| U-Cr Binary Alloys with Anomalous Glass-Forming Ability |
Huogen HUANG1( ),Hongyang XU1,Pengguo ZHANG1,Yingmin WANG2,Haibo KE1,Pei ZHANG1,Tianwei LIU1 |
1 Institute of Materials, China Academy of Engineering Physics, Jiangyou 621907, China 2 Key Laboratory of Materials Modification by Laser, Ion and Electron Beams (Ministry of Education), School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China |
|
Cite this article:
Huogen HUANG,Hongyang XU,Pengguo ZHANG,Yingmin WANG,Haibo KE,Pei ZHANG,Tianwei LIU. U-Cr Binary Alloys with Anomalous Glass-Forming Ability. Acta Metall Sin, 2017, 53(2): 233-238.
|
|
|
Abstract As for actinide metallic glasses, a minor branch of metallic glasses, almost all of them are binary alloys and their glass-forming rule has been insufficiently studied. Considering that binary alloy systems are the base of ternary or more component glass systems that possess better glass-forming ability, binary glass systems U-Fe, U-Co and U-Cr are chosen for study. After earlier investigation on the first two systems, the glass formation in U-Cr system is explored in this work. According to the eutectic criterion, a series of U-Cr alloys were designed at the Cr-side of the eutectic point U81Cr19. Under the preparation of melt-spinning, these alloys can be formed into a single amorphous phase with the capacity of crystallizing at about 700 K. The reduced crystallization temperature (Trx) of some U-Cr alloys exceeded 0.6, higher than those of U-Fe and U-Co metallic glasses, and comparable to those of ordinary bulk amorphous alloys. Being inconsistent with the prediction based on thermodynamics, kinetics and efficient structural packing, U-Cr alloy system shows anomalous strong glass-forming ability among reported actinide binary glasses. This abnormal behavior might be related to the existence of comparatively more mediate metastable phases in U-Cr system, which can be speculated from the multi-peak crystallization phenomenon. This system could be a potential system model for studying the glass formation of actinide amorphous alloys further.
|
|
Received: 01 July 2016
|
| Fund: Supported by National Natural Science Foundation of China (No.51501169), National Defense Basic Scientific Research (No.B1520133007), and Scientific and Technological Development Foundation of China Academy of Engineering Physics (Nos.2013A0301015 and 2014B0302047) |
| [1] | Sun Y, Zhang F, Ye Z, et al.‘Crystal Genes’ in metallic liquids and glasses[J]. Sci. Rep., 2016, 6: 23734 | | [2] | Risti? R, Zadro K, Paji? D, et al.On the origin of bulk glass forming ability in Cu-Hf, Zr alloys[J]. EPL, 2016, 114: 17006 | | [3] | Klement W, Willens R H, Duwez P.Non-crystalline structure in solidified gold-silicon alloys[J]. Nature, 1960, 187: 869 | | [4] | Miracle D B,Louzguine-Luzgin D V, Louzguina-Luzgina L V, et al. An assessment of binary metallic glasses: correlations between structure, glass forming ability and stability[J]. Int. Mater. Rev., 2010, 55: 218 | | [5] | Laws K J, Miracle D B, Ferry M.A predictive structural model for bulk metallic glasses[J]. Nat. Commun., 2015, 6: 8123 | | [6] | Chen H S.Glassy metals[J]. Rep. Prog. Phys., 1980, 43: 353 | | [7] | Li J H, Dai Y, Cui Y Y, et al.Atomistic theory for predicting the binary metallic glass formation[J]. Mater. Sci. Eng., 2011, R72: 1 | | [8] | Dong D D, Zhang S, Wang Z J, et al.Composition interpretation of binary bulk metallic glasses via principal cluster definition[J]. Mater. Des., 2016, 96: 115 | | [9] | Bleiberg M L, Jones L J.The effect of pile-irradiation on U3Si[J]. Trans. AIME, 1958, 212: 758 | | [10] | Huang H G, Ke H B, Wang Y M, et al.Stable U-based metallic glasses[J]. J. Alloys Compd., 2016, 684: 75 | | [11] | Ray R, Musso E.Amorphous alloys in the U-Cr-V system [P]. US Pat., 3981722, 1976 | | [12] | Giessen B C, Elliott R O.Properties of metallic glasses containing actinide metals: I. Thermal properties of U-M glasses (M=V, Cr, Mn, Fe, Co, and Ni) [A]. Proceedings of the 3rd International Conference on Rapid Quenching[D][C]. Brighton, UK: The Metals Society, 1978: 406 | | [13] | Elliott R O, Giessen B C.On the formation of metallic glasses based on U, Np or Pu[J]. Acta Metall., 1982, 30: 785 | | [14] | Huang H G, Ke H B, Zhang P, et al.Effect of minor alloying on the glass formation of U-based alloys[J]. J. Alloys Compd., 2016, 688: 599 | | [15] | Huang H G, Wang Y M, Chen L, et al.Study on formation and corrosion resistance of amorphous alloy in U-Co system[J]. Acta Metall. Sin., 2015, 51: 623 | | [15] | (黄火根, 王英敏, 陈亮等. U-Co系非晶合金的形成与耐蚀性研究[J]. 金属学报, 2015, 51: 623) | | [16] | Venkatraman M, Neumann J P, Peterson D E. The Cr-U (Chromium-Uranium) system[J]. Bull. Alloy Phase Diag., 1985, 6: 425 | | [17] | Li G X, Wu S.Nuclear Fuels [M]. Beijing: Chemical Industry Press, 2007: 49 | | [17] | (李冠兴, 武胜. 核燃料[M]. 北京: 化学工业出版社, 2007: 49) | | [18] | Wang W H.The nature and properties of amorphous matter[J]. Prog. Phys., 2013, 33: 177 | | [18] | (汪卫华. 非晶态物质的本质和特性[J]. 物理学进展, 2013, 33: 177) | | [19] | Ke H B, Xu H Y, Huang H G, et al.Non-isothermal crystallization behavior of U-based amorphous alloy[J]. J. Alloys Compd., 2017, 691: 436 | | [20] | Rest J.A generalized hard-sphere model for the irradiation induced viscosity of amorphous binary alloys[J]. Comput. Mater. Sci., 2008, 44: 207 | | [21] | Adam G, Gibbs J H.On the temperature dependence of cooperative relaxation properties in glass-forming liquids[J]. J. Chem. Phys., 1965, 43: 139 | | [22] | Hou Z S, Lu G X.Principle of Metals [M]. Shanghai: Shanghai Science and Technology Press, 1990: 28 | | [22] | (侯增寿, 卢光熙. 金属学原理 [M]. 上海: 上海科学技术出版社, 1990: 28) | | [23] | Takeuchi A, Inoue A.Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element[J]. Mater. Trans., 2005, 46: 2817 | | [24] | Egami T, Waseda Y.Atomic size effect on the formability of metallic glasses[J]. J. Non-Cryst. Solids, 1984, 64: 113 | | [25] | Douglas J F, Betancourt B A P, Tong X H, et al. Localization model description of diffusion and structural relaxation in glass-forming Cu-Zr alloys[J]. J. Stat. Mech., 2016, 2016: 054048 |
|