 郭瑞鹏, 吴 杰 等. 钛合金粉末热等静压近净成形研究进展 [J]. 金属学报, 2018, 54: 1537
|
| 9 |
Yin Y J, Zhang P, Zhou J X, et al. Correction on Shima yield criterion for Ti6Al4V powder HIP process [J]. J. Huazhong Univ. Sci. Technol. (Nat. Sc. Ed.), 2018, 46(6): 14
|
|
殷亚军, 张 朋, 周建新 等. Ti6Al4V合金粉末热等静压Shima屈服准则修正 [J]. 华中科技大学学报(自然科学版), 2018, 46(6): 14
|
| 10 |
Lang L H, Bu G L, Xue Y, et al. Determine key parameters of simulation constitutive and process optimization for titanium alloy (Ti-6Al-4V) hot isostatic pressing [J]. J. Plast. Eng., 2011, 18(4): 34
|
|
郎利辉, 布国亮, 薛 勇 等. 钛合金热等静压模拟本构关键参数确定及工艺优化 [J]. 塑性工程学报, 2011, 18(4): 34
|
| 11 |
Samarov V, Seliverstov D, Froes F H. Fabrication of near-net-shape cost-effective titanium components by use of prealloyed powders and hot isostatic pressing [A]. Titanium Powder Metallurgy: Science, Technology and Applications [C]. Boston: Butterworth-Heinemann, 2015: 313
|
| 12 |
Goirand B, Gallardo J F, Bosson R. Vinci hydrogen turbopump: A new step in safe, faster and cheaper developments [A]. Proceedings of the 36th AIAA/ASME/SAE/ASEE Joint Propulsion Conference and Exhibit [C]. Las Vegas: AIAA. 2000, doi:10.2514/6.2000-3156
|
| 13 |
Yoon S H, Choi C H, Kim J. HIP activities for turbopump components of Korea space launch vehicle [A]. Proceedings of the 12th International Conference on Hot Isostatic Pressing (HIP '17) [C]. Millersville: Materials Research Forum LLC, 2019: 79
|
| 14 |
Guo R P, Xu L, Cheng W X, et al. Effect of hot isostatic pressing parameters on microstructure and mechanical properties of powder metallurgy Ti-5Al-2.5Sn ELI alloy [J]. Acta Metall. Sin., 2016, 52: 842
|
|
郭瑞鹏, 徐 磊, 程文祥 等. 热等静压参数对Ti-5Al-2.5Sn ELI粉末合金组织与力学性能的影响 [J]. 金属学报, 2016, 52: 842
doi: 10.11900/0412.1961.2016.00018
|
| 15 |
Lütjering G, Williams J C. Titanium [M]. 2nd Ed., Berlin Heidelberg: Springer, 2007: 1
|
| 16 |
Lu Z C, Zhang X H, Ji W, et al. Investigation on the deformation mechanism of Ti-5Al-2.5Sn ELI titanium alloy at cryogenic and room temperatures [J]. Mater. Sci. Eng., 2021, A818: 141380
|
| 17 |
Billinghurst Jr E E. Tensile properties of cast titanium alloys: Titanium-6Al-4V ELI and titanium-5Al-2.5Sn ELI [R]. Huntsville: National Aeronautics and Space Administration, 1992
|
| 18 |
Lu Z G. Preparation and hot deformation of Ti2AlNb alloy prepared by powder metallurgy [D]. Hefei: University of Science and Technology of China, 2019
|
|
卢正冠. 粉末冶金Ti2AlNb合金的制备及热变形研究 [D]. 合肥: 中国科学技术大学, 2019
|
| 19 |
Wu J, Xu L, Lu Z G, et al. Preparation and electron beam welding of HIP powder metallurgy Ti-22Al-24Nb-0.5 Mo alloys [J]. Rare Met. Mater. Eng., 2017, 46(S1): 241
|
|
吴 杰, 徐 磊, 卢正冠 等. 热等静压粉末Ti2AlNb合金的制备及电子束焊 [J]. 稀有金属材料与工程, 2017, 46(S1): 241
|
| 20 |
Chen W X, Xu L, Lei J F, et al. Effects of powder size segregation on tensile properties of Ti-5Al-2.5Sn ELI alloy powder [J]. Chin. J. Nonferrous Met., 2013, 23: 362
|
|
程文祥, 徐 磊, 雷家峰 等. 粉末粒度偏析对Ti-5Al-2.5Sn ELI粉末合金拉伸性能的影响 [J]. 中国有色金属学报, 2013, 23: 362
|
| 21 |
Liu Q M, Wu J, Chen Y L, et al. Effect of temperature and powder particle size on mechanical properties and microstructure of PM Ti2AlNb alloy prepared via hot isostatic pressing [J]. Chin. J. Mater. Res., 2019, 33: 161
|
|
刘巧沐, 吴 杰, 陈玉龙 等. 热等静压温度和粉末粒度对Ti2AlNb合金组织与性能的影响 [J]. 材料研究学报, 2019, 33: 161
doi: 10.11901/1005.3093.2018.509
|
| 22 |
Lu Z G, Wu J, Xu L, et al. Powder size influence on tensile properties and porosity for PM Ti2AlNb alloy prepared by hot isostatic pressing [J]. Acta Metall. Sin. (Engl. Lett.), 2019, 32: 1329
|
| 23 |
Christian J L, Hurlich A. Mechanical properties of titanium alloys at cryogenic temperatures [A]. Proceedings of 1967 Cryogenic Engineering Conference Stanford University Stanford [C]. California: Springer, 1995. doi:10.1007/978-1-4757-0516-4_35
|
| 24 |
Grinder O. Surface oxidation of steel powder [J]. Steel Res. Int., 2010, 81: 908
|
| 25 |
Xu L, Tian X S, Wu J, et al. Microstructure and mechanical properties of inconel 718 powder alloy prepared by hot isostatic pressing [J]. Acta Metall. Sin., 2023, 59: 693
doi: 10.11900/0412.1961.2021.00586
|
|
徐 磊, 田晓生, 吴 杰 等. 热等静压成形Inconel 718粉末合金的显微组织和力学性能 [J]. 金属学报, 2023, 59: 693
|
| 26 |
Nayan N, Singh G, Antony Prabhu T, et al. Cryogenic mechanical properties of warm multi-pass caliber-rolled fine-grained titanium alloys: Ti-6Al-4V (normal and ELI grades) and VT14 [J]. Metall. Mater. Trans., 2018, 49A: 128
|
| 27 |
Arul Kumar M, Wroński M, McCabe R J, et al. Role of microstructure on twin nucleation and growth in HCP titanium: A statistical study [J]. Acta Mater., 2018, 148: 123
|
| 28 |
Huang C W, Ge P, Zhao Y Q, et al. Research progress in titanium alloys at cryogenic temperatures [J]. Rare Met. Mater. Eng., 2016, 45: 254
|
|
黄朝文, 葛 鹏, 赵永庆 等. 低温钛合金的研究进展 [J]. 稀有金属材料与工程, 2016, 45: 254
|
| 29 |
Grässel O, Krüger L, Frommeyer G, et al. High strength Fe-Mn-(Al, Si) TRIP/TWIP steels development-properties-application [J]. Int. J. Plast., 2000, 16: 1391
|
| 30 |
Yuan W X, Mei J, Samarov V, et al. Computer modelling and tooling design for near net shaped components using hot isostatic pressing [J]. J. Mater. Process. Technol., 2007, 182: 39
|
| 31 |
Abouaf M, Chenot J L, Raisson G, et al. Finite element simulation of hot isostatic pressing of metal powders [J]. Int. J. Numer. Methods Eng., 1988, 25: 191
|
| 32 |
Van Nguyen C, Bezold A, Broeckmann C. Inclusion of initial powder distribution in FEM modelling of near net shape PM hot isostatic pressed components [J]. Powder Metall., 2014, 57: 295
|
| 33 |
Abdelhafeez A M, Essa K E A. Influences of powder compaction constitutive models on the finite element simulation of hot isostatic pressing [J]. Procedia CIRP, 2016, 55: 188
|
| 34 |
Gurson A L. Plastic flow and fracture behavior of ductile materials incorporating void nucleation, growth, and interaction [D]. Providence: Brown University, 1975
|
| 35 |
Gurson A L. Continuum theory of ductile rupture by void nucleation and growth: Part I—Yield criteria and flow rules for porous ductile media [J]. J. Eng. Mater. Technol., 1977, 99: 2
|
| 36 |
Tvergaard V. On localization in ductile materials containing spherical voids [J]. Int. J. Fract., 1982, 18: 237
|
| 37 |
Aravas N. On the numerical integration of a class of pressure-dependent plasticity models [J]. Int. J. Numer. Methods Eng., 1987, 24: 1395
|
| 38 |
Wu J. Preparation and mechanical properties optimization of powder metallurgy Ti-22Al-24Nb-0.5Mo Alloys [D]. Beijing: University of Chinese Academy of Sciences, 2016
|
|
吴 杰. 粉末冶金Ti-22Al-24Nb-0.5Mo合金的制备和性能调控 [D]. 北京: 中国科学院大学, 2016
|
| 39 |
Arzt E, Ashby M F, Easterling K E. Practical applications of hotisostatic pressing diagrams: Four case studies [J]. Metall. Mater. Trans., 1983, 14A: 211
|
| 40 |
Broeckmann C. Hot isostatic pressing of near net shape components-process fundamentals and future challenges [J]. Powder Metall., 2012, 55: 176
|
| 41 |
Svoboda A, Häggblad H Å, Karlsson L. Simulation of hot isostatic pressing of a powder metal component with an internal core [J]. Comput. Methods Appl. Mech. Eng., 1997, 148: 299
|
| 42 |
Xu L, Guo R P, Chen Z Y, et al. Mechanical property of powder compact and forming of large thin-wall cylindrical structure of Ti55 alloys [J]. Chin. J. Mater. Res., 2016, 30: 23
doi: 10.11901/1005.3093.2015.284
|
|
徐 磊, 郭瑞鹏, 陈志勇 等. Ti55粉末合金的拉伸性能和薄壁筒体结构的成型 [J]. 材料研究学报, 2016, 30: 23
|
| 43 |
Olevsky E, Maximenko A, Van Dyck S, et al. Container influence on shrinkage under hot isostatic pressing—I. Shrinkage anisotropy of a cylindrical specimen [J]. Int. J. Solids Struct., 1998, 35: 2283
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|