					Cite this article:
						|  |  
    					|  |  
    					| ANALYSIS OF CRACK FORMATION AT INNER SURFACE OF 1Cr13 THICK WALL TUBE APPLIED IN NUCLEAR REACTOR |  
						| SU Guoyue, ZHANG Zhen |  
						| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |  
						|  |  
					
			      SU Guoyue ZHANG Zhen. ANALYSIS OF CRACK FORMATION AT INNER SURFACE OF 1Cr13 THICK WALL TUBE APPLIED IN NUCLEAR REACTOR. Acta Metall Sin, 2011, 47(9): 1153-1154.	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract  Tempering brittleness is an important reason for microcrack formation and cracking in thick wall tube made by steel 1Cr13 which is applied in reactor driving mechanism. This article analysed the quenching effect caused by hot rolling followed by air cooling, tempering brittleness caused by annealing followed by slow cooling, and influence of rolling on the cracking direction. Improper heat treatment condition derives martensite transformation and tempering brittleness, which make the steel cracking when rapidly cold rolling. Tangential tensile stress caused by squashing the tube during rolling is the reason for the formation of longitudinal crack. |  
															| Received:  06 April 2011 |  
            
									            
									               
																												  
															| [1] Fujita T, translated by Ding W H, Zhang Z J, Chen Y Z. Heat Treatment of Stainless Steel. Beijing: Mechanical Industry Press, 1983: 23(Fujita T 著, 丁文华, 张渚江, 陈玉璋  译. 不锈钢的热处理. 北京: 机械工业出版社, 1983: 23)[2] Japan Society for Heat Treatment, translated by Liu W Q, Guo C Y, Yu X Q. Guide for Heat Treatment (Part B). Beijing: Mechanical Industry Press, 1987: 60(日本热处理技术协会 著, 刘文泉, 郭成言, 于学勤 译. 热处理指南(下册). 北京: 机械工业出版社, 1987: 60)[3] Krauss G, translated by Li C M, Xie X W, Liu R F. Principles of Heat Treatment of Steel. Beijing: Metallurgical Industry Press, 1987: 23(Krauss G 著, 李崇谟, 谢希文, 刘纫馥 译. 钢的热处理原理. 北京: 冶金工业出版社, 1987: 23)[4] Michael FMcGuire. Stainless Steels for Design Engineers. Materials Park, Ohio: AMS International, 2008: 126[5] Li L S. Plastic Deformation Theory of Steel Tube(Part A). Beijing: Metallurgical Industry Press, 1985: 358(李连诗. 钢管塑形变形原理(上册). 北京: 冶金工业出版社, 1985: 358) |  
             
								                
															
																| 
																																																																									