| EFFECTS OF Ti AND Mn CONTENTS ON THE PRECIPITATE CHARACTERISTICS AND STRENGTHENING MECHANISM IN Ti MICROALLOYED STEELS
PRODUCED BY CSP |
| WANG Changjun 1, YONG Qilong 1, SUN Xinjun 1, MAO Xinping 2, LI Zhaodong 1, YONG Xi 1 |
1. Institute of Structural Materials, Central Iron and Steel Research Institute, Beijing 100081
2. Guangzhou Zhujiang Steel Limited Liability Company, Guangzhou 510730 |
|
Cite this article:
WANG Changjun YONG Qilong SUN Xinjun MAO Xinping LI Zhaodong YONG Xi. EFFECTS OF Ti AND Mn CONTENTS ON THE PRECIPITATE CHARACTERISTICS AND STRENGTHENING MECHANISM IN Ti MICROALLOYED STEELS
PRODUCED BY CSP. Acta Metall Sin, 2011, 47(12): 1541-1549.
|
|
|
Abstract As an advanced manufacturing technology to produce hot rolled strips, compact strip production (CSP) process was developed at the end of last century and has been widely applied due to its high efficiency and low cost. Compared with the traditional technology, the advantages of CSP technology benefited from the refinement of austenitic grains and precipitation strengthening in the steels. This is because cooling rate is higher during the solidification of slab and the direct charging slab temperature is also higher in the CSP process, resulting in much higher solute contents in the solid solution before hot rolling than expected by the experiences from traditional steel production. So far, the Ti microalloyed steels produced by CSP process already have good performance and have drawn much attention on Ti precipitate behaviors and strengthening mechanism. However, the influence of alloying element Mn on the Ti microalloyed steels produced by CSP, especially the synergistic effect of Mn and Ti, was rarely reported. Therefore, in this work the microstructure and precipitate characteristics of two Ti microalloyed steels with different Ti and Mn contents produced by CSP process were studied by electron backscatter diffraction (EBSD) technology and high resolution transmission electron microscope (HRTEM). The results show that the steel with higher Ti and Mn contents has a higher frequency of small–angle grain boundary. Furthermore, the weight fraction of TiC precipitates with particle size smaller than 10 nm increases significantly, from 7.6% in the lower Ti and Mn steel to 26.1% in the higher Ti and Mn steel. However, the amount of Fe3C precipitates decreases markedly. In addition, the strengthening mechanism analysis of the two tested steels show that grain refinement strengthening and dislocation strengthening make great contribution to the yield strength, while the precipitation strengthening is the primary reason which causes the difference in the strength between two tested steels.
|
|
Received: 20 June 2011
|
| Fund: Supported by National Basic Research Program of China (No.2010CB630805) |
| [1] Yu H, Kang Y L, Wang K L, Fu J, Wang Z B, Liu D L. Mater Sci Eng, 2003; A363: 86[2] Huo X D, Liu D L, Wang Y L. J Univ Sci Technol Beijing, 2004; 11: 133[3] Mao X P, Sun X J, Kang Y L, Lin Z Y. Acta Metall Sin, 2006; 42: 1091(毛新平, 孙新军, 康永林, 林振源. 金属学报, 2006; 42: 1091)[4] Yi H L, Du L X, Wang G D. ISIJ Int, 2006; 46: 754[5] Misra R D K, Nathani H, Hartmann J E. Mater Sci Eng, 2005; A394: 339[6] BaiMZ, Liu D L, Lou Y Z, Mao X P. J Univ Sci Technol Beijing, 2006; 13: 230[7] Xu G, Gan X L, Ma G J. Mater Des, 2010; 31: 2891[8] Liu D L, Wang Y L, Huo X D, Chen N J, Shao W R. Acta Metall Sin, 2002; 38: 647(柳得橹, 王元立, 霍向东, 陈南京, 邵伟然. 金属学报, 2002; 38: 647)[9] Kunishige K, Nagao N. ISIJ Int, 1989; 29: 940[10] Mao X P, Sun X J, Kang Y L, Lin Z Y, Zhou J. Iron Steel, 2005; 40: 65(毛新平, 孙新军, 康永林, 林振源, 周建. 钢铁, 2005; 40: 65)[11] Liu W J, Jonas J J. Metall Trans, 1988; A19: 1403[12] Liu W J, Jonas J J. Metall Trans, 1988; A19: 1415[13] Bale G W, Liu W J, Jonas J J. Metall Trans, 1989; A20: 1371[14] Zurob H S, Hutchinson C R, Brechet Y, Purdy G. Acta Mater, 2002; 50: 3075[15] Maehara Y, Yotsumoto K, Tomono H, Nagamichi T, Ohmori Y. Mater Sci Technol, 1990; 6: 793[16] Zhou J, Kang Y L, Mao X P. J Univ Sci Technol Beijing, 2008; 15: 389[17] Nagata M T, Speer J G, Matlock D K. Metall Mater Trans, 2002; A33: 3099[18] Yong Q L, Ma M T, Wu B R. Microalloyed Steel–Physical and Mechanical Metallurgy. Beijing: Mechanic Industry Press, 1989: 62(雍岐龙, 马鸣图, 吴宝榕. 微合金钢--物理和力学冶金. 北京:机械工业出版社, 1989: 62)[19] Ashby M F. Strengthening Methods in Crystals. London: Applied Science Publishers Ltd., 1971: 137[20] Yong Q L. Secondary Phases in Steels. Beijing: Metallurgical Industry Press, 2006: 47(雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 47)[21] Gladman T. Mater Sci Technol, 1999; 15: 30[22] Mao X P. Microalloying Technology on Thin Slab Casting and Direct Rolling Process. Beijing: Metallurgical Industry Press, 2008: 100(毛新平. 薄板坯连铸连轧微合金化技术. 北京: 冶金工业出版社, 2008: 100)[23] Weng Y Q. Ultra–Fine Grained Steels. Beijing: Metallurgical Industry Press, 2008: 58(翁宇庆. 超细晶钢. 北京: 冶金工业出版社, 2008: 58)[24] Akben M G, Chandra T, Plassiard P, Jonas J J. Acta Metall, 1984; 32: 591[25] Liu W J, Sun Y, Jonas J J. Metall Trans, 1989; A20: 1907[26] Mizui N, Takayama T, Sekine K. ISIJ Int, 2008; 48: 845 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|