| SIMULATION OF THERMAL BEHAVIOR DURING STEEL SOLIDIFICATION IN SLAB CONTINUOUS CASTING MOLD I. Mathematical Model |
| CAI Zhaozhen, ZHU Miaoyong |
| School of Materials and Metallurgy, Northeastern University, Shenyang 110004 |
|
Cite this article:
CAI Zhaozhen ZHU Miaoyong. SIMULATION OF THERMAL BEHAVIOR DURING STEEL SOLIDIFICATION IN SLAB CONTINUOUS CASTING MOLD I. Mathematical Model. Acta Metall Sin, 2011, 47(6): 671-677.
|
|
|
Abstract Thermal behavior of the solidifying shell in continuous casting mold is very important to final steel products. In the present work, one two–dimension transient thermal–mechanical coupling finite element model was developed to simulate the thermal behavior of steel solidifying in slab continuous casting mold by using the sequential coupling method. In this model, in order to get the physical properties of steel at high temperature, a microsegregation model which would give the relationship of phase fractions and temperature for acquiring the physical properties with δ/γ transformation in mushy zone was established. And the heat flux was obtained according to the displacement between the surface of solidifying shell and the hot face of mold as solidification contraction, the liquid/solid structure and distribution of mold flux, the temperature distribution of slab surface and mold hot face, and air gap distribution. In addition, the rate–dependent elastic–viscoplastic constitutive equation was applied to account for the evolution of shell stress in the mold.
|
|
Received: 09 December 2010
|
| Fund: Supported by National Outstanding Young Scientist Foundation of China (No.50925415) and Fundamental Research Funds for the Central University of China (No.N100102001) |
| [1] Jing D J, Cai K K. Acta Metall Sin, 2000; 36: 403(荆德君, 蔡开科. 金属学报, 2000; 36: 403)[2] Jing D J, Cai K K. J Univ Sci Technol Beijing, 2000; 22: 417(荆德君, 蔡开科. 北京科技大学学报, 2000; 22: 417)[3] Wang E G, He J C. Sci Technol Adv Mater, 2001; 2: 257[4] Savage J, Prichard W H. J Iron and Steel Inst, 1954; 178: 91[5] Han H N, Lee J E, Yeo T, Won Y M, Kim K H, Oh K H, Yoon J K. ISIJ Int, 1999; 39: 445[6] Kim K, Han H N, Yeo T, Lee Y, Oh K H, Lee D N. Ironmaking Steelmaking, 1997; 24: 249[7] Li C S, Thomas B G. Metall Trans, 2004; 35B: 1151[8] Meng Y, Li C S, Parkman J, Thomas B G. In: Rappaz M ed., Solidification Processes and Microstructures, Charlotte: TMS, 2004: 33[9] Stone D T, Thomas B G. Can Metall Q, 1999; 38: 363[10] Ueshima Y, Mioguchi S, Matsumiya T, Kajioka H. Metall Trans, 1986; 17B: 945[11] EL–Bealy M, Thomas B G. Metall Trans, 1996; 27B: 689[12] Kawawa T. Tekko–Binran (Handbook for Steel). 3rd Ed. Tokyo: ISIJ, 1981: 205[13] Nakada H, Susa M, Seko Y, Hayashi M, Nagata K. ISIJ Int, 2008; 48: 446[14] Watanabe K, Suzuki M, Murakami K, Kondo H, Miyamoto A, Shiomi T. Tetsu Hagan´e, 1997; 83: 115(渡边圭旧, 铃木真, 村上腾彦, 近藤裕计, 宫本明,yun见刚温,铁と钢, 1997; 83: 115)[15] Saraswat R, Maijer D M, Lee P D, Mills K C. ISIJ Int, 2007; 47: 95[16] Tsutsumi K, Nagasaka T, Hino M. ISIJ Int, 1999; 39: 1150[17] Cho J W, Shibata H, Emi T. ISIJ Int, 1998; 38: 440[18] Shibata H, Kondo K, Suzuki M, Emi T. ISIJ Int, 1996; 36(Suppl.): S179[19] Yamauchi A, SorimachK, SakuryT, Fujii T. Tetsun Hagan´e, 1993; 79: 167(山内章, 反町健一, sui谷敏和, 藤井彻也. 铁と钢; 1993, 79: 167)[20] Cho J W, Emi T, Shibata H, Suzuki M. ISIJ Int, 1998;38: 834[21] Xu S L. Algorithm Commonly Used Procedures Set (C Description Language). 3rd Ed, Beijing: Tsinghua University press, 2004: 188(徐士良. 常用算法程序集(C语言描述)(第三版), 北京: 清华大学出版社,2004: 188)[22] Yamauchi A, Emi T, Seetharaman S. ISIJ Int, 2002; 42: 1084[23] Anand L. Trans ASME, 1982; 104: 12[24] Brown S B, Kim K H, AnanL. Int J Plast, 1989; 5: 95[25] Clyne T W, Wolf M, Kurz W. Metall Trans, 1982; 13B: 259[26] Davies G J, Shin Y K. Solidification Technology in the Foundry and Cast House. London: The Metal Society, 1979: 517[27] Kim K, Yeo T, Oh K H, Lee D N. ISIJ Int, 1996; 36: 284[28] Matsumiya T, Saeki T, Tanaka J, Ariyoshi T. Tetsu Hagan´e, 1982; 68: 1782(松宫彻, 佐伯毅,田中純, 有吉敏彦. 铁と钢, 1982, 68: 1782) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|