| [1] Campbell J.Castings. 2nd Ed., Oxford: Elsevier Butterworth-Heinemann, 2003: 178 [2] Tiryakioglu M, Campbell J, Staley J T.Scr Mater, 2003; 49: 873 [3] Li P, Lee P D, Maijer D M, Lindley T C.Acta Mater, 2009; 57: 3539 [4] Nyahumwa C, Green N R, Campbell J.Metall Mater Trans, 2001; 32A: 349 [5] Casellas D, Perez R, Prado J M.Mater Sci Eng, 2005; A398: 171 [6] Yi J Z, Gao Y X, Lee P D, Lindley T C.Metall Mater Trans, 2006; 37B: 301 [7] Lee S G, Gokhale A M, Patel G R, Evans M.Mater Sci Eng, 2006; A427: 99 [8] Lee S G, Gokhale A M.Scr Mater, 2007; 56: 501 [9] Hangai Y, Kuwazuru O, Yano T, Utsunomiya T, Murata Y, Kitahara S, Bidhar S, Yoshikawa N. Mater Trans, 2010; 51: 1574 [10] Nicoletto G, Konecna R, Fintova S.Int J Fatigue, 2012; 41: 39 [11] Felberbaum M.PhD Dissertation, Ecole Polytechnique Federale de Lausanne, 2010 [12] Felberbaum M, Rappaz M.Acta Mater, 2011; 59: 6849 [13] Zhao H D, Wang F, Li Y Y, Xia W.J Mater Proc Technol, 2009; 209: 4537 [14] Zhao H D, Bai Y F, Ouyang X X, Dong P Y.Trans Nonferrous Met Soc China, 2010; 20: 2064 [15] Nagasekhar A V, Caceres C H, Kong C.Mater Charact, 2010; 61: 1035 [16] Maire E, Grenier J C, Daniel D, Baldacci A, Klocker H, Bigot A.Scr Mater, 2006; 55: 123 [17] Kuwazuru O, Murata Y, Hangai Y, Utsunomiya T, Kitahara S, Yoshikawa N.J Solid Mech Mater Eng, 2008; 2: 1220 [18] Caty O, Buffiere J Y, Maire E, Adrien J.Adv Eng Mater, 2011; 13: 194 [19] Yi J Z, Gao Y X, Lee P D, Flower H M, Lindley T C.Metall Mater Trans, 2003; 34A: 1879 [20] Asta M, Beckermann C, Karma A, Kurz W, Napolitano R, Plapp M, Purdy G, Rappaz M, Trivedi R.Acta Mater, 2009; 57: 941 [21] Zhao H D, Wu C Z, Li Y Y.Inter J Cast Met Res, 2008; 21: 313 [22] Zhao H D, Wu C Z, Li Y Y, Ohnaka I.Acta Metall Sin, 2008; 44: 1340 (赵海东, 吴朝忠, 李元元, 大中逸雄. 金属学报, 2008; 44: 1340) [23] Chen Z W.Mater Sci Eng, 2003; A348: 145 [24] Lee P D, Chirazi A, See D.J Light Met, 2001; 1: 15 [25] Tiryakioglu M.Mater Sci Eng, 2007; A465: 287 [26] Tiryakioglu M.Mater Sci Eng, 2009; A520: 114 |