Fe-based oxide dispersion strengthened (ODS) alloys are widely used in advanced aircrafts and gas turbine engines due to their good high temperature strength, creep properties and hot-corrosion resistance. Traditionally, ODS alloys are prepared by internal oxidation and mechanical alloying. However, internal oxidation cannot be applied to multi-component alloys. It is difficult to guarantee other elements from being oxidized. On the other hand, the use of mechanical alloying will bring in impurities in the process of ball milling which will compromise the purification of alloy particles surface. In this work, TiO2 xerogel prepared by using sol-gel method was added to the thermite powder mixture and the mixture was then ignited by using a tungsten filament. It solidified rapidly after the molten metal flowed into the bottom of the graphite mold because of the gravity field. It was found that Al2O3 and NiAl were formed in situ in the molten metal. Therefore, Al2O3 nanoparticles and NiAl reinforced Fe-based ODS alloy could be prepared by using this method. The phase composition and morphology of the Fe-based ODS alloy were investigated by using the combination of OM, SEM, TEM, XRD. The size of Al2O3 nanoparticles and the influence of Brownian motion and interface energy on the distribution and movement of the Al2O3 nanoparticles were investigated. The mechanical properties of the Fe-based ODS alloy with different contents of TiO2 xerogel was investigated by using mechanical properties testing machine. The experimental results show that the Fe-based ODS alloy consists of ferrite a-FeNiCrAl, NiAl, and Al2O3 nanoparticles. The diameter of Al2O3 nanoparticles is approximately 10 nm. Both Brownian motion and interface energy affect the motion of Al2O3 nanoparticles during the solidification, however, interface energy is dominant. The interface energy between Al2O3 nanoparticles and NiAl is lower than that of Al2O3 and ferrite a-FeNiCrAl. Therefore, nearly all the Al2O3 nanoparticles are connected with the NiAl phase. Higher TiO2 xerogel additions increase the tensile strengthen and elongation of the Fe-based ODS alloy. When the content of TiO2 xerogel is 1.24%, the tensile strength of the Fe-based ODS alloy attains 849 MPa and the elongation is 13%. Continuing adding the TiO2 xerogel results in the release of large quantities of gas which produces holes in the Fe-based ODS alloy and these holes decrease the mechanical properties of the alloy.
Table 1 Chemical composition of experimental thermite
Fig.1 Schematic of the thermite reaction setup
Fig.2 Sketch of tensile sample (unit: mm)
Fig.3 OM images of Fe-based oxide dispersion strengthened (ODS) alloy synthesized by thermite reaction process with TiO2 xerogel contents of 0 (a), 0.87% (b), 1.24% (c) and 1.98% (d)
Fig.4 XRD spectrum of Fe-based ODS alloys synthesized by thermite reaction process with addition of 0.87%TiO2 xerogel
Fig.5 SEM images of Fe-based ODS alloys synthesized by thermite reaction process with addition of 0 (a, b), 0.87% (c, d), 1.24% (e, f) and 1.98% (g, h) TiO2 xerogel at low (a, c, e, g) and high (b, d, f, h) magnification
Fig.6 TEM images (a, d) and SAED patterns (b, c, e) of Fe-based ODS alloy synthesized by thermite reaction process with addition of 0.87%TiO2 xerogel in dendrite (a, b), base (c) and interdendritic (d, e) regions (Figs.6b, c and e correspond to the SAED patterns of rectangle areas 1, 2 in Fig.6a and rectangle area in Fig.6d, respectively )
Fig.7 Stress-strain curves for Fe-based ODS alloys synthesized by thermite reaction process with different contents of TiO2 xerogel addition
Fig.8 Effect of different contents of TiO2 xerogel on tensile strength and elongation for Fe-based ODS alloys synthesized by thermite reaction process
Fig.9 SEM images of fractographs of Fe-based ODS alloys synthesized by themite reaction process with addition of 0 (a), 0.87% (b), 1.24% (c) and 1.98% (d) TiO2 xerogel
[1]
Pickering F B. Int Metall Rev, 1976; 21: 227
[2]
Taillard R, Pineau A. Mater Sci Eng, 1982; A56: 209
[3]
Zhu S M, Tjong S C, Lai J K L. Acta Mater, 1997; 46: 2969
[4]
Kimenkov M, Lindau R, Moslang A. J Nucl Mater, 2009; 386-388: 557
[5]
Benjamin J S, Volin T E. Metall Trans, 1974; 5: 1929
[6]
Gilman P S, Benjamin J S. Annu Rev Mater Sci, 1983; 13: 279
[7]
Suryanarayana C. Mater Manuf Process, 2007; 22: 1
[8]
Xi W J, Peng R L, Wu W, Li N, Wang S B, Johansson S. J Mater Sci, 2012; 47: 3585
[9]
Xi W J, Yin S, Lai H Y. J Mater Sci, 2000; 35: 45
[10]
Xi W J, Yin S, Lai H Y. J Mater Process Technol, 2003; 137: 1
[11]
Xi W J, Zhou H P, Ma C L, Duan H P, Zhang T. J Mater Sci, 2007; 42: 2489
[12]
Zhang K Q, Zhang K F. Met Technol, 2006; 8: 870
[13]
Wu W, Xi W J. Inorg Chem, 2011; 27: 659
[14]
Shui M, Song Y, Wang Q, Ren Y. Curr Appl Phys, 2010; 10: 1360
[15]
Baumli P, Sytchev J, Kaptay G. J Mater Sci, 2010; 45: 5177
[16]
Gregory S R. J Mater Sci, 2011; 46: 5881
[17]
Triantafyllou G, Angelopoulos G N, Nikolopoulos P. J Mater Sci, 2010; 45: 2015
[18]
Nikolopoulos P, Agathopoulos S, Tsoga A. J Mater Sci, 1994; 29: 4393
[19]
Sharan A, Cramb A W. Metall Mater Trans, 1997; 28B: 465