Please wait a minute...
Acta Metall Sin  2010, Vol. 46 Issue (5): 607-612    DOI: 10.3724/SP.J.1037.2009.00785
论文 Current Issue | Archive | Adv Search |
PREPARATION OF SUBMICRO AND NANOSIZED MAGNESIUM ALLOYS BY MULTIPLY COMPRESSED DEFORMATION
YANG Xuyue1; 2); SUN Zhengyan1); ZHANG Lei1)
1) School of Materials Science and Engineering; Central South University; Changsha 410083
2) Key Laboratory of Nonferrous Metal Materials Science and Engineering; Ministry of Education; Central South University; Changsha 410083
Cite this article: 

YANG Xuyue SUN Zhengyan ZHANG Lei. PREPARATION OF SUBMICRO AND NANOSIZED MAGNESIUM ALLOYS BY MULTIPLY COMPRESSED DEFORMATION. Acta Metall Sin, 2010, 46(5): 607-612.

Download:  PDF(788KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Twining--induced grain refinement in magnesium alloy AZ31 has been studied by using multiple compression, i.e., changing the loading direction after each pass. The tests were carried out to 50 passes at room temperature with pass strain of 0.05 and 0.1 under a strain rate of 3×10-3 s-1. The structure evolution is characterized by the formations of c-axis extension twins and c-axis compression twins, and their intersections in various directions, followed by the appearance of fragmented structure. The gradual formation of very fine grains along the c-axis compression twins with increasing cumulative strain finally leads to a ultra-fine grained structure with an average grain size of about 80-150 nm. Low strain may promote the rapid formation of more amounts of mutually crossing twins due to orientation change from pass to pass. The ultra-fine grain evolution can be accelerated by increasing pass strain. The grain refinement mechanisms under cold multiple deformation were discussed in some details.

Key words:  magnesium alloy      multiple deformation      twinning      grain refinement      deformation band     
Received:  25 November 2009     

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2009.00785     OR     https://www.ams.org.cn/EN/Y2010/V46/I5/607

[1] Wang Q D, Lin J B, Peng L M, Chen Y J. Acta Metall Sin, 2008; 44: 55
(王渠东, 林金保, 彭立明, 陈永军. 金属学报, 2008; 44: 55)
[2] Xia K,Wang J T, Wu X, Chen G, Gurvan M. Mater Sci Eng, 2005; A410–411: 324
[3] Lin H K, Huanga J C, Langdon T G. Mater Sci Eng, 2005; A402: 250
[4] Yang X Y, Miura H, Sakai T. Mater Trans, 2003; 44: 197
[5] Xing J, Yang X Y, Miura H, Sakai T. Mater Trans, 2005; 46: 1646
[6] Kim S H, You B S, Yim C D, Seo Y M. Mater Lett, 2005; 59: 3876
[7] Wang L N, Yang P, Xia W J, Chen Z H, Chen D, Li X, Meng L. Acta Metall Sin, 2009; 45: 58
(王丽娜, 杨平, 夏伟军, 陈振华, 陈鼎, 李萧, 孟利. 金属学报, 2009; 45: 58)

[8] Cottam R, Robsonb J, Lorimer G, Davis B. Mater Sci Eng, 2008; A485: 375
[9] Sun H Q, Shi Y N, Zhang M X, Lu K. Acta Mater, 2007; 55: 975
[10] Jain A, Agnew S R. Mater Sci Eng, 2007; A462: 29
[11] Gehrmann R, Frommert M M, Gottstein G. Mater Sci Eng, 2005; A395: 338
[12] Barnett M R. Mater Sci Eng, 2007; A464: 1, 8
[13] Cooling S L, Pashak J F, Sturkey L. Trans AM Soc Met, 1959; 52: 94
[14] Nave M D, Barnett M R. Scr Mater, 2004; 51: 881
[15] Li X, Yang P, Wang L N, Meng L, Cui F. Mater Sci Eng, 2009; A517: 160
[16] Yang X Y, Jiang Y P. Acta Metall Sin, 2010; 46: 451
(杨续跃, 姜育培. 金属学报, 2010; 46: 451)
[17] Wang Y N, Huang J C. Acta Mater, 2007; 55: 897
[18] Yoshinaga H, Horiuchi R. Horiuchi: Trans JIM, 1963; 4: 1
[19] Yang X Y, Zhang L. Acta Metall Sin, 2009; 45: 1303
(杨续跃, 张雷. 金属学报, 2009; 45: 1303)
[20] Galiyev A, Kaibyshev R, Gottstein G. Acta Mater, 2001; 49: 1199
[21] Liu C M, Liu Z J, Zhu X R, Zhou H T. Trans Nonferrous Met Soc China, 2006; 16: 1
(刘楚明, 刘子娟, 朱秀荣, 周海涛. 中国有色金属学报, 2006; 16: 1)

[22] Reed–Hill R E. Trans AIME, 1960; 218: 554
[23] Barnett M R, Nave M D, Bettles C J. Mater Sci Eng, 2004; A386: 205

[1] SHAO Xiaohong, PENG Zhenzhen, JIN Qianqian, MA Xiuliang. Unravelling the {101¯2} Twin Intersection Between LPSO Structure/SFs in Magnesium Alloy[J]. 金属学报, 2023, 59(4): 556-566.
[2] ZHANG Zhefeng, LI Keqiang, CAI Tuo, LI Peng, ZHANG Zhenjun, LIU Rui, YANG Jinbo, ZHANG Peng. Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. 金属学报, 2023, 59(4): 467-477.
[3] ZHU Yunpeng, QIN Jiayu, WANG Jinhui, MA Hongbin, JIN Peipeng, LI Peijie. Microstructure and Properties of AZ61 Ultra-Fine Grained Magnesium Alloy Prepared by Mechanical Milling and Powder Metallurgy Processing[J]. 金属学报, 2023, 59(2): 257-266.
[4] TANG Weineng, MO Ning, HOU Juan. Research Progress of Additively Manufactured Magnesium Alloys: A Review[J]. 金属学报, 2023, 59(2): 205-225.
[5] LI Xiaobing, QIAN Kun, SHU Lei, ZHANG Mengshu, ZHANG Jinhu, CHEN Bo, LIU Kui. Effect of W Content on the Phase Transformation Behavior in Ti-42Al-5Mn- xW Alloy[J]. 金属学报, 2023, 59(10): 1401-1410.
[6] ZHOU Hongwei, GAO Jianbing, SHEN Jiaming, ZHAO Wei, BAI Fengmei, HE Yizhu. Twin Boundary Evolution Under Low-Cycle Fatigue of C-HRA-5 Austenitic Heat-Resistant Steel at High Temperature[J]. 金属学报, 2022, 58(8): 1013-1023.
[7] CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng. Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact[J]. 金属学报, 2022, 58(5): 660-672.
[8] ZENG Xiaoqin, WANG Jie, YING Tao, DING Wenjiang. Recent Progress on Thermal Conductivity of Magnesium and Its Alloys[J]. 金属学报, 2022, 58(4): 400-411.
[9] WU Guohua, TONG Xin, JIANG Rui, DING Wenjiang. Grain Refinement of As-Cast Mg-RE Alloys: Research Progress and Future Prospect[J]. 金属学报, 2022, 58(4): 385-399.
[10] LIU Jie, XU Le, SHI Chao, YANG Shaopeng, HE Xiaofei, WANG Maoqiu, SHI Jie. Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel[J]. 金属学报, 2022, 58(3): 365-374.
[11] LI Shaojie, JIN Jianfeng, SONG Yuhao, WANG Mingtao, TANG Shuai, ZONG Yaping, QIN Gaowu. Multimodal Microstructure of Mg-Gd-Y Alloy Through an Integrated Simulation of “Process-Structure-Property”[J]. 金属学报, 2022, 58(1): 114-128.
[12] DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo. Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate[J]. 金属学报, 2021, 57(8): 1000-1008.
[13] WANG Huiyuan, XIA Nan, BU Ruyu, WANG Cheng, ZHA Min, YANG Zhizheng. Current Research and Future Prospect on Low-Alloyed High-Performance Wrought Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1429-1437.
[14] PAN Fusheng, JIANG Bin. Development and Application of Plastic Processing Technologies of Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1362-1379.
[15] WANG Xuemei, YIN Zhengzheng, YU Xiaotong, ZOU Yuhong, ZENG Rongchang. Comparison of Corrosion Resistance of Phenylalanine, Methionine, and Asparagine-Induced Ca-P Coatings on AZ31 Magnesium Alloys[J]. 金属学报, 2021, 57(10): 1258-1271.
No Suggested Reading articles found!