| Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy |
GAO Bo1,2,WANG Lei1,2( ),SONG Xiu1,2,LIU Yang1,2,YANG Shuyu3,CHIBA Akihiko4 |
1. Key Lab for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China 2. School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China 3. College of Mechanical Engineering, Shenyang University, Shenyang 110044, China 4. Institute for Materials Research, Tohoku University, Sendai 980-8577, Japan |
|
Cite this article:
GAO Bo, WANG Lei, SONG Xiu, LIU Yang, YANG Shuyu, CHIBA Akihiko. Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy. Acta Metall Sin, 2019, 55(10): 1273-1281.
|
|
|
Abstract In 2006, stable γ' phase was found in Co-Al-W alloy, which provides a new way for developing Co-based superalloys. In order to meet the requirements for applications, the Co-Al-W-based superalloys need to have good oxidation and corrosion resistance. But the oxidation and corrosion resistance of the Co-Al-W-based superalloys is relatively low. In this work, pre-oxidation treatments were used to improve the oxidation and corrosion resistance. Three types of pre-oxidation treatments were carried out at 900 ℃ (in air), 950 ℃ (in air) and 1000 ℃ (in 1%O2+99%Ar), which were marked as 900-PreO, 950-PreO and 1000-LPreO, respectively. High temperature oxidation tests of both the pre-oxidation treated and untreated superalloys were carried out at 1000 ℃. And hot corrosion behaviors were also investigated at both 800 and 850 ℃. XRD, SEM and EDS were used to examine the characteristics of the oxidation and corrosion behaviors. The results show that the pre-oxide layers of the superalloys after different pre-oxidation treatments are compact. During oxidation at 1000 ℃, the Cr2O3 scale in 900-PreO treated superalloy is oxidized to form volatile products, and the diffusion resistance of both oxygen and the metal elements through the oxide layer is poor. In 1000-LPreO treated superalloy, serious spallation of the oxides occurs and leads to poor oxidation resistance. In 950-PreO treated superalloy, since the continuous CoCr2O4 and Al2O3 scales help to reduce the diffusion of oxygen and the metal elements, the mass gain of 950-PreO treated superalloy is consequently decreased. During the hot corrosion process, the pre-oxide layer of 950-PreO treated superalloy can hinder the diffusion of corrosive medium. Therefore, the corrosion resistance can be significantly improved by 950-PreO treatment, and the mass gain is decreased by over 80%.
|
|
Received: 31 January 2019
|
|
|
| Fund: Supported by National Natural Science Foundation of China(U1708253);National Science and Technology Major Project(2017-VI-0002) |
| [1] | Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 1 | | [2] | Sato J, Omori T, Oikawa K ,et al. Cobalt-base high-temperature alloys [J]. Science, 2006, 312: 90 | | [3] | Saal J E, Wolverton C. Thermodynamic stability of Co-Al-W L12γ' [J]. Acta Mater., 2013, 61: 2330 | | [4] | Guo J T. Materials Science and Engineering for Superalloys (Book 3) [M]. Beijing: Science Press, 2010: 123 | | [4] | (郭建亭. 高温合金材料学(下册) [M]. 北京: 科学出版社, 2010: 123) | | [5] | Shinagawa K, Omori T, Sato J ,et al. Phase equilibria and microstructure on γ' phase in Co-Ni-Al-W system [J]. Mater. Trans., 2008, 49: 1474 | | [6] | Xue F, Zhou H J, Ding X F, et al. Improved high temperature γ' stability of Co-Al-W-base alloys containing Ti and Ta [J]. Mater. Lett., 2013, 112: 215 | | [7] | Bauer A, Neumeier S, Pyczak F, et al. Microstructure and creep strength of different γ/γ'-strengthened Co-base superalloy variants [J]. Scr. Mater., 2010, 63: 1197 | | [8] | Yan H Y, Vorontsov V A, Dye D. Alloying effects in polycrystalline γ' strengthened Co-Al-W base alloys [J]. Intermetallics, 2014, 48: 44 | | [9] | Omori T, Oikawa K, Sato J, et al. Partition behavior of alloying elements and phase transformation temperatures in Co-Al-W-base quaternary systems [J]. Intermetallics, 2013, 32: 274 | | [10] | Birks N, Meier G H, Pettit F S. Introduction to the High-Temperature Oxidation of Metals [M]. 2nd Ed., Cambridge: Cambridge University Press, 2006: 1 | | [11] | Li M S. High Temperature Hot Corrosion of Metals [M]. Beijing: Metallurgical Industry Press, 2001: 239 | | [11] | (李美栓. 金属的高温腐蚀 [M]. 北京: 冶金工业出版社, 2001: 239) | | [12] | Zhang Y. Cyclic oxidation behavior of two novel Co-base superalloys [D]. Shenyang: Northeastern University, 2018 | | [12] | (张 莹. 两种新型钴基高温合金的循环氧化行为 [D]. 沈阳: 东北大学, 2018) | | [13] | Gao B, Wang L, Liu Y, et al. Corrosion behavior of new type Co-based superalloys with different Ni contents [J]. Corros. Rev., 2017, 35: 455 | | [14] | Xu Y T, Xia T D, Yan J Q. Effect of alloying element tungsten on hot corrosion behavior of novel Co-Al-W superalloys [J]. Chin. J. Nonferrous Met., 2011, 21: 110 | | [14] | (徐仰涛, 夏天东, 闫健强. 合金元素钨对新型Co-Al-W合金热腐蚀行为的影响 [J]. 中国有色金属学报, 2011, 21: 110) | | [15] | Xu Y T, Xia T D, Yan J Q. Effect of alloying elements to hot corrosion behavior of novel Co-Al-W superalloy [J]. J.Chin. Soc. orros. Prot., 2010, 30: 457 | | [15] | (徐仰涛, 夏天东, 闫健强. 合金元素对新型Co-Al-W合金热腐蚀行为的影响 [J]. 中国腐蚀与防护学报, 2010, 30: 457) | | [16] | Klein L, Shen Y, Killian M S ,et al. Effect of B and Cr on the high temperature oxidation behaviour of novel γ/γ′-strengthened Co-base superalloys [J]. Corros. Sci., 2011, 53: 2713 | | [17] | Guo J T. Materials Science and Engineering for Superalloys (Book 1) [M]. Beijing: Science Press, 2008: 664 | | [17] | (郭建亭. 高温合金材料学(上册) [M]. 北京: 科学出版社, 2008: 664) | | [18] | Huang L, Sun X F, Guan H R ,et al. Dgradation behavior of aluminide coatings on directionally solidified nickel base superalloy M951 [J]. Corros. Sci. Prot. Technol., 2005, 17: 34 | | [18] | (黄 粮, 孙晓峰, 管恒荣等. 定向凝固高温合金M951低压渗铝涂层的高温氧化及相变过程 [J]. 腐蚀科学与防护技术, 2005, 17: 34) | | [19] | Talic B, Molin S, Hendriksen P V, et al. Effect of pre-oxidation on the oxidation resistance of Crofer 22 APU [J]. Corros. Sci., 2018, 138: 189 | | [20] | Ou D R, Cheng M J. Effect of pre-oxidation on the oxidation resistance of spinel-coated Fe-Cr ferritic alloy for solid oxide fuel cell applications [J]. J. Power Sources., 2014, 247: 84 | | [21] | Li Z M, Qian S Q, Wang W, et al. Effect of preoxidation temperature on high temperature cyclic oxidation resistance of GH3128 superalloy [J]. Rare Met. Mater. Eng., 2012, 41: 1980 | | [21] | (李志明, 钱士强, 王 伟等. 预氧化温度对GH3128合金抗高温循环氧化性能的影响 [J]. 稀有金属材料与工程, 2012, 41: 1980) | | [22] | Young D J. High Temperature Oxidation and Corrosion of Metals [M]. Amsterdam: Elsevier, 2008: 193 | | [23] | Zheng L, Zhang M C, Dong J X. Oxidation behavior and mechanism of powder metallurgy Rene95 nickel based superalloy between 800 and 1000 ℃ [J]. Appl. Surf. Sci., 2010, 256: 7510 | | [24] | Sun D J, Liang C Y, Shang J L ,et al. Effect of Y2O3 contents on oxidation resistance at 1150 ℃ and mechanical properties at room temperature of ODS Ni-20Cr-5Al alloy [J]. Appl. Surf. Sci., 2016, 385: 587 | | [25] | Li T F. High Temperature Oxidation and Hot Corrosion of Metals [M]. Beijing: Chemical Industry Press, 2003: 30 | | [25] | (李铁蕃. 金属高温氧化和热腐蚀 [M]. 北京: 化学工业出版社, 2003: 30) | | [26] | Li X, Peng X Y, Duan Y L ,et al. Thermal oxidation behavior of commercial purity titanium at high temperature [J]. Chin. J. Nonferrous Met., 2013, 23: 2190 | | [26] | (李 旭, 彭小燕, 段雨露等. 工业纯钛的高温热氧化行为 [J]. 中国有色金属学报. 2013, 23: 2190) |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|