Effect of Pre-Tension on the Fatigue Fracture of Under-Aged 7N01 Aluminum Alloy Plate
TIAN Ni1,2(), SHI Xu1, LIU Wei1, LIU Chuncheng3, ZHAO Gang1,2, ZUO Liang2,4
1.School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China 2.Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), Northeastern University, Shenyang 110819, China 3.Engineering Training Center, Northeastern University, Shenyang 110819, China 4.Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
Cite this article:
TIAN Ni, SHI Xu, LIU Wei, LIU Chuncheng, ZHAO Gang, ZUO Liang. Effect of Pre-Tension on the Fatigue Fracture of Under-Aged 7N01 Aluminum Alloy Plate. Acta Metall Sin, 2022, 58(6): 760-770.
7N01 aluminum alloy is the main load-bearing structure material for bullet train bodies due to its high specific strength, high specific stiffness, good magnetic-shielding ability, strong corrosion resistance, and good formability and weldability. The fatigue performance of materials and components used in bullet trains determines their security. It is unavoidable that there is pre-deformation during the assembly process of aluminum alloy components, which will influence the active service and fatigue performance of the aluminum alloy. It is important not only to clarify the relationship between pre-deformation and fatigue performance but also to reveal the mechanism of pre-deformation on the fatigue fracture of 7N01 aluminum alloy, to ensure the security of the bullet train. In this study, the effect of pre-tensile deformation on the fatigue property, fatigue fracture initiation, and fatigue crack propagation characteristics of a commercial 7N01 aluminum alloy plate at under-aged conditions was studied using tensile and fatigue tests combined with microstructure analysis. As the pre-tensile deformation increased to 20%, the results showed that the shape, size, number, distribution of second phase particles, as well as the size and morphology of thin strips grain of under-aged 7N01 aluminum alloy plate were almost the same. However, the under-aged 7N01 aluminum alloy plate has a significant strain-hardening effect after pre-tensile at room temperature, with the yield strength, tensile strength, and hardness increased from 181 MPa, 233 MPa, and 95 HV (without pre-tensile deformation) to 254 MPa, 271 MPa, and 117 HV (after 20% pre-tensile deformation), while the elongation decreased from 23.2% to 5.2%. Under the 175 MPa pulsating tensile load condition (stress ratio R = 0), the overall fatigue life of the under-aged 7N01 aluminum alloy plate first reduced, then prolonged, and then decreased as pre-tensile deformation increased. Without pre-tensile deformation, the fatigue life of under-aged 7N01 aluminum alloy plate is about 6.06 × 105 cyc, and when prolonged by about 75%, it reaches about 1.06 × 106 cyc after 5% pre-tensile deformation. However, the fatigue life of the under-aged 7N01 aluminum alloy plate is decreased to 4.21 × 105 and 2.89 × 105 cyc after 3% and 20% pre-tensile deformation, respectively. The evenly distributed high-density dislocations or dislocation cells resulted in 5%-16% pre-tensile deformation in the under-aged 7N01 aluminum alloy plate, which can prolong the fatigue life of the alloy plate by over 23%.
Fund: National Natural Science Foundation of China(51871043);Fundamental Research Funds for the Central Universities of China(180212010);Natural Science Foundation of Liaoning Province(2019-MS-113)
About author: TIAN Ni, associate professor, Tel: (024)83671571, E-mail: tiann@atm.neu.edu.cn
Fig.1 Specimen size for tensile and fatigue tests (unit: mm)
Fig.2 OM images of under-aged 7N01 aluminum alloy plate and after different pre-tensile deformations (along longitudinal section, non-etched) (a) three-dimensional diagram, undeformed(b) undeformed (c) 3% (d) 5% (e) 8% (f) 12% (g) 16% (h) 20%
Fig.3 OM images of grains of under-aged 7N01 aluminum alloy plate and after different pre-tensile deformations (along longitudinal section) that were observed by polarized light microscope (a) three-dimensional diagram, undeformed (b) undeformed (c) 3% (d) 5% (e) 8% (f) 12% (g) 16% (h) 20%
Fig.4 TEM images of under-aged 7N01 aluminum alloy plate and after different pre-tensile deformations (a) undeformed (b) 3% (c) 5% (d) 8% (e) 12% (f) 16% (g) 20%
Fig.5 Mechanical properties of under-aged 7N01 aluminum alloy plate after different pre-tensile deformations (a) microhardness (b) yield strength, tensile strength, and elongation
Fig.6 Fatigue life of under-aged 7N01 aluminum alloy plate after different pre-tensile deformations
Fig.7 SEM images of fatigue sources of under-aged 7N01 aluminum alloy plate after different pre-tensile deformations (a) undeformed (b) 3% (c) 5% (d) 8% (e) 16% (f) 20%
Fig.8 SEM images of fatigue crack propagation of under-aged 7N01 aluminum alloy plate after different pre-tensile deformations (a) undeformed (b) 3% (c) 5% (d) 8% (e) 16% (f) 20%
Term
0%
3%
5%
8%
12%
16%
20%
λi
+ + +
+ +
+ + + +
+ + + +
+ + + +
+ + + + +
+
λp
+ +
+ +
+ + + + +
+ + + +
+ + +
+
+
λ
+ + + + +
+ + + +
+ + + + + + + + +
+ + + + + + + +
+ + + + + + +
+ + + + + +
+ +
Table 1 Contribution results of pre-tensile deformation on fatigue crack initiation resistance (λi), fatigue crack propagation resistance (λp), and fatigue life (λ) of under-aged 7N01 aluminum alloy plate after different pre-tensile deformations
Fig.9 Schematics of fatigue crack propagation of under-aged 7N01 aluminum alloy plate after different pre-tensile deformations (a) undeformed (b) 3% (c) 5% (d) 8% (e) 12% (f) 16% (g) 20%
1
Deschamps A, Texier G, Ringeval S, et al. Influence of cooling rate on the precipitation microstructure in a medium strength Al-Zn-Mg alloy [J]. Mater. Sci. Eng., 2009, A501: 133
2
Heinz A, Haszler A, Keidel C, et al. Recent development in aluminium alloys for aerospace applications [J]. Mater. Sci. Eng., 2000, A280: 102
3
Liu W H, Liu W B, Bao A L. Microstructure and properties of ceramic coatings on 7N01 aluminum alloy by micro-arc oxidation [J]. Procedia Eng., 2012, 27: 828
doi: 10.1016/j.proeng.2011.12.527
4
Branco R, Costa J D, Borrego L P, et al. Effect of tensile pre-strain on low-cycle fatigue behaviour of 7050-T6 aluminium alloy [J]. Eng. Fail. Anal., 2020, 114: 104592
doi: 10.1016/j.engfailanal.2020.104592
5
Branco R, Borrego L P, Costa J D, et al. Effect of pre-strain on cyclic plastic behaviour of 7050-T6 aluminium alloy [J]. Procedia Struct. Integr., 2019, 17: 177
doi: 10.1016/j.prostr.2019.08.024
6
Niendorf T, Lotze C, Canadinc D, et al. The role of monotonic pre-deformation on the fatigue performance of a high-manganese austenitic TWIP steel [J]. Mater. Sci. Eng., 2009, A499: 518
7
Gustavsson A, Melander A. Fatigue of a highly prestrained dual-phase sheet steel [J]. Fatigue Fract. Eng. Mater. Struct., 1995, 18(2): 201
doi: 10.1111/j.1460-2695.1995.tb00155.x
8
Uemura T. A fatigue life estimation of specimens excessively prestrained in tension [J]. Fatigue Fract. Eng. Mater. Struct., 1998, 21: 151
doi: 10.1046/j.1460-2695.1998.00223.x
9
Al-Rubaie K S, Del Grande M A, Travessa D N, et al. Effect of pre-strain on the fatigue life of 7050-T7451 aluminium alloy [J]. Mater. Sci. Eng., 2007, A464: 141
10
Schijve J. The effect of pre-strain on fatigue crack growth and crack closure [J]. Eng. Fract. Mech., 1976, 8: 575
doi: 10.1016/0013-7944(76)90031-X
11
Froustey C, Lataillade J L. Influence of large pre-straining of aluminium alloys on their residual fatigue resistance [J]. Int. J. Fatigue, 2008, 30(5): 908
doi: 10.1016/j.ijfatigue.2007.06.011
12
Arora P R, Raghavan M R. Effect of tensile prestrain on fatigue strength of aluminum alloy in high cycle fatigue [J]. J. Eng. Mater. Technol., 1973, 95: 76
doi: 10.1115/1.3443135
13
Hodgson P, Parker B A. The composition of insoluble intermetallic phases in aluminium alloy 6010 [J]. J. Mater. Sci., 1981, 16: 1343
doi: 10.1007/BF01033850
14
Adrien J, Maire E, Estevez R, et al. Influence of the thermomechanical treatment on the microplastic behaviour of a wrought Al-Zn-Mg-Cu alloy [J]. Acta Mater., 2004, 52: 1653
doi: 10.1016/j.actamat.2003.12.009
15
Benoit S G, Chalivendra V B, Rice M A, et al. Characterization of the microstructure, fracture, and mechanical properties of aluminum alloys 7085-O and 7175-T7452 hollow cylinder extrusions [J]. Metall. Mater. Trans., 2016, 47A: 4476
16
Hou L G, Xiao W L, Su H, et al. Room-temperature low-cycle fatigue and fracture behaviour of asymmetrically rolled high-strength 7050 aluminium alloy plates [J]. Int. J. Fatigue, 2021, 142: 105919
doi: 10.1016/j.ijfatigue.2020.105919
17
Wen K, Fan Y Q, Wang G J, et al. Aging behavior and fatigue crack propagation of high Zn-containing Al-Zn-Mg-Cu alloys with zinc variation [J]. Prog. Nat. Sci., 2017, 27: 217
doi: 10.1016/j.pnsc.2017.02.002
18
Tian N, Zhao G, Zuo L, et al. Study on the strain hardening behavior of Al-Mg-Si-Cu alloy sheet for automotive body [J]. Acta. Metall. Sin., 2010, 46: 613
doi: 10.3724/SP.J.1037.2009.00799
Wang Z X, Li H, Wei X Y, et al. Effects of prior strain on static tensile properties and fatigue lives of 2E12 aluminum alloy [J]. Rare Met. Mater. Eng., 2010, 39(): 138
Wang X S, Liang F, Zeng Y P, et al. SEM in situ observations to the effects of inclusion on initiation and propagation of the low cyclic fatigue crack in super strength steel [J]. Acta. Metall. Sin, 2005, 41: 1272
Bai S, Liu Z Y, Gu Y X, et al. Microstructures and fatigue fracture behavior of an Al-Cu-Mg-Ag alloy with a low Cu/Mg ratio [J]. Mater. Sci. Eng., 2011, A530: 473
23
Xu L P, Wang Q Y, Zhou M. Micro-crack initiation and propagation in a high strength aluminum alloy during very high cycle fatigue [J]. Mater. Sci. Eng., 2018, A715: 404
24
Yao W X, Guo S J. Gigacycle fatigue life distribution of aluminum alloy LC4CS [J]. Acta. Metall. Sin., 2007, 43: 399
Zang X C, Xie L Y, Hu J X, et al. Effect of service on fracture mechanical properties of 7N01 aluminum alloy [J]. J. Northeast. Univ. (Nat. Sci.), 2017, 38: 1442
Jian H G, Jiang F, Wei L L, et al. Crystallographic mechanism for crack propagation in the T7451 Al-Zn-Mg-Cu alloy [J]. Mater. Sci. Eng., 2010, A527: 5879
27
Nandana M S, Udaya Bhat K, Manjunatha C M. Influence of retrogression and re-ageing heat treatment on the fatigue crack growth behavior of 7010 aluminum alloy [J]. Procedia Struct. Integr., 2019, 14: 314
doi: 10.1016/j.prostr.2019.05.039